54000. Need dip tank paint to avoid drips sags and runs.
54001. Hard chrome plating solution effect on cadmium plated part
54002. Nickel sulfamate filtering issues
54003. My gold plating rubs off in 15-20 seconds!
54004. Temperature limitations of black anodised aluminium 6082-T6
54005. Removal of Alumina Inclusion from SS316L Electropolished Surface
54006. Black oxide or Cad plating. Which one is better? camera
54007. Need to electroplate gold and silver Chalices for Worship {1/7/10}
54008. Need 440 A Stainless {1/7/10}
54009. Anyone know where to buy "Kold Black"? {1/7/10}
54010. Need X-Ray Thickness Tester
54011. Need equipment for water immersion test for passivation of stainless steel {1/7/10}
54012. How to raise pH of acid using DI water
54013. Avoiding pinholes when plating neodymium iron boron
54014. Co/W or Ni/W alloy coatings on stainless steel? which one?
54015. Gold testing from diggers
54016. Removing Oil Paint from new brass hardware.
54017. A "yellow pewter" metal for low temp casting
54018. Can I make my stainless steel appliances have a swirly look?
54019. Repair enamel-on-steel baking dish camera
54020. Query about rectifier capacity
54021. Salt spray test on assembly - galvanic corrosion problem
54022. How to strip tin-nickel plate
54023. Baked zinc plating vs. zinc without bake
54024. Setting up a paint booth for lacquering
54025. Autophoretic Coating castings and the best surface preparation method for this.
54026. Galvanize flake off problem in 25 mm thick angles
54027. Hard chrome finish on 316 stainless
54028. Purpose of Hydroxides in Silver Plating Baths
54030. Wipe cleaning cold rolled steel
54031. Alternative plating process for Chrome on ZAMAK metal camera
54032. Need Deoxidine 314 and 301 {1/8/10}
54033. Galvanized Kitchen Counter Top
54034. Are unused M-2 Gold Salts saleable?
54035. Annealing needed after SS 316 shaft welding (LOX fluid)?
54036. Benzene removal with surfactants
54037. Recycling of Chrome Hydroxide cakes from plating solution
54038. What Dyes Work Well with Alodine T5900
54039. Remelting zinc onto galvanized members after welding process in the field.
54040. Lacquer yellowing
54041. Corrosion problem in galvanized steel tubular profiles finished with powder coating
54042. Cracking or crazing of powder coating
54043. Need plating that has a higher than average frictional characteristics
54044. Metal treatment before painting
54045. ENP vs. Chrome Plating for ball valves
54046. Cost Comparison Between 316 SS, 316L SS and Alloy 20
54047. Heat released in electropolishing of stainless steel
54049. Clear Coated Anodized Aluminum vs. Winter Road Salt ?
54050. Painting anodized alloy wheels
54051. Factory stainless needs a mirror finish
54052. Does stainless steel flatware with a shiny (mirror) finish scratch easily over time?
54053. Could working in foundry inhaling aluminum fumes cause Parkinson's ?
54054. Disposing of Chromic Acid Bright Dip
54055. How to Ti plate a stainless steel 2" spherical shift knob to heat for a "burnt" look
54056. Blistering in Nickel Sulfamate Electroforming
54057. 18K White Gold becomes magnetic when filed or cut in half
54058. Iron Phosphate performance test
54059. Need chrome plated tubing {1/12/10}
54060. Difference between black oxide and nitriding
54061. Orthophosphate in Cu Pyrophosphate Bath
54062. How to obtain RH950 Condition
54063. Starting a plant suitable for zinc plating with yellow passivation
54064. Pretreatment for painting of aluminum flat sheet
54065. Standard thickness for plating on ABS
54066. Need small mufflers coated to shine like chrome {1/13/10}
54067. How to repair or paint over damaged silver plating on candle sticks? camera
54068. Aircraft firewall cleanup camera
54069. Need ASTM F519-06 Test Specimes type 1.c {1/13/10}
54070. How to stop the rusting process on iron WITHOUT altering the look of the rusted surface? camera
54071. Pretreatment for powder coating on aluminium castings (PDC)
54072. Need Ferroxyl Testing Service {1/14/10}
54073. Laser marking cracks ceramic tools
54074. Cadmium is being used in Asian charm bracelets
54075. Problems with residual static electricity after protective film removal from construction panels
54076. Seeking tining of copper pins small batch {1/14/10}
54077. Need Nickel Plating Service {1/14/10}
54078. Need used low voltage DC with superimposed AC anodizing rectifier {1/14/10}
54079. Need used filter presses
54080. Need rotary vacuum drum
54081. How do I reclaim gold plating from Mil-Spec Connector Pins? camera
54082. Recovering gold that was mixed with aluminum camera
54083. Coatings/platings for visible and infrared light mirror
54084. Recoating Vintage Dishware
54085. Stripping to determine Chromic Acid Anodizing thickness
54086. Tungsten carbide coating on aluminum
54087. Silver plating over electroless nickel for salt fog resistance
54088. Architectural black oxide work {1/15/10}
54089. Want to buy gold melting machine {1/15/10}
54090. Spring Tool Dip/Spin Machine
54091. Complexing Agent to reduce wt% of Nickel in ZnNi plating
54092. 316 SS Electropolishing
54093. Polishing Titanium with Power Tools?
54094. Polishing carbon steel w/ decorative inlay
54095. Material Needed for Drink Dispensing Robot
54096. Can gold be reclaimed from old ceramic dishes with gold trim on the edges
54097. Why did my silver toned bowl turn black in the dish washer?
54098. Is Silver Deposit the same as Silverplate
54099. Can One Buy Treated to Paint Aluminium Anywhere?
54100. Gauging problem after case hardening
54101. QQ-Z-235 vs. ASTM-B633
54102. Chemical wet analysis of nickel strike to determine iron content
54103. Controlling Zinc Granules on edges of galvanized coils camera
54104. Hot dip tin discolors
54105. Aluminium addition to Galvanising Kettle
54106. How to Make Nickel Plated Copper Heatsinks Shiny?
54107. Bright Acid Copper adhesion issues
54108. Gold plating on thin Molybdenum wires
54109. Scratches on my chrome plated hydraulic cylinders
54110. Will nickel plating the top of cookstoves work?
54111. Corrosion problem on tin plated brass buttons
54112. Epoxy Resin and Anodized Aluminium
54113. Mild steel blackening
54114. Activated Carbon heavily pitting 304 stainless steel
54115. Need AMS 2417 Zinc-Nickel plating service {1/19/10}
54116. Need black oxide on stainless steel bolts {1/19/10}
54117. Need Mil-Std-171 anodizing service {1/19/10}
54118. Need to install stainless passivation and enameling capacity {1/19/10}
54119. Copper roof on the Atlantic
54120. Should I use acid on my old aluminum boat? Lye is bad for aluminum? camera
54121. Refinishing antique "rubbed" solid brass bathroom sinks camera
54122. How to get low current flow from a large rectifier
54123. Passivation Tank Liner?
54124. Stripping of EN with Nitric plus acetic acid mix
54125. Fabricating a diamond polishing scaife by plating
54126. Can zinc plating plus chromate on SPCC peel off or flake?
54127. Post-fab heat treatment of aluminum
54128. Will post-anodizing punched holes discolor?
54129. Trivalent Coating vs Anodizing
54130. Request for formulation of etching chemical
54131. A chemical reaction question
54132. How to remove gold paint from antique silver pitcher? camera
54133. Making metal trim "antique" for fashion
54134. Cleaning on hardened jobs before Zinc Plating
54135. Looking for company to refinish Woodard aluminum furniture {1/20/10}
54136. What's a control?
54137. Dipping your own jewelry
54138. White corrosion on stainless steel hardware joining structural steel
54139. Alternative to Zinc Chromate for outboard motors in salt water
54140. How to remove "m seal" stains from ceramic wash basin?
54141. Manganese phosphate removal from steel. What chemicals will do this?
54142. Cathodic electro deposition of paint by barrel method
54143. Dichromating of aluminium casting machines
54144. What is reasonable Rz finish on stainless steel roller?
54145. We require a coating to replace hot dip galvanising
54146. Anticorrosive epoxy coating for 50% sulfuric acid
54147. Does Welding increase permeability of 316L Stainless Steel?
54148. Anode-cathode ratios for E-coating
54149. HOW COULD I REDUCE AND REMOVE ZINC DROSS
54150. Nickel Plating (Wood's Nickel Strike and Sulfamate Nickel)
54151. Zamak 5 Plating process questions
54152. Alodine treatment to Mil-C-5541 Class 3 on cast aluminium parts, AlSi10Mg T6
54153. Black IP plating on Tungsten Ring Jewelry
54154. Alternative titration method to anaylze HF and ammonia bifluoride
54155. Interpreting salt spray testing results
54156. Copper base material with arc spray aluminum coating camera
54157. Chrome Plating on Aluminium
54158. Zinc Plating of brake components?
54159. Need to order ALUMINUM already ANODIZED {1/22/10}
54160. Black oxide on H13 tool steel
54161. How do I get an antiqued metal finish? camera
54162. Low Temperature Powder Coating
54163. Coating Steel Wire with Niobium, then Anodizing the Coating to Create Colors
54164. Need silver plating of telecommunication components {1/26/10}
54165. Need SSPC or NACE-qualified inspection service {1/26/10}
54166. Need Salt spray testing per ASTM-B117 {1/26/10}
54167. Need HCN destruct unit for chemical industry {1/26/10}
54168. QUESTION RELATING TO DIN 50961
54169. Removing aluminum arc spray coating from aluminum substrate
54170. Testing adherence of chrome plated shafts
54171. Zinc Plating process : Guide me from cleaning through drying
54172. Trivalent silver plating
54173. Cold sealing after color anodizing
54174. Copper contaminnation in Hard and Type 2 Anodize Tanks
54175. Soak temp and time
54176. Need refinishing of 100% copper globe stand {1/27/10}
54177. Seeking Electro Tin-Lead Finish of CRS/Stainless Steel Chassis {1/27/10}
54178. Materials that can be 14K plated
54179. NiCl2 vs MgCl2 in a Nickel speed bath
54181. Mechanism of adhesion between nickel and stainless steel
54182. Homeowner needs advice on refinishing bronze Andirons
54183. Powder coating over zinc spray surface
54184. Re-chrome bronze boat hardware
54185. Visual Inspection Coupons for Chromate Conversion
54186. Measuring hard anodise thickness concentricity
54187. pH and acid measurement in stainless steel pickling
54188. Hard chrome plating parameters
54189. Spraying zincate onto an aluminum automobile
54190. Powder Coating Screws
54191. Hard coatings for magnesium
54192. Chromating of zinc phosphate coated part
54193. Maximum allowable metal contaminant levels in various plating baths
54194. Air Agitation for an anodizing tank
54195. Turn a wedding band into another piece of jewelry
54196. Trying to make mild steel take on a copper color with patina
54197. Marine Transportation of Mill Scale
54198. Wanted consultant for manufacture MIG Wire {1/29/10}
54199. Need ASTM B633 zinc plating service {1/29/10}
54200. Where to Buy Parts For Old Vibratory Tumblers {1/29/10}
54201. Powder coating a galvanized sliding gate
54202. Paint directly to conversion coating (alodine, iridite, chem film etc)?
54203. Electroless nickel plating on cast iron parts
54204. Electrodeposited hard chrome plating vs salt spray requirement
54205. Phosphating or Galvanizing --which is better before finishing it with powder coating camera
54206. What happens to raw aluminum sheets when they rub against one another
54207. Is this Satin Chrome or Paint?
54208. Why is black iron pipe 21 feet long and galvanized pipe 20?
54209. Ocean cottage lighting fixtures
54210. Reinforcing Titanium plate with 316L Stainless Steel
54211. AFNOR Cup vs. ISO Cup
54212. Automatic aluminium anodize thickness inspection
54213. White Rust on zinc plated articles camera
54214. Low Lubricity Plating on Zinc Die-Cast
54215. Which stainless steel grade suitable for Bus Shelter ... 304 or 316 ?
54216. Other finishes for pewter castings
54217. How to make iron turn black color without using black paint
54218. Perkins' Permanent Stereotype Steel Plate: can cast steel have been used successfully?
54219. Gold or Other Metal Plating on Aluminum for Chemical Resistance to Mild Aqueous Conditions
54220. Corten steel coating for backdrop for museum artifacts
54221. Iridium mirrored coatings on motorcycle face shields
54222. Are Mirro Wearever Cookware Teflon Fumes poisonous to pet birds?
54223. Want dark green antique on brass zippers
54224. Zinc Die Cast Components = Improving washing performance
54225. Parts turns blue after silver plating
54226. Tin plating turns black after 5 to 6 months
54227. Delayed plating peel off
54228. Life of zinc phosphating on SECC material if not painted
54229. Need cadmium plating {2/2/10}
54230. Need electrophoretic lacquering of silver plated jewelry {2/3/10}
54231. Electrolysis of copper sulfate in soil
54232. Where Can I Buy PVC Coating For Wire Mesh Lobster Traps ?
54233. Can a magnet cause a metal to increase it's corrosion rate
54234. How to induce non uniform thickness in electroless plating?
54235. A project head line
54236. Plastic coating a coffee table to embed photos
54237. Turning Copper Green Fast
54238. Cleaning rust on iron gates
54239. Lockheed Martin requirement: NKP300
54240. Removing Alodine from magnesium components
54241. Removal of EDM Wire Cut Brass Residue
54242. How to apply coatings over zinc and cadmium platings
54243. E-coating of parts that were manufactured to size
54244. Electroless nickel plating on already plated parts
54245. Rhodium Plating darkens or blues the diamonds
54246. How much thickness is required of tin plating on copper busbar
54247. Is Bead Blast finish possible on aluminum
54248. How to finish titanium cylinder liners
54249. Seeking grey hardcoat anodizing for 5052/6061 color matching critical {2/5/10}
54250. Need mild ultrasonic degreasing agent {2/5/10}
54251. Tell me about cyanide process for gold dissolution
54252. Painting a countertop to look like granite
54253. Finding no aluminum sulfate in anodizing tank although I put it there
54254. Clean Earth Silver Plating Solution: Cyanide Free?
54255. Xylene-resistant touch up paint for automotive
54256. What pipe material for Platinum-Rhodium plating filter?
54257. Using Extracted Licorice in hot dip galvanizing
54258. Zinc vs. Nickel Plating, and Rack vs. Barrel
54259. Hard anodized coating will not accept color (black)
54260. Addition of ammonium bifluoride to increase titanium etch rate
54261. Will electropolishing Titanium/Stainless Steel artwork improve corrosion resistance
54262. Qualified finisher needed to coat stainless belt buckles {2/5/10}
54263. How to give mild finished steel an "antiqued" look?
54264. How to re-rifle and re-blue Winchester model 1906
54265. Clear coating Aluminum: Oil based vs Water based?
54266. 40 year old stainless utensils suddenly formed blisters
54267. How can I learn to do Paint Production?
54268. How to slow down the solidifying process for Bismuth-tin alloy?
54269. Pitting of hot dipped Galvannealed parts during e-coating
54270. Real-time thickness data collection on pipe galvanizing line
54271. Percentage of lead consumption in continuous galvanizing line?
54272. Acid cadmium vs. Cyanide cadmium bath
54273. Need anti impression lacquer for aluminum after chrome passivation process camera
54274. 430 series stainless steel electropolishing
54275. Learning never ends - teach me making of liquid polishing material
54276. What material will offer high coefficient of friction but not be abrasive?
54277. Seeking 14 kt gold plating for a jewelry piece {2/9/10}
54278. Wanted wheel polishing machine for truck aluminum wheels {2/9/10}
54280. Electrolysis in copper pipes and pipe hangers.
54281. I need hydraulic parts for a Belmont barber chair camera
54282. Chrome finish has eroded from taps and pipe work
54283. Sulfuric Acid turned brownish color
54284. Finishing a Stainless Steel Tree
54285. My gold ring has tunred white
54286. Any problem using "zine china" salad utensils as serving spoons?
54287. Recoating a Griddle
54288. Help us turn our emotionally valuable yellow gold into meaningful white gold wedding rings!
54289. Brass coated steel needs to be redone, can I spray paint it? camera
54290. How to tell the difference between mild steel and core 10
54291. About full function of deionized chromotography by ion exchhange resin
54292. Acid Recovery System for pickling wastewater
54293. High Gloss Powder Coat Losing Its Gloss
54294. Nickel sulfamate pitting problem
54295. Zinc plating problems in case-carburized component
54296. RoHS Compliance for Nickel Plating
54297. Clear Anodizing Finish with a gray appearance.
54298. Double coat anodizing aluminum
54299. Problems getting on anodized surface after applying surface protection tape
54300. Black coating, inexpensively onto steel part
54301. Corrosion in CE3MN and CK3MN cast FEED/Concentrate ports
54302. Mos2 coating
54303. Seeking Brass Plating {2/9/10}
54304. Re-tinning of hobart 8 quart mixing bowl {2/9/10}
54305. Indium tin oxide
54306. Electrogalvanized nails for 3 tab shingles?
54307. Coating druzy quartz with titanium
54308. Solar Air Heating Coating for Absorber Plates
54309. Question about old sterling spoons
54310. Elevator Door Scratches
54311. Reviving copper-plated fireplace cover
54312. Rules for Plating in Mexico
54313. How to make mirror finish on aluminium longlasting ?
54314. Rusting metal
54315. Black Zinc Turning Green
54316. Soften C26000 brass
54317. Seeking Plating Company {2/11/10}
54318. Seeking company to gold plate sterling silver {2/11/10}
54319. Powdercoating my bike chassis {2/11/10}
54320. Chrome plating fiberglass {2/11/10}
54321. Need 24K Gold on 1"x 1"x 56"Long Brass Shower Door Piece {2/11/10}
54322. Will copper dissolve in hydrochloric acid under 100 degrees celcius?
54323. Ratio for caustic soda solution
54324. What is a better application: Nickel Plated or Nickel-Tin?
54325. Why did my copper gutters turn a streaky black?
54326. How to patina a polished copper range hood camera
54327. Copper paste
54328. Looking for a protective coating for acid sensitive items with sharp edges
54329. Help! Expensive "weathered brass" faucet ruin by cleaning product
54330. Safety in Serving
54331. Cu/Ni 5b dark
54332. ASTM B 633
54333. Rate of Sodium Carbonate Build-up in Stored Cyanide Plating Baths
54334. Technique for recycling Caustic Soda
54335. Green gritty bukduo on nickel rounds in the anode baskets
54336. Screw threads will not accept Go gage after chrome plating
54337. Chrome hard plating flaking on loaded threaded fasteners
54338. Electroplating lead on brass items
54339. Area of anode with respect to cathode in chrome bath
54340. Plating nickel over lead and brass
54341. Clear anodizing that looks like gray paint.
54342. Anodizing and Light Metals
54343. Is a Finish Required
54344. Need electroforming gold, silver, copper and pewter solution - wholesale {2/12/10}
54345. Want to Buy Chrome Plating Business in Dallas Ft Worth area {2/12/10}
54346. ACIDIC PRETREATMENT OF TITANIUM
54347. Saline chamber test interrupted...may I continue?
54348. Protecting Aluminum From Steam
54349. Newly painted car has very fine scratches all over due to hand washing at repair shop
54352. Treatment system for hotel
54353. Calculating the usage of chemicals per kg plated
54354. Cathode Trouble
54355. Zinc brightener
54356. Re chroming fishing reel parts {2/16/10}
54357. Plating Copper - Bright Colors {2/16/10}
54358. Textured Silver Anodizing on 6061-T6 {2/16/10}
54359. Hard Chrome or Decorative Chrome on this Drive Part camera
54360. Charcoal filtering for air pollution control of small-scale nickel plating
54361. Water Treatment Clarifier Problem
54362. Continuous ultra filtration in electrophoretic lacquer bath
54363. Galvanising S G iron castings
54364. Copper strike on zinc diecastings
54365. Tin Plating Issues
54366. Gold won't stick to SS parts
54367. How can I keep automotive trim bright when anodized
54368. Chem Film Surface Resistance Measurements
54369. Electropolishing Stainless Steel
54370. Anti corrosion coating for springs
54371. Info on battery grade nickel plated steel
54372. Post plating "blackening" of nickel plating
54373. Best material for master model for silicone mold
54374. Re-powder coating of an old aluminum
54375. Finger pain because of wedding band?
54376. Artist worried about inhaling chemicals but wants to buy cyanide
54377. Starting a clear chromate and Tufram coating operation
54378. Old silverplating shop for sale as residence -- any dangers I should know about?
54379. Copper Solution was contaminated
54380. Don't have chemical know-how about plating, can you help?
54381. Printer has excessive plate wear
54382. Black spots after machining and white spots after cadmium electroplating on Al-7075 T6 material
54383. Second-hand metal poisoning from my roommate's job?
54384. High friction durable coating needed for 6000 and 7000 series aluminum alloys
54385. 410 SS castings turning black after Nitric 1 passivation
54386. How much chrome passivation goes on the strip and how much to waste?
54387. Gravure Copper and Chrome Platers Wanted by Diamond Turning Machining Company camera{2/18/10}
54388. pH rise in nickel electrolysis
54389. Pretreatment process for zinc electroplating of heat treated parts
54390. PALADIN COATING {2/18/10}
54391. Does the Temperature of Water Affect the Rate of Oxidation of a Nail?
54393. How to demagnetize stainless steel pins
54394. Black Oxide's affect on 316 stainless corrosion properties
54395. Gold plating over nickel plating for outdoor application
54396. Best preplate for decorative copper nickel chrome on leaded brass
54397. Chrome Plating Pitting and Metals Contamination
54398. Anodizing cast aluminum
54399. Phosphating Process after Cold Forging
54400. Thin film, dry type, corrosion resistant treatment after nitriding
54401. Maximum Thickness of Powder Coating
54402. Hot Dip Galvanising Bath for Economic Development Initiative
54403. Source needed to cadmium plate copper wire {2/19/10}
54404. Need vibratory polishing machine and media {2/19/10}
54405. Using titanium anodes in a iron containing copper plating setup
54406. Plating on plastics books?
54407. Coating Aluminum onto Copper
54408. NEED ELECTROPLATED FINISH - NICKEL PEWTER {2/19/10}
54409. Need stainless steel wire, with nickel strike {2/19/10}
54410. NAILS RUSTING! I NEED HELP!
54411. Need copper parts gold and silver plated {2/19/10}
54412. Need extrusion roller engraved (product development) {2/19/10}
54413. Risks and Challenges of Tin Plating in Mexico
54414. Need Brass Chandelier Dulled {2/23/10}
54415. NEED MY BRASS CANDELABRAS REFINISHED OR REPLATED {2/23/10}
54416. Need center caps plated {2/23/10}
54417. Electrolytically recovering Scrap Copper
54418. Blueing didn't take after bead blasting nickel plated barrel
54419. Testing iron concentration in AMS 2700 passivation tank
54420. Contamination problem in e-coat system?
54421. UF Module Suddenly Failed To Separate E Coat
54422. Copper Plating Teflon or Similar Plastics to Allow Soldering of Wires to it camera
54423. Problem in nickel plating
54424. Nitric acid as a component to balance pH for chromate bath
54425. Stainless steel weld discoloration after electropolishing camera
54426. Surface prep to stop high temperature discolouration of 304 stainless?
54427. Swimwear Hardware Inquiry camera
54428. Need Dark Patina Bronze Samples {2/25/10}
54429. Need Dupont 606 S polishing compound or equal {2/25/10}
54430. Silver plated connection
54431. What is this process (not Aurora plating) called? camera
54432. Powder paint adherence problems
54433. How to reduce the resistance of PVD films?
54434. Speed up the electroless nickel deposition
54435. Which is easier to finish, brass or zamak?
54436. White deposits zinc-cobalt plated aluminum
54437. What compound is cadmium bloom/whiskers?
54438. Titanium clear sealing camera
54439. Best Aluminum Choice for Long Lasting Anodization?
54440. Are aluminum die castings vs. forgings more plateable?
54441. Is there chromate in chromic acid anodized components?
54442. Switching from anodized finish to Iridite
54443. Need acetal alcohol applicator {2/25/10}
54444. Dip my ATV plastics in camouflage please {2/25/10}
54445. Ferrite testing and corrosion testing
54446. Cost of Alodine 5200 coating installation
54447. Spent pickling acid treatment
54448. Salt Fog Cabinet Setting for ASTM B117 vs. ISO9227?
54449. Laser Etchable Epoxy Paints
54450. Most economical painting for steel piles rented for immersed seawater condition
54451. Using Quench Tank Overflow for Rinsing
54452. Are there any methods known to make an electrogalvanized Galvannealed alloy?
54453. Electroplating Peels Off Aluminum Extruded Sections
54454. Are internally scuffed tubes okay in air conditioner?
54455. Melting of Electrowinned Zinc
54456. Coating sodium metal with T6 aluminum, beryllium copper, Invar and/or molybdenum.
54457. Selective precipitation of gold from aqua regia, leaving PGM in solution
54458. Availability of concentrates to make "Concrete Acid Stains"
54459. Carbon in gold plate
54460. Silver plating process
54461. Yellowing in electroplated tin on aluminum camera
54462. Reflective pre-finish needed for stamped parts
54463. Small shot blast/peen cabinets?
54464. Want technology for Nickel Electroformed Nameplates {3/1/10}
54465. Want to Buy Dip Spin Coating Equipment {3/1/10}
54466. Recovering gold from investment powder paste
54467. Acid zinc plating questions
54468. Rhodium plating
54469. Clear coat for bottle cap floor? camera
54470. Can porcelain coating salvage cooktop bezels?
54471. Base coat combination for recycled plastic
54472. Grinding of chrome plating resulting in peeling off on titanium parts
54473. Black marks on gold plated items(nose pins)
54474. Reducing pitting and blisters in silver plated components
54475. Rhodium plating parameters
54476. Re-phosphating sheared edges of pre-phosphated strip
54477. Cement vs. epoxy lining for protection of sea water intake steel pipe
54478. Need silver ladle plated {3/1/10}
54479. Small 2 Stroke Piston - Adhesion Testing of Plating
54480. What alloy are VW Aristo OEM wheels? Will powder coating damage them?
54481. Etched ss after electropolishing camera
54482. Anodized products for use in contact with food
54483. Compatibility of a brass valve in a steel air receiver
54484. Need plating barrel for plating ABS plastic {3/3/10}
54485. Paint for acrylic mirrors
54486. 316 stainless steel can't be polished without pits, inclusions or voids
54487. Want antitarnish treatment for bright dipped brass that is good to 200 C
54488. Sanding 439 stainless steel
54489. ECoat Source for 31 Foot Long Parts in Southeast! {3/3/10}
54490. Copper vs. brass flash on steel wire clips, before nickel plating?
54491. Problems of gold plating onto copper jewelry
54492. Can't find Hard Anodizing in Turkey
54493. Galvanic concern with stainless or epoxy coated "hot tapping" of copper piping?
54494. Electroless plating starts fast, then slows to a stop
54495. Stainless or Zinc Plated Screws on Aluminum, how much/fast will corrosion occur?
54496. Require waterbased lacquers for plastics {3/3/10}
54497. Need O'Keefe & Merritt stove and a Barber's Chair replated {3/4/10}
54498. Need Testing Equipment for water immersion testing MIL-STD-753 {3/4/10}
54499. Galvanic Corrosion - Stainless Steel Rod with Carbon Steel Nut
54500. Need help with Keystone rims
54501. Bad chrome plating from China
54502. Best method to blacken chromed forks on Honda Z50?
54503. Question about repairing gold filled object by selective plating?
54504. What plating is safe to lick?
54505. Carryover of power in the plating tank with power off
54506. Remove silica from drinking water
54507. Identifying L605 surfaces that are contaminated with 17-4
54508. Single rinse tank between pickling and fluxing
54509. Blackening or Phosphating of injection mold plates?
54510. Looking for an anodizer Pittsburgh {3/8/10}
54511. Need Black Chrome for CAMERA PARTS {3/8/10}
54512. Corrosion problems on copper-nickel plated zinc parts exposed to toilet cleaning liquids camera
54513. Durability of Flash Gold Plating on Brass
54514. Electroplating brass wedding bands with Copper-Nickel-Rhodium. HELP!
54515. Why does chromic acid anodize have excessive white powder residue after DI sealing
54516. Rephosphating on phosphated SECC material
54517. Blasting of Zirconia
54518. Zinc on steel solution
54520. Why not galvanize propellers?
54521. Do the amount of diamonds in your setting affect the rhodium plating?
54522. HELP! The fumes are so strong!
54523. Primer paint vs rust preventative oil coating
54524. Thickness of Galvanizing on MS Section
54525. Cadmium Bloom Repair
54526. Zinc nickel plating curing time?
54527. CD DVD nickel stamper scraps - recycle or sell?
54528. Tin plating gray deposits
54529. Hard anodizing 2014 aluminum
54530. Mirror polishing stainless steel for a mold insert to make an aircraft lens
54531. Surface treatment for EN AW 1050A Aluminum (European spec)
54532. Need light box stove varnished camera{3/10/10}
54533. Need Pearl Glanza {3/11/10}
54534. Hard Anodize Problem on AL2024
54535. Chemistry of the Loonie
54536. How to get shiny stable surface on brass until we can get it into nickel plating
54537. Why did the ancients copper plate gold rings?
54538. Boyfriend wants to "pan" catalytic converters like you do for gold
54539. Kitchen cooker changes colour
54540. Need hot barrel painting equipment and process for small parts in bulk {3/11/10}
54541. Paraffin test for hydrogen de-embrittlement
54542. Electroless nickel on steel shaft - hard ground surface for rotary lip seal contact?
54543. Silver plating is not shiny and white
54544. How to get a matte surface before aluminum anodizing?
54545. Looking for a Distressed Antique Bronze finish for aluminum substrate
54546. Seeking large filter press
54547. Corrosion testing and ferrite testing
54548. Vinyl pipe paint
54549. Best finish to avoid corrosion bonding of steel exposed to calcium chloride (road salts)
54550. Electroless nickel on steel and stainless steel substrate in marine environment
54551. Galvanized steel building allergy?
54552. Why Don't Electric Fences Kill Us?
54553. Need aluminum coil anodizing line {3/12/10}
54554. Hard chrome plating ENGINE cylinders? (2 stroke to be exact)
54555. Successfully Plating Cobalt on Beryllium
54556. Stainless steel ring toy needs a safe finish so kids don't get poisoned
54557. Testing to tell Geomet Vs Dacromet
54558. Maintaining high finish on copper sprinklers
54559. Ruthenium finishing
54560. Treating Acid Waste
54561. Brilliant copper finish
54562. Need to brass plate old kitchen hinges {3/16/10}
54563. Looking for Spiral Contractometer
54564. Copper plating on gravure cylinder
54565. Coating identification from a picture camera
54566. Enamel (porcelain) coating with powder or paint
54567. Adhesion of Gold to Quartz
54568. FeSO4 Electrolysis to restore Sulphuric Acid
54569. Heat resistant coating for wood
54570. Looking for a DYI method for a baked-on shellac finish for sheet brass
54571. Heating zinc plated springs to dull the finish
54572. Polished chrome vs brushed chrome door lever handles
54573. Bronze Plating: Cyanide vs. Alkaline Pyrophosphate
54574. Need steel washers plated to TSH7702G {3/18/10}
54575. Need barrel plating tin or zinc in precious metal tones {3/18/10}
54576. Need "Star Wars" plastic "armor" chromed {3/18/10}
54577. Dog pan that turned black
54578. Spec for galvanized outdoor tables
54579. Gold necklaces turn black after electrodeposition
54580. Nickel Electroplating is peeling off Stainless Steel dental instruments
54581. Any one providing USP class 6 approved powder? Grey or Black {3/19/10}
54582. How has my electroplating experience made me a valuable Chemical Engineer?
54583. Recovery of gold from thiourea based electropolishing solution
54584. Create slippery surface on PP Plastic
54585. Dry Film Lube on Stainless Steel
54586. Does excess galvanising coating thickness affect the steel structure?
54587. Peeling after nickel and gold plating
54588. Question about reverse plating in Watt's bath
54589. Yellow chemical conversion on Al turns PINK when exposed to vacuum
54590. What media and liquid for polishing silver coins in a vibratory finisher?
54591. Want brass door knocker Satin Nickel Plated {3/19/10}
54592. Need used 100 cu ft gasketed filter press
54593. Want Silver Plating that glows in the dark
54594. What does the number 1 mean on a very old Made in Italy ladies compact mean? camera
54595. Using Krylon Clear Fusion on golf balls
54596. Aluminum Fishing Reel Corrosion
54597. Hard chrome plating thickness to avoid peel off
54598. Solderable Plating on Beryllium Copper to Survive Heat Treat
54599. Pulse Reverse Copper Plating
54600. Improve nickel adhesion to silver paste
54601. Trivalent chrome plating chemistry
54602. Intermittant pitting after HAE magnesium anodise
54603. Temperature limits for MIL-DTL-5541 chemical conversion coatings
54604. Iron contamination of austenitic stainless steels results in rust and further corrosion
54605. Need reducer liquid: sodium hypophosphite {3/22/10}
54606. Determination of the throwing power of a Wood's nickel plating bath
54607. Chemical passivation method for inconel alloy
54608. When Did Silver First Start Tarnishing?
54609. Looking to electroplate with a nonporous acid/etchant resistant metal
54610. Cleaning rust from iron siding
54611. How to Recover Silver and cadmium from used HNO3
54612. In house test for SS 304
54613. Controlling fumes from hot dip sheet galvanizing kettle
54614. Can't get required 100 micron coating when galvanizing with Galfan zinc alloy
54615. Zinc plated screws are failing salt spray test
54616. How to preserve polished steel
54617. Need anodizing for some car parts in Austin {3/24/10}
54618. Requirement of Ion exchange/Resin column {3/24/10}
54619. How to remove nickel oxide by simple chemical method
54620. Chemical equation for pickling of steel with acid
54621. Spanish-style aged/rusted finish to mild steel balusters
54622. PMMA-coated PC failure camera
54623. Surface activator for adhesive bonding of stainless steel
54624. Surface preparation of stainless steel for re-painting camera
54625. Problem with electroless nickel deposition on carbon fibres
54626. Galvanic corrosion of zinc plated steel bolts on aluminum parts?
54627. Effect of sulfur content of 304 ss on electropolishing
54628. Polishing large (4 ft dia.) SS 304 spherical surfaces camera
54629. Want Kuwahara bike frame and forks electroplated {3/24/10}
54630. Looking for copper conductive paint in Mumbai {3/24/10}
54631. 304 ss wire needed {3/24/10}
54632. Need sterling silver galvanization for metal pieces up to dia 75 cm {3/24/10}
54633. Can you plate zinc on a roll of stainless steel?
54634. Nickel sulfamate plating without depolarized nickel
54635. Air agitation energy consumption/costs
54636. Hydrogen embrittlement due to NaOH?
54637. Powder coating over vinyl wash
54638. Nickel and aluminium content for galvanizing startup?
54639. Brighteners for electroless nickel plating
54640. Chrome plating run-out
54641. Contamination limits for Woods Nickel Strike
54642. Cad plating and sil glyde
54643. Instructions for black rhodium plating
54644. Plating for fixtures exposed to mineral oil
54645. Adhesive that will survive anodizing
54646. How to avoid flow marks in electropolishing process
54647. Want Fishing Reel Side Plates Painted Pink {3/26/10}
54648. Seeking Black Zinc Rack Plating of 1010 Steel {3/26/10}
54649. Want to buy a hot dip tinning machine {3/26/10}
54650. Why do we get low phosphorous electroless nickel with basic bath and high phosphorous with acidic bath?
54651. How to clean Lead Coated Copper?
54652. What does CASS test results mean relative to durability in years
54653. How to formulate a Pewter Patina
54654. Best type of brass for chrome plating
54655. Recasting zinc anodes from zinc rounds
54656. What is the reason pure tin plate discolored after aging
54657. Silver versus tin plating of copper for 480 volt switchgear
54658. Zinc phosphating bath is turning very dark green and non functional
54659. Remove scale from hot rolled steel stairs in prep for gun-bluing
54660. Need JS 500 BLACK finish on fasteners {3/29/10}
54661. Need Stainless Steel auto window trim Chrome Plated {3/29/10}
54662. Need magnesium motorcycle swingarm stripped and recoated {3/29/10}
54663. Want my Antique Brass PO BOX Doors silver or pewter plated {3/29/10}
54664. Black Oxide on Bronze and Stainless Steel {3/29/10}
54665. Need vendor in Minnesota for NADCAP AMS-2700, Type VII or VIII {3/29/10}
54666. Need chrome-look coating paint {3/29/10}
54667. Need Used Vacuum Cadmium Chamber Needed {3/29/10}
54668. Plating iron onto iron with a transition to the anode becoming silver(and/or copper)
54669. Type III (hard) aluminum anodizing, sealing and surface properties
54670. Crystals developing on solder/copper areas camera
54671. BLISTER FORMATION AFTER FEW DAYS OF ALKALINE ZINC PLATING
54672. Belated blisters in alkaline zinc plating
54673. Hard chrome plating for food processing
54674. Need Uniform and Very Heavy Zinc Phosphate Coating for Drawn Wires
54675. Reaction between black oxide finished s.s. screws, and Cor-ten (weathering steel) sheeting
54676. Need black coating on stainless
54677. Need Clear Coating and Dying Techniques for Structural Steel
54678. Itching from handling black oxided parts
54679. What causes blisters in chrome plated plastic parts
54680. Yellow chromate doesn't look like full gold
54681. Anti tarnish treatment for old silver flatware
54682. Optimum anode to cathode distance?
54683. What liquid causes hands to wrinkle the fastest
54684. Is melting zinc pennies with a torch hazardous?
54685. For fasteners that will be zinc plated, is a pretreatment of black oxide a problem?
54686. Masking Small Parts for Plating
54687. Aging new nickel-plated guitar tuners
54688. How to remove two coats of paint and primer off of enamel or porcelain coated patio table?
54689. Hi-phos hard nickel plating over epoxy?
54690. Alternative to anodise?
54691. Need Rigid Almite Coating on 6061-T6 Aluminum {3/31/10}
54692. What solution to use for etching of 20 Mn Cr 5 samples?
54693. What galvanic potential is used for chromate conversion coated aluminum?
54694. Want to seal a beautiful distressed metal table
54695. Substitute for sulphuric acid for electro polishing stainless steel
54696. Rhodium plated or silver plated - what is the best?
54697. Looking for a vendor in SEATTLE, WA to head coat screws {3/31/10}
54698. Metal Roofing Repair
54699. Need a low maintenance finish to keep galvanized corrugated roofing shiny camera
54700. How to reduce COD
54701. Zinc Trivalent - Yellow Dye Co-Deposition vs. Post Passivate Application
54702. Need to have hard urethane parts electro plated {3/31/10}
54703. Sublimation coating for chrome steel
54704. Tin, Lead, Copper Plating need for bronze bushings {4/2/10}
54705. Allergic to Nickel Sulfate and Black Rubber Mix
54706. Comparing options for clear finish on mild steel handrails
54707. How to Dull Bright Polished Steel Knife Blade
54708. How to strip nickel (electroless) off steel parts?
54709. Dichromate for hot-dip galvanizing
54710. How to verify passivation treatment of Ti alloy?
54711. Appropriate micron level for anodizing
54712. Need Electroless nickel / Electrolytic hard gold plating {4/5/10}
54713. Need Type III Hard Anodizing (Black) {4/5/10}
54714. VERY HIGH FLOW HYPOCHLORITE GENERATOR {4/5/10}
54715. Patina recipes for bronze vegetables and fruit
54716. What's the right size rectifier for copper electroforming?
54717. HCl scrubber that doesn't need water
54718. Electro galvanized coating thickness
54719. Need help making 6 stage iron phosphate bath last more than 6 weeks
54720. Need Phosphoric Acid Anodize per BAC5555 {4/6/10}
54721. RoHs Compliant Zinc Plating
54722. Alodine 1200s: How do I get class 1A AND class 3?
54723. New plant for rotogravure cylinder unit {4/6/10}
54724. Etching a design in aluminum
54725. TT-F-325 ENGRAVING FILLER PASTE REPLACEMENT
54726. How to set up Hard Anodizing line
54727. How to deal with waste nickel solution
54728. Leopard print effect on re works
54729. Need Hard Anodizing Service {4/6/10}
54730. What will dissolve a miniature steel screw in brass clock plate
54731. Hobbyist needs a very hard finish for a fretless bass fingerboard
54732. Newly Blued firearm rusted in under a week
54733. Making thread gage for preanodizing of internal threaded part
54734. Want Jeep steps (stainless steel) powdercoated or painted black {4/7/10}
54735. Need several epoxy resin bars repaired {4/7/10}
54736. Corrosion Rates and PH Levels
54737. Flow of air in a small paint spray booth
54738. Nonaqueous Plating of Si, W, Ti ?
54739. Need black nickel plating of Foose wheels {4/8/10}
54740. Heat Treating 4130 Steel
54741. Yellowish spots after wave soldering process
54742. What happens in salt bath nitriding if temperature exceeds 580 C?
54743. How to prevent sludge formation in 80 deg C caustic bath
54744. Determination of tungsten in Ni-W-P
54745. Blue chromate and staining
54746. How can I get maximum copper plating deposition?
54747. Need to anodize a part that is 152" long - Midwest USA {4/7/10}
54748. Need Zinc-Iron Plater {4/7/10}
54749. Need a grinding blade with Course grit Diamond composite coating {4/9/10}
54750. LOOKING FOR QUALITY FINISHERS IN DELHI {4/9/10}
54751. We need small amount of Potassium Cyanide (KCN) for tin types {4/9/10}
54752. Life Span of Yellow zinc plating Vs CR3 (ROHS compliance)
54753. Peroxide-sulphuric bright-dip for brass wire becomes saturated with copper
54754. Freshness of electroless nickel bath vs. speed
54755. Will Nickel plate to Tin? What about Lead?
54756. How can I fully restore the plating on old watch bands?
54757. Seeking detailed info on anodising and dyeing copper
54758. Cleaning 6AL4V titanium plate after grinding
54759. Grit on Bright Nickel Electroplated Polished Brass Parts
54760. Biocombatible paint for medical devices
54761. Seeking Zinc Oxide Manufacturer in {4/12/10}
54762. Thermal Sprayed Aluminium
54763. Zinc Black Chromate changes during shipping
54764. Cleaning up a lexan window
54765. Need informatin on Rose Gold, White Gold, Yellow Gold plating.
54766. Electroless copper plating on PVC pipe
54767. Please suggest a black finish for brass
54768. Low embrittling cadmium plates for corrosion
54769. CRCA vs GPSP steel as a substrate for powder coating?
54770. Tin plating over nickel plating on brass oxidized to black problem over tin plating
54771. I want the formula for bright copper plating
54772. Finishes Safe for Domestic Birds
54773. Breathing acid fumes for 15 hours left me sick
54774. Aluminum sticks to ruby spheres like it's an aluminum magnet
54775. Black Chrome plating on ABS Plastic
54776. Caustic Etch Analysis-aluminium anodizing
54777. Gravure printing ON - not WITH - steel
54778. Need brass bed polished and lacquered (Sacramento CA area) {4/13/10}
54779. Need MIL-PRF-85285 Painting {4/13/10}
54780. Acceptable Color Variation on Anodized Aluminum Products
54781. Need PVD coating in Monterrey {4/14/10}
54782. Grammatical question regarding Iridite?
54783. Stainless steel turns black after post weld heat treat
54784. Seeking Black Nickel or Black Rhodium Plating for jewelry {4/14/10}
54785. How is tungsten carbide jewelry blackened?
54786. Best method for Color Coding music wire springs
54787. Seek various finishes on brass tubing and fittings {4/14/10}
54788. New structural steel plant needs hot dipped galvanizing service {4/14/10}
54789. Need OEM temporary protection adhesive for painted parts {4/14/10}
54790. Want to build new eco-friendly galv plant {4/14/10}
54791. Removing Easy Off cleaner from black iron on my Harley
54792. Will a magnet stick to sheet metal after I paint it?
54793. Russian sourced kitchen tap valve internal plating delamination. Health hazard? camera
54794. Plating Leaded Stained Glass Pieces
54795. Galvanic compatibility and plating materials
54796. Post blue zinc plating defect -- rough texture
54797. How can brass (an alloy) be electroplated?
54798. Reflector coatings for IR lamp
54799. Is Zinc plating QQ-Z-325 Type I, Class 2 RoHS Compliant
54800. Need coating of a set of Dirylite {4/15/10}
54801. Electroless copper plating on PVC cylinder {4/15/10}
54802. Can old Refrigerator Grill type shelf racks be used as BBQ grills?
54803. Stopping the 'bleeding' of high carat gold through rhodium plate
54804. How would I deburr a Dremel-opened minikeg?
54805. Quantitative analysis of Saccharin in Nickel Plating Bath
54806. Heat Treating and Magnetism in 400 Series Stainless
54807. Prepare for electrical bond per HP14-30?
54808. Salt Spray hours on Zinc
54809. Want translucent color on nickel plated ABS parts
54810. Fluxing steel prior galvanizing
54811. Any alternate electroplating salts which can give silver colour?
54812. Brown spots on zinc plated tube camera
54814. Can't get required anodizing thickness on A380 casting
54815. Preparing a tank surface for use in food processing
54816. Pinhole defects on the buffed stainless steel strip surface
54817. Red fish hooks...how are they colored?
54822. Black Trivalent Chromate heat resistance
54823. Galvanneal horse trailer? camera
54824. Deburring machined brass and copper parts
54825. Unable to achieve paint adhesion over cad plate
54826. Can't electroform gold all the way into the corners camera
54827. Very hard dark grey corrosion on cast iron!
54828. Tube Material for ordinary surface condenser
54829. Seeking High Reflectance Aluminum Plating
54830. Copper vs. cast iron for a fire pit?
54831. What is the most durable option to apply color to 304 stainless steel gate latch?
54832. Color matching hardcoat aluminum with Teflon
54833. Antique Tin Ceiling Refinishing camera
54834. Chromium electroplating of carbon fiber
54835. Fatigue concern with hardcoating 6061 twice. camera
54836. How can I make plating solutions safely
54837. Testing "Distilled water" for its "purity"
54838. New Truck Detailer - Need Pros' Help
54839. Why did Thermal Zinc Coating shrink my fasteners?
54840. Best aluminium for gloss black anodising?
54841. Hard chrome plating needs microscopic bubbles
54842. Surface finish improvement in barrel tumbling process
54843. Surface roughness after hard chrome plating
54844. Is Immersion Copper Plating Real?
54845. Corrosion removal - tin plated cans camera
54846. Gold Plating with Hoover and Strong Solution
54847. 50ish Mercury coupe baby buggy? camera
54848. Repairing scratches on Corten Steel sculpture due to rough handling in transport
54849. Best marine finish for cast A380 part camera
54850. Can you powder coat over a black oxide finish?
54851. Alternative to Electroless Nickel Plating
54852. Need to refinish scratched porcelain stove top
54853. Deterring corrosion on aluminum alloys (Bravo III outdrive) camera
54854. Avoiding peeling in painting aluminium castings for motorbikes
54855. Seeking plating/aurora finish on multiple small paintball gun pieces
54856. Seeking Bright Dip Anodizer
54857. Need Nickel S pellets
54858. Gas Burner Grate on Wolf Stove is rusting
54859. Microwave HotPot fusing oven
54860. Is mixing galvanized roofing with aluminum roofing a galvanic problem?
54861. Replacement for Alodine 1201
54862. Baked/Washed metal frames won't take a powder coat finish. Need help!
54863. Black Oxide on stainless steel: appearance/wear resistance?
54864. Test "kit" for sulphuric acid pickle solution
54865. Simple test for galvanized metal
54867. Spots appear on zinc plating after 48 hours under normal environment
54868. Oxidation on stainless steel chain
54869. Medical Implant and Instrument Passivation
54870. Trying to match welded and unwelded stainless steel finishes
54871. Plater to replate the components of 6 identical scuba regulators
54872. Need Drylac 144/90052 Black Smooth Matte 25-40
54873. Electroplating Zinc onto a Penny
54874. Is my ring, marked "10k PB", gold plated lead?
54875. Muriatic acid as wood bleach?
54876. Determination of phosphate (TSP) in neutralization bath
54877. Need to remove chrome and nickel plating from Eagle alloy wheels
54878. Stripper for acid copper plate off of zinc die castings
54879. Hot Dip Galvanising of fabricated sheet metal assembly
54880. Want our brass finish to be green-yellow
54881. How to increase Chrome plating hardness
54882. Zinc Clear over Nickel Plated Brass - Salt Spray Test Failure
54883. Masking for plating rhodium over shell and soft stone
54884. Cleaning and passivating 316 stainless cables near the ocean using Naval Jelly?
54885. Grit blasted finishes on 300 series stainless steel
54886. Need vacuum cadmium plating
54887. Need Gold Plating of large cylinders
54888. Is Chroming of Rubber Possible?
54889. Want to know how to Electroform a non Metallic Object
54890. Sterling Theda?
54891. Performance of an SCR rectifier vs Tap Switch
54892. Using a former fuel oil tank as a DM water tank
54893. Salt spray testing assembly with both zinc plated and galvanized components
54894. Nickel pellets vs. S-rounds
54895. Yellow chromate for Cad, Zinc and Zinc/Nickel
54896. Pitting on antique brass finishing
54897. Galvanic potentials: SS316 Vs Duplex stainless steel
54898. Need polishing from 45 RMS to 5 on tool steel
54899. Need nickel or chrome coating of plastic beads
54900. Electroforming gold jewelry on copper, and can't remove last traces of copper
54901. 925 Pandora bracelets sold on Ebay are turning red camera
54902. I gold plate car emblems but now encounter plastic ones
54903. Lightweight alternative to copper enameling? camera
54904. Is Stainless Steel finish or Black Oxide on Stainless more durable?
54905. Can torching galvanized rails cause seizures
54906. Pot left on the burner for 6 hours; are the fumes dangerous to your health?
54907. Regeneration and Passivation of Used Titanium Cathodes
54908. Powder coating over galvanized steel and cast iron
54909. Camouflage powder coat?
54910. Welding galvanneal
54911. Adhesion failure plating electroless nickel on F357 Casting
54912. Plating 1095 spring steel for fresh water lake area protection
54913. How to tell if chemfilm was done camera
54914. Want to set up a plant for colour anodizing
54915. Want to know how to do two-color anodizing
54916. Melonite / SBN process for highest wear resistance?
54917. Chemical percentage and process of stainless steel,carbon steel,monel,inconal,hestalloy,alloy steel in tube product
54918. Robotic slot finishing with abrasive cords
54919. Mirror Polishing HSS M2 plates
54920. Corrosion and wear resistant coatings for copper? Also for Zinc? Other material?
54921. Seeking nitric passivation of Ti-6Al-4V implants
54922. Need hard anodizing of very long parts
54923. Need Dry Lubricant applied per Mil-L-46147
54924. Will trade 6000 amp rectifier for a smaller one
54925. Need plating equipment, buffing equipment and solutions
54926. Dip Spin machine needed
54927. What is "Hard Silver Coating" vs. Silver Plating
54928. Creating a rusted pattern on fabric camera
54929. Artistically painting a decorative metal wall clock camera
54930. Paidar 1920's porcelain Barber Chair
54931. Process Similar to Aluminium Anodizing but for Zinc?
54932. Chrome-look spray application
54933. Electrolytic reaction - aluminum with stainless and brass
54934. Which electroplating machine is best?
54935. Recovering the zinc from zinc dross
54936. Inspecting E-Coat on sunroofs
54937. Can't get good Black Oxide on reworked parts
54938. What are the restrictions on Hot Dip Galvanizing in
54939. Why is Hot Dip Galvanized coating thickness dropping?
54940. Copper Contamination in Cadmium Plating Baths
54941. Difference between copper anodes with phosphorous content
54942. What is the normal color of duplex sealing of MIL-A-8625 type 2 class 1 parts
54943. Zinc Phosphate grain problem
54944. Does tumbling with alumina create issues for later welding of 304 stainless steel parts?
54945. Overused tack cloth made oak floor tacky
54946. Need Cold Black Oxide close to Northern Indiana
54947. Need vitreous enamel and selective coating plant for aluminium sheet
54948. What is the white rust in aluminum alloys composed of?
54949. Why is rhodium plated onto gold jewelry instead of onto less expensive metals
54950. Metal finishing issues in classic car restoration
54951. Need a local certified provider to rechrome my 1971 Dodge Challenger bumpers
54952. Can anodized wheels be chromed or powder coated?
54953. Gold plating vs Silver plating for electrical contacts
54954. Flowmarks along anodized part camera
54955. Need grill rechromed
54956. Need venetian mirror re-silvered
54957. Looking for suppliers in North East Mexico with zinc plating capabilities
54958. Need pure lead plating on an inconel vacuum seal
54959. Chroming a header pipe for a bike camera
54960. Need information on non-cyanide jewelry bombing camera
54961. Black Stains after Electropolishing of 410 SS camera
54962. General Metal Finish Selection
54963. Wear resistance of chromate over cadmium
54964. Pretreatment for Electroless Nickel (EN) on Brass
54965. Material differences: CRCA and 5052
54966. How to restore chrome commercial faucets?
54967. Undisputed best coating system for high volume small stamped steel parts?
54968. Improving surface finish on 6061 Aluminum Anodized bore
54969. How much will it cost me to start photo chemical etching?
54970. How do I create a pitted and corroded finish on 420J Stainless Steel? camera
54971. Bubbles and Blister formation during trimetal plating
54972. Bright Dip will be my downfall!
54973. Which is good process: buffing vs. glass beading
54974. Ventilation requirements for plating shop
54975. Need cleaning chemicals for copper-lead-zinc sintered products
54976. Mysterious Black Nickel Plating on Copper
54977. Aluminum pool coping is pitting and rusting
54978. One-part vs. two part epoxy for fiberglass boat?
54979. Decoration technologies to apply over chrome plated plastic
54980. Want satin crystalline finish from anodizing camera
54981. Typical finished color for MIL-A-8625F Type III anodize of 7075-T6 material
54982. Black electrophoretic vs. black chrome finishes
54983. Need anodizing shop that meets AAMA612
54984. Need compartmentalized stainless tank for etching aluminum
54985. Anodizing motorcycle clutch basket with non-removable steel components
54986. My white gold ring did turn black camera
54987. Analytical technique for confirmation of 49% HF solution
54988. Using Zinc Plated Nuts on Galvanized Bolts
54989. Temperature of Hard Chrome Reverse Etch
54990. Cycle for the preparation of polished cast iron prior to hard chrome plating
54991. Round White Spot after Anodising
54992. Copper Plating Matte - Colored Result
54993. Cleaning calcium deposits out of industrial drain lines
54994. Is there a special coating for Steam Coils in Zinc Phosphate System to help remove build-up
54995. Design studio needs 29 serving tables plated or blackened camera
54996. Differentiating between HDG and SB?
54997. Is it possible to coat Aluminium and Stainless steel with a food grade polymer
54998. Rust Preventive Oil in Hot Dip Galvanizing


The finishing.com Hotline has been on the Internet since '95 and includes more than 50,000 threads about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to: start at our home page, view the most recent letters, or search the site.


© finishing.com, inc., 1995-2012