Immersion Tin


2000

I am looking for any information on immersion tin or immersion gold processes pertaining to the PCB manufacturing process. Specifically I'm interested in any studies comparing Immersion Tin or Immersion Gold vs. HASL finishes in the application of micro electronics. Thanks, Rick Jackson

Rick Jackson
- Melbourne, Florida, USA


2000

You might get this publication: "Implementing Cleaner Printed Wiring Board Technologies: Surface Finishes" (EPA 744-R-00-002); it can be ordered from the Pollution Prevention Information Clearinghouse online through the EPA Website or download from www.epa.gov/dfe. The Design for the Environment EPA project did a good job in their "Making Holes Conductive" project.

James Totter
James Totter, CEF
- Tallahassee, Florida


2006

Sir,

Immersion Tin is primarily a three-step process: Cleaning-Microetching-Immersion Tin. But Some suppliers give an option of conditioning the copper surface before Immersion Tin. Please could someone clarify whether I should go for conditioning step before Immersion Tin?

Sonali Kokane
plating shop employee - Mumbai, Maharashtra, India



If you have a question in mind which seems off topic, please Search the Site

ADD a Comment to THIS thread START a NEW threadView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.