"How to blacken stainless steel parts"



1999

Need information on the blacking and passivation of stainless steel parts. Thanks

Bob Zulewski
finishing shop - Old Hickory, Tn
^


1999

A black oxide coating is a very good way to blacken ss parts and they can be done pretty inexpensively by many plating and finishing jobshops. A quality afterfinish coating is paramount to achieving a lasting, quality finish.

Dan Brewer
chemical process supplier - Gurnee, Illinois
^

none
finishing.com is made possible by ...
this text gets replaced with bannerText
spacer gets replaced with bannerImages

Q, A, or Comment on THIS thread SEARCH for Threads about ... My Topic Not Found: Start NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

 
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g, Train'g
& Software


About/Contact    -    Privacy Policy    -    ©1995-2021 finishing.com, Pine Beach, New Jersey, USA