51000. After effects of H2O2 addition to
waste water [India]
51001. Need yellow trivalent chromating
[United States]
51002. Searching for a technical document
describing how tin plating reacts in a humid environment
[Illinois]
51003. Passivating heat tint areas
[California]
51004. I want to paint my chrome the same
color as my bike, how? [New Mexico] ![]()
51005. How to soften steel after
welding [Florida]
51006. Ask a suggestion for a corrosion
prevention on mild steel [Sri Lanka]
51007. Copper has oxidized to black
color [Italy]
51008. Setting up a small scale nickel
sulfamate bath in a university [New Zealand]
51009. Bathing resin castings in precious
metals -- what's it called and how do you find out about it?
[Vermont]
51010. Rubber roller for tape test
[California]
51011. Delayed flaking on crimped parts
[Michigan]
51012. Watts nickel bath contaminated with
hydrazine [Indonesia]
51013. How to tell gold anodize from gold
chromate? [China]
51014. How to tell white brass from
aluminum bullet cases [Illinois]
51015. Steel anode baskets are gassing in
tank [Louisiana]
51016. Cleaning and preparation of metals
for plating [Canada]
51017. Need brass redipping [New
Jersey]
{1/23/09}
51018. Seeking plating, surface
finishing [California]
{1/23/09}
51019. Temperature/Discoloration Data
Needed for 304 Stainless [Washington]
51020. What conductivity setting for
Caustic Etch Rinse Tank? [South Dakota]
51021. Tri-chrome or chrome-free Brass
Iridite? [Minnesota]
51022. Rubber to metal bonding with Viton
B [Texas]
51023. Black oxide on Tribaloy T400
[New Zealand]
51024. Galvalume Blackening without oxygen
deprivation [Indiana]
51025. Electroless plating?
[Malaysia]
51026. MIL-DTL-5541 Failing Humidity
[Washington]
51027. Causes of streaking in machined
7075-T6 aluminum [Taiwan]
51028. Manganese Phosphate Coating
Thickness [Colorado]
51029. Cost of type 2 versus type 3
anodize [Texas]
51030. Cost cutting in powder coating
finishing [India]
51031. Etchant for copper weld surface
after mechanical cleaning? [Turkey]
51032. Material recommendation for pump
shaft for salt water usage [India]
51033. Stainless Steel Brush Finish in
Aluminium Profiles [India]
51034. Zinc Coating 210 litre / 55 gallon
drums [South Africa]
51035. Alodine? Chromating Alum tubes.
[Illinois]
51036. History of Parco-lubrite, zinc
phosphate, and manganese phosphate coatings [New York]
51037. Experience with chrome additive
[Canada]
51038. How to protect a nickel plated
shower drain from tarnishing? [Texas]
51039. Construction manager wants "GO
SAINTS" painted on new galvanized gymnasium roof [California]
![]()
51040. What effect does soda have on
pennies mass/weight? [Virginia]
51041. Rhodium plating white gold and
Titanium ring [Australia]
51042. Galvanized Steel fumes making your
skin smell [Minnesota]
51043. 250 micron Nickel Deposit With High
ductility and Low hardness(175HV) [India]
51044. What is the best plating process for
general purpose military electronics enclosures [Maryland]
51045. Sodium Dichromate passivation
question [Indiana]
51046. Need amyl nitrite durules/suppliers
list in India [India]
{1/27/09}
51047. Submerged hook for anode sheets
? [Australia]
51048. Hazards of gas evolution from nitric
titration? [England]
51049. Cr(VI) Exposure from Grinding Hard
Chrome Plated Steel [Minnesota]
51050. Sludge problem in anodizing line
[Turkey]
51051. How to remove cured epoxy adhesive
from stainless steel [Minnesota]
51052. Wax coating on stainless steel
fasteners [India]
51053. Powdercoating certification
school? [Utah]
51054. Electroforming Bath operate at room
temperature [Iraq]
51055. Can I redo Zinc plate chromate?
[England]
51056. Hard black problem
[Philippines]
51057. Steels specified for hot Ferric
Chloride solutions [Zimbabwe]
51058. Dissimilar metals attack hurricane
shutter industry [Florida]
51059. Recovering Gold from Used Gold
Bath [India]
51060. Plating on coil, music wire
springs? [Australia]
51061. Why not plate gold follow with tin
plating? [Malaysia]
51062. Acid copper is behaving uniquely
[India]
51063. Shadows in nickel electroforming
[New Jersey]
51064. Gold Chem-Film Finishing Different
Shades [Iowa]
51065. Anodized Stainless Steel Coil?
[Illinois]
51066. Aluminum gassing out during powder
coating operations [Indiana]
51067. Steel tubes Chromium detachment
under compressive loading [UK]
51068. Results and disposal of materials
stripped from....... [Nebraska]
51069. Chrome plate aluminum [Florida]
{1/29/09}
51070. I want to get scratches out of glass
on the front of a mirror [Minnesota]
{1/29/09}
51071. Seeking JWI Sludge Dryers
[Michigan]
{1/29/09}
51072. Contractometer for Stress
Measurement [Illinois]
{1/29/09}
51073. Need Silver Brightner (black
powder) [India]
{1/29/09}
51074. 420 Stainless Steel Appearance
Standard [Mexico]
51075. I need a new method for refining
gold from my factory's floor dust? [India]
51076. Solder Reflow Problem with nickel
underlayer- silver plating [Turkey]
51077. Aluminium for watch cases
[India]
51078. How to mask [Texas]
51079. Coloring Stainless Steel
[Pennsylvania]
51080. Galvanizing Zinc Splashes
Problem! [Egypt]
51081. How to make copper look like
wood [Canada]
51082. Powder coating(texture) [Iran]
![]()
51083. How to paint a CorTen Transport
Container? [New Jersey]
51084. Our job requires sandblast and zinc
painting of tube steel 10 x 7 x 30' [Washington]
{1/30/09}
51085. We need Mil Spec Black Oxide
Fasteners [Illinois]
{1/30/09}
51086. Air trapping in CED Coating
[India]
51087. Activating and sensatizing graphite
for electroless copper without palladium [India]
51088. Need brass tinted lacquer
[Arkansas]
51089. Need 0.001" zinc plating on MS
screws, even the heads [India]
51090. Need refinishing for brass floor
lamp [New Jersey]
{1/30/09}
51091. Seeking zinc plater for large steel
machine frames [Connecticut]
{1/30/09}
51092. Seeking 2.5 mil Cu plating of 30
pcs. of 316SS aprox. 10"X12"x3/16" [New York]
{1/30/09}
51093. Plating zinc on brass wire
[India]
51094. Electroless nickel as applied to
aluminium ? [Mexico]
51095. E-Nickel Plating for pump cylinder;
thermal cycling [Oregon]
51096. Nickel plating of ceremonial spurs -
how thick should it be? [Canada]
51097. Non toxic, less labour intensive
precleaning of cold blackodising components. [India]
51098. Mil-C-5541, Class 1A, Type II RoHS
Compliant [Minnesota]
51099. SouthWest Spring Mfg'er seeking shot
peening provider [Texas]
{2/2/09}
51100. Seeking a Used Thermal Deburring
Machine [Illinois]
{2/2/09}
51101. Electroplating Aluminium Oxide onto
Nichrome Wire - help me please [UK]
51102. Gold-Copper Alloy Plating--How to
control the relative deposition? [UK]
51103. Estimating Rectifier Operational
Costs [Hungary]
51104. Hydrogen Embrittlement
[Pennsylvania]
51105. What should be ED and UF parameters
for a low turn over ED bath [Pakistan]
51106. White rust after powder coating hot
dip galvanized steel [New Zealand] ![]()
51108. Chrome Plating that is pitting, but
not "gas pits" [Illinois]
51109. Blackening treatment of SS 316 / 304
for best solar absorption [India]
51110. Manganese phosphate problem
[Iran]
51111. How to achieve black colour
phosphating [India]
51112. Dacromate coating vs. Dacromet
[Qatar]
51113. Galvanizing and powder coating of
Lighting Poles [UAE]
51114. Grainy look under my polished
stainless steel [Michigan]
51115. E - COATING of jewelry
[India]
51116. Time limit before baking for
hydrogen relief [Washington]
51117. Plated gold ornaments gets black or
brown on handling or exposure to atmosphere [India]
51118. Strip Edge Wiper [India]
51119. CLOUDY LIKE APPERANCE ON CHROME
PRINTED CYLINDER [Philippines]
51120. Company that can coat and hone a
rotary housing [Canada]
{2/5/09}
51121. How to etch nickel over copper
substrate [Hong Kong]
51122. I think I was cheated on E Bay
[Pennsylvania]
51123. Plating to solve current
leakage? [Honduras]
51124. Need kit for Platinum Coating on
Copper [Canada]
{2/5/09}
51125. Need a shop to do Red Anodize color
match [California]
{2/5/09}
51126. Chrome plating aluminium please help
update [Poland]
51127. Conductive Stainless Steel Plating
Question [Ohio]
51128. Low pH at the dm plant
[India]
51129. PVD Aluminium corrosion issue
[Canada]
51130. How to remove scratches from
stainless with a clear coat on it? [California]
51131. Exterior mild steel sealant
[California] ![]()
51132. Metal rusting in alcohol water
[Utah]
51133. Electroplating [Ohio]
51134. Common filter paper must not be used
for filtration of boiled potassium permanganate solution
[Ghana]
51135. Characteristics of chromium plating
wastewater [Philippines]
51136. Inhaled hydrochloric acid [West
Indies]
51137. Chrome removal [Delaware]
51138. Looking for the best/easiest way to
patina several very large brass pieces [Texas]
51139. Bright finish [New Jersey]
51140. Diamonds? [Canada]
51141. Article "Small Precision Aluminium
Alloy Sand Castings" by Gerald Smith [Washington]
51142. Why is the cost of Zn electroplating
given by Rs/kg( weight of sample) and not Rs/sq.feet [India]
51143. How to clean filter press
effectively? [Malaysia]
51144. PH adjustment in a Nickel electro
bath [France]
51145. How to strip "hang" the steel needs
to be galvanized? [Egypt]
51146. Sandblasting 4130 chromemoly
[Ohio]
51147. POROSITY IN ALUMINIUM COMPONENTS
[India]
51148. Electroless Au plating on Au
[France]
51149. Electroplating onto bismuth
[Wisconsin]
51150. Electropolishing of tin silver
alloy [India]
51151. Help With Blast Abrasion of Hardened
Steel [Colorado]
51152. Solar Application [Colorado]
51153. Replating silver on tuba
[Illinois]
{2/9/09}
51154. Need supplier for TSH7702G
plating [Kentucky]
{2/9/09}
51155. Seeking black oxide finisher
[New York]
{2/9/09}
51156. Need hot dip galvanization
equipment [Yemen]
{2/9/09}
51157. Rhodium plating/polishing and
sterling silver [Tennessee]
51158. Choose a copper or a stainless steel
chimney cap? [Tennessee]
51159. Electroplating stainless steel
buckles [India]
51160. G609 black anodized aluminum
alloy [New York]
51161. Copper Roof over bay window
destroyed by brick mortor acid wash? [Colorado]
51162. FV520B materials and heat
treatment [England]
51163. Red residue problem with
conventional hot black oxide (280 - 290 F) [South Carolina]
51164. Problem in heat treatment of
electroless nickel plating [India]
51165. Plating and Clear Coat Die cast zinc
to emulate 430SS [Tennessee]
51166. Does X15TN Stainless Steel need to
be passivated, if so what "group" does it fit into? [Oregon]
51167. Orange peel effect from
electropolishing [Tennessee]
51168. Product design
[Massachusetts]
51169. Bronzed Brass Plating [India]
{2/10/09}
51170. Need 4 steel chair frames
replated [New Jersey]
{2/10/09}
51171. I NEED HELP ABOUT STEEL UTENSILS
POLISHING MACHINE [India]
{2/10/09}
51172. Industrial Waste Assignment
[Ireland]
51173. Spray pyrolysis [UK]
51174. Flash Gold Electroforms are more
bonded to the mandrel than Nickel Electroforms? [Philippines]
51175. Want to chrome dip the grille on my
truck [Florida]
51176. SS202 or 304 Kitchen Baskets - Which
is recommended? [India]
51177. Gold plated silver dollar
[Florida]
51178. Disadvantages of h2o2 treatment in
refinery waste stream [India]
51179. Determine the rochelle salt of an
alkaline copper bath [Mexico]
51180. Plating on Plastic was cracked
[Vietnam]
51181. Why Polypropylene Bags??
[Massachusetts]
51182. Electroplating haze causes on
plastics [Australia]
51183. Copper Plating [Alabama]
51184. Hard chrome for pure copper
process [China]
51185. Electroforming Bath operate at room
temperature [Iraq]
51186. How to control line length in a
brushed finish? [Florida]
51187. Anodize - satin mask, black [New
Hampshire]
51188. Passivation [Mexico]
51189. Electro polishing of brass part
[Iran]
51190. Pure copper part done by cnc
process [China]
51191. SS 304 or SS 316 for the purified
storage tank in the R.O. plant [Egypt]
51192. Long term corrosion of 416 SS in a
medical device [Florida]
51193. Can an N9 or N7 Surface Finish be
achieved by a planar machine [Pakistan]
51194. Dacromate Coating/Plating
[Singapore]
{2/11/09}
51195. Photo Resist Dry Film [UAE]
{2/11/09}
51196. RoHS compliant chem film in a
touch-up pen? [Canada]
{2/11/09}
51197. Carbolux Unit [Minnesota]
{2/11/09}
51198. Looking for Cad oxide [Florida]
{2/11/09}
51199. How do I stop a copper
electroforming solution from peeling or curling away from glass
surfaces [South Carolina] ![]()
51200. Heating the fluxing solution
[Saudi Arabia]
51201. Aluminum Plating [Minnesota]
51202. RoHS compliance in chem film for
aluminum [California]
51203. Passivation of 420 Stainless Steel
and Color Changes [California]
51204. How to identify visually process
finishes? [California]
51205. Need SS Polishing Media
[California]
{2/12/09}
51206. Black finish to replace cyanide
based current product [Australia]
{2/12/09}
51207. Best pretreatment steps for AZ63 Mg
alloy? [India]
51208. Paint a Steel Retaining
Wall/Seawall [Michigan]
51209. Bedliner-like spray paint?
[North Carolina]
51210. Nomenclature of Material
[India]
51211. Primer to powder coat 1008
steel? [Kentucky]
51212. Hydrochloric Acid Concentration!
[Egypt]
51213. Electroless nickel plating on
steel [Belgium]
51215. White Blemishes/Spots on nitric
passivated cobalt chromium alloy [Ireland]
51216. What type of barrel do you use to Cd
plate washers to prevent them sticking together [Michigan]
51217. Types of zinc used for
galvanizing [Egypt]
51218. EMC spring get bubbled after zinc
plating, look for solution, thank you! [China]
51219. Conductivity of bare Aluminum vs.
Chemical Convert [Colorado]
51220. Troubleshooting guide for fluoride
phosphate? [California]
51221. Factors to consider for new variator
motor in galvanizing plant [India]
51222. Maintaining a Surface Finish after
Anodizing [Minnesota]
51223. 3000 small brass screws need AS
4169-2004 plating [Indiana]
{2/13/09}
51224. Need test coupons and 4% HF / 18%
HNO3 acid solution for titanium etch [Mexico]
{2/13/09}
51225. How to extract silver from tin
dross? [Thailand]
51226. Art student looking to plate copper
onto steel [Texas]
51227. Remove gilding from rare silver
coin [UK]
51228. Coloring and etching aluminum for
organic look [New York]
51229. Microwave oven for baking e coat
[India]
51230. Turning copper sulfate into copper
and sulfuric acid [New Mexico]
51231. Is Iridite 17P RoHS compliant?
[New York]
51232. Liquid Nitriding over Chrome
plating [Canada]
51233. Plasma nitriding vs. ion
nitriding [Indonesia]
51234. Problem in hard chrome plating an
ID [India]
51235. Silver plating on female threads
[India]
51236. Sharpies, scorching, and drip
stains.... [New York]
51237. Paint is bleeding under our
masking [Georgia]
51238. SS304 Forging Rust [Ireland]
51239. Vibration finishing machine on SS 2B
finish sheet [UAE]
51240. Varnishing cast iron?
[Belgium]
51241. Friction material for spoon brake on
rubber wheels [UK] ![]()
51242. Colloidal Silica Removal from
Treated Effluent [India]
51243. Finishing Problems of Sculpture in
Copper Alloys [Virginia] ![]()
51244. REACH Regulations [Illinois]
51245. Testing procedure of purity
percentage for zinc oxide [India]
51246. Nickel plating inside of steel
tubing as a rust inhibiter [California]
51247. Bolts: strip chrome, re-plate, and
TiN coat [Texas]
{2/16/09}
51248. Need small benchtop lacquer curtain
coating machine [Minnesota]
{2/16/09}
51249. Nitric acid titration
[India]
51250. Quantitative Chem Film Testing
[Canada]
51251. Waterwheel hardware [Colorado]
![]()
51252. How to prevent golden colour in
stainless steel cookware [Spain]
51253. Trying to solder to chrome [New
York] ![]()
51254. Hazards of P-chloromercuriphenyl
sulfonic acid? [South Africa]
51255. Contractor looking for solution to
tone down the brightness of new Gavalume roof [California]
51256. How to prevent or minimize
electrolysis of water [Oklahoma]
51257. Do color chips work
[California]
51258. Chroming cycle fenders
[Wisconsin]
{2/16/09}
51259. Need gold plating removed from
stainless flatware [New York]
{2/16/09}
51260. Need roller coating machines for
coating grained aluminium plates for printing [India]
{2/16/09}
51261. Need Dacromet Solution [Qatar]
{2/16/09}
51262. Zinc boat anodes not doing their
job! [Australia]
51263. Adhesive to match stainless
steel [Canada]
51264. Help in Ultrasonic Cleaning
[Florida]
51265. How to weld 316L Marine Handrails
w/o discoloration [Texas]
51266. What metal are my doorknobs? And how
do I refinish them? [Pennsylvania] ![]()
51267. Chrome plating a tooth for
jewelry [California]
51268. Can I melt silverplate and skim the
silver from the top of the kiln? [Arizona]
51269. Cleaning galvanized tin ceiling
[Georgia]
51270. Iron PPM Analysis in zinc iron
bath? [Montana]
51271. Suitable cup for fused TinLead.
[India]
51272. New to powder coating. Seeking all
the info I can obtain. [Kansas]
51273. Looking for best paperback book for
the powder coating beginner [Kansas]
51274. Throwing power of ced paint
[Pakistan]
51275. 2 years finishing aircraft cable,
and consistency still eludes us! [Kentucky]
51276. Can bronze similar to SAE62 be TiN
coated or is the process temperature a concern? [Mexico]
51277. Pitting within hard chrome on
aluminium [UK]
51278. Centerless grinding of hard
chrome [Texas]
51279. Compare dual ni and triple ni
decorative chrome plating [India]
51280. Quality Problem [India]
51281. Need watertight seal between
anodized aluminum and molded urethane. [South Dakota]
51282. Cleaning for aluminium cycle to
avoid blisters [India]
51283. Is it possible to measure the
coating thickness after phosphatizing? [India]
51284. Lacquering and post treatment
[Pakistan]
51285. Paint chip off of fishing lures too
easily [Connecticut]
51286. Flame resistant applications...ie
Stove top grates [Illinois]
51287. Need bronze candelabra repair
[New Jersey]
{2/18/09}
51288. Brass electropolishing
[Iran]
51289. Urgently need to install a
galvanizing plant [Honduras]
{2/18/09}
51290. Need Platinum Cobalt Plating
[Ireland]
{2/18/09}
51291. Staining of zinc countertop
[Virginia]
51292. Hardcoat Anodizing - Surface Area
Calculation of a tube [Rhode Island]
51293. Can't get Zinc chromate
electroplating in thread [Philippines]
51294. Best tube material for Ammonia
Applications? [Saudi Arabia]
51295. Flash rust after drying in oven
[Missouri]
51296. Electroclean voltage/current
settings [England]
51297. Seeking Apple Aluminum Finish
[California]
{2/18/09}
51298. Refinishing chrome from an aluminum
snare drum [Massachusetts]
51299. Need chrome re-plating of steel
rings [Australia]
{2/18/09}
51300. Which drink contains more
electrolytes? [Saudi Arabia]
51301. Need MIL-DTL-83488 or AMS 2427
qualified suppliers [Texas]
{2/20/09}
51302. Plating Pt black on gold
substrate [California]
51303. Determining hardness of thin
anodisation layers [Netherlands]
51304. LOOKING FOR A NIKASIL OR COMPARABLE
PLATING COMPANY IN CHINA [China]
{2/20/09}
51305. Need PVD coating machine
[Pakistan]
{2/20/09}
51306. How to prepare the gold
solution? [Malaysia]
51307. Zincalume and galvanised iron
poisoning in tankwater [Australia]
51308. Diamond Like Coating - any info?
[North Carolina]
51309. Home Remedy for Stripping Chrome
from Aluminum? [Nevada]
51310. Want paint that looks exactly like
chrome finishing [Texas]
51311. Salt spray test failed when powder
coating perform on fabricated components braket areas and drain
holes [India]
51312. My nickel anode bags are stiff?
Why? [Pennsylvania]
51313. Aluminum surface finish
[India]
51314. Are Silicone Masking Plugs a
Threat? [New York]
51315. Best Stainless Alloy for Potassium
Hydroxide [Texas]
51316. Can we store concentrated sodium
hydroxide in zinc container? [India]
51317. Etchant required to etch h13 hot die
steel [India]
51318. Cracks after hard chrome plating on
ground induction hardened piston rods [India]
51319. How to finish, attach and hang
painted figure cutouts on a wall? [Canada] ![]()
51320. Artist wants to use silver x-ray
film [California]
51321. Poor Adhesion in Plating Nickel over
Aluminum [Mexico]
51322. HAE - Why bifluoride-dichromate
treat with moist heat aging? [Connecticut]
51323. Want zinc hot spray / flame spray
equipment [South Africa]
{2/23/09}
51324. Black chrome on motorcycles
[Pennsylvania]
{2/23/09}
51325. Replate Bathroom Hardware to Satin
or Polished Nickel/Chrome [Virginia]
{2/23/09}
51326. Occluding Quasicrystals in Nickel
Plating [Texas]
51327. Deep Aluminum Etching
[California]
51328. Silver potassium cyanide
preparation [India]
51329. How to do antique bronze finish
[Vermont]
51330. Can I use magnesium-based adsorbent
to treat remaining nickel in the wastewater with pH more than
9.5? [Vietnam]
51331. Stripping Copper off
Zinc/Aluminum [Rhode Island]
51332. Will porosity of aluminium lead to
blisters of pin size? [India]
51333. Treating Blemishes on Anodized
Aluminium [South Africa]
51334. What test equipment is available for
nitric acid and ammonium bifluride for stainless steel pickling?
[Kentucky]
51335. Need galvanized sheeting [India]
{2/24/09}
51336. Consultant needed - Removal of
Nickel in presence of other salts [California]
{2/24/09}
51337. Need to have steel bolt heads plated
to prevent corrosion [Pennsylvania]
{2/24/09}
51338. Concrete painted driveway needs a do
over [Oklahoma]
51339. Details of Bengough Stuart
Process [India]
51340. Is it possible to selectively
re-patinate worn away areas of black patination on brass
[England]
51341. SPOTTY/INCOMPLETE ANODIZE SULFURIC
BLACK [Massachusetts]
51342. Electroless nickel plating on brass
terminal [Malta]
51343. Need NC 11 etching chemical
[Hungary]
{2/24/09}
51344. Electropolishing Aluminum
[Maryland]
51345. Need brass plating of aluminum
part [Connecticut]
{2/24/09}
51346. Does 316L stainless steel get weaker
with repeated heating/cooling cycles? [Australia]
51347. Stripping Galvanize
[Australia]
51348. Metallic defects on chrome plating
thermoplastic part [France]
51349. What is needed to achieve Antiqued
Bronze Finish on plate steel? [South Carolina]
51350. Electropolishing chemistry and
procedure for nickel silver [Canada]
51351. Iron phosphating tank is leaking
[India]
51352. Color tone [Egypt]
51353. How to remove algae form the nickel
plating tank ? [India]
51354. Need re-chroming of my auto
wheels? [Florida] ![]()
{2/25/09}
51355. Requisition of electropolishing
solution for jewelry products (18Kt and 22Kt) [India]
{2/25/09}
51356. Need a 1" consumption meter for
chromic acid [India]
{2/25/09}
51357. Ni electroplating on steel from
Watts bath for nano research [Saudi Arabia]
51358. My rhodium necklace sticks to a
magnet [Canada]
51359. Protecting a Pool Skimmer Lid
against Chlorine [Oregon]
51360. Keeping copper coffee table
shiny [India]
51361. What does it mean to get a ring
dipped? [Arkansas]
51362. How do I blacken mild steel for use
in very high temps [UK]
51363. Need a ruined pot repaired [West
Virginia]
51364. Test of Zirconium in Chrome free
Passivation [India]
51365. Gold + Copper + Cadmium
separation [France]
51366. TDS vs PPM? [UAE]
51367. Convert weight percentage (EDX) into
ppm [Malaysia]
51368. Stripping agent for powder coats
[India]
51369. Stripping Copper-Nickel-Indium
alloy [Scotland]
51370. Need info on Powder Coating benefits
to Mitigate Heat [Arizona]
51371. Required Pretreatment before E
Coating [India]
51372. Galvanizing coating thickness for
Nuts [Saudi Arabia]
51373. Can't remove blue-black from
maraging steel for E-nickel plating [Iran]
51374. White rust questions [North
Carolina] ![]()
51375. For gemstone electroplating: How
delicate and thin can my copper electroplating lines be to later
plate with gold? [Thailand]
51376. Hard Chrome Plating on Inner
Surfaces [India]
51377. Pitting "Nickel material" for my
pipe NiCr Plating [Indonesia]
51378. White chalk like appearance on
aluminium cargo containers [New Zealand]
51379. Green "stain" on Black Aluminum
[Colorado]
51380. Finishing of Chromate Coating
[Malaysia]
51381. Trying to set up a chem film
line! [New Mexico]
51382. Important variables for ultrasonic
cleaning bath? [Mexico]
51383. Stainless Steel Pipes Used in
drencher systems for passenger ships [Jordan]
51384. Need corrosion expert to de-rust
machinery [Florida]
{2/25/09}
51385. Need equipment and process chemistry
for hard chrome on ABS [Saudi Arabia]
{2/25/09}
51386. The difference between corrosion and
oxidation? [Japan]
51387. Removing Aluminium Deposition From
Parts with base material: Aluminium [Malaysia]
51388. Polishing SS starting with 2B (2D?)
finish - initial step [Maryland]
51389. Bronzing bathroom fixtures
[Texas]
51390. Painting aluminum statues
[UK]
51391. REFINING USED GOLD PLATING
SOLUTION?? [Australia]
51392. A different Zinc/ Hydrogen
Embrittlement question [California]
51393. Retouch of hot-dipped galvanized
item [Philippines]
51394. Ni- PTFE coating vs. Ferrox
coating [India]
51395. Conductive layer for nickel
electroforming [Portugal]
51396. Problems with adhesion of chrome on
420 stainless steel [Virginia]
51397. Nickel plating peels off after
pressing [China]
51398. Etching Inconel 600 with Ferric
Chloride [Missouri]
51399. Corrosion on SS Tank
[Indonesia]
51400. Corrosion possibility between
galvanized steel and PE coated steel [South Korea]
51401. Use of Stainless Steel jigs to cut
out stripping after galvanizing [South Africa]
51402. Nickel sulfamate bath problem
[Texas]
51403. Need diamond welding rod used for
core bits of oilfield [China]
{2/27/09}
51404. What's our zinc level?
[Michigan]
51405. CPVC solvent was used on PVC pipes.
Is this okay? [Georgia]
51406. Bar-B-Que Heat Plate Materials
[Florida]
51407. Benzotriaole Removal [South
Carolina]
51408. Electroless Nickel is too smooth for
my needs, I need a rougher finish [Canada]
51409. Improve Brightness in Sulphamate
Electroforming bath [Mexico]
51410. Electropolishing of Aluminum vs
Bright-dip [California]
51411. Corrosion of anodized 7075 T73 vs
7075 T6 aluminum [California]
51412. Fastening a stainless steel frame
with galvanized rods and bolts [Canada]
51413. Can hot dip galvanizing be
misunderstood as electroplate galvanizing [South Africa]
51414. Removing silver paint from Cast Iron
Fireplace [UK]
51415. What is the best option, to use
spray chrome or reflexive powdering? [Indiana]
51416. Powder coating over insta-rust
[California]
51417. Specifying electroless nickel
thickness [California]
51418. Obtaining 600 hour salt spray for a
Zinc Clear, Chromate - Plate [Michigan]
51419. Matte tin finish vs bright tin
finish [New York]
51420. Need Food Grade Knives - etched with
our logo [Singapore]
{3/3/09}
51421. What is equivalent weight of B2O3
against 1.0 M NaOH titration [India]
51422. Flux regeneration plan
[Turkey]
51423. Problem Replating Electroless Nickel
on Aluminium [UK]
51424. Black dirty deposits at silver
plated parts [India]
51425. Effect of chlorine on SS304
[India]
51426. Need 86% Tungsten carbide high
velocity thermal spray coating [Mexico]
{3/3/09}
51427. Chrome plating process in aluminum
wheels [Argentina]
51428. Can I change the texture of an
existing silver item? (from plain, smooth texture to a rough cut)
[Australia] ![]()
51429. Painting metal trim molding [New
York]
51430. To dull Life Shine solid brass
lacquered brass [Canada]
51431. Need paint and laquer for 1973
Gibson Les Paul Custom [Canada]
51432. Salt spray testing for SS 304
[India]
51433. Look to be "Flow lines" after black
hard coat anodize, 6061 T6 alum. [Connecticut]
51434. Yellow-Brown stain on Solution heat
treated Aluminum [Canada]
51435. Rules and Regulation for Anodising
Process [UAE]
51436. Need Sn96.5%Ag3.5% plating on copper
prototype and production metal stamping application [California]
{3/4/09}
51437. Need chroming of small Brass
pieces [New York]
{3/4/09}
51438. Need the base of a coffee table
brass plated [New Jersey]
{3/4/09}
51439. Need my titanium ring anodized to a
gold/copper color [California]
{3/4/09}
51440. Need to qualify a supplier that does
aluminum anodizing per MIL-A-8625F - in Tijuana, Tecate or
Mexicali. [California]
{3/4/09}
51441. Looking for a tin/zinc process
[Wisconsin]
{3/4/09}
51442. Need selective coating on SS 304
tubing [India]
{3/4/09}
51443. Need to buy Alodine 600 [Spain]
{3/4/09}
51444. I need a good explanation on the
Hex/Tri issue [Michigan]
51445. Looking for information on spec
MFZn13TC [Ohio]
51446. Ferric chloride vs ferrous
[UK]
51447. Stripping Aluminum from Nickel
[California] ![]()
51448. Restoration of Civil War era iron
cemetery fence [Mississippi] ![]()
51449. What finishing process could expose
powder coated aluminum parts to fluorine? [Ohio]
51450. Warping during black oxiding
[Massachusetts]
51451. How to avoid green corrosion of
copper material after silver plating [Malaysia] ![]()
51452. What are the different types of cad
plating and how to tell them apart? [Virginia]
51453. Want thick layer passivate for zinc
plating [Israel]
51454. Sealing Hard Coat: nickel acetate
vs. hot DI [Arizona]
51455. 6063 Aluminum Alloy Corrosion
[Wisconsin]
51456. Inspection post passivation for
closed / non visible systems [Singapore]
51457. Why is thickness of Manganese
Phosphating varying? [India]
51458. Burrs are unavoidable in sheet metal
punching [India]
51459. Remove Teflon coating around
thread [Canada]
{3/5/09}
51460. Address of the latest machinery to
refine impure silver [India]
{3/5/09}
51461. Starting a paint manufacturing
[Nigeria]
51462. Nitric Acid concentration and
temperature for clean Ni from glass [Singapore]
51463. Totem Pole Wheelchair Wheel
Sculpture Finish for 12' aluminum pole [Kentucky] ![]()
51464. Restoring silverware after using
bronze cleaner [Ohio]
51465. Can we gold plate polymer and
plaster? [UK]
51466. Help prevent a murder! "Gold tint"
discoloration on overheated stainless coffee maker [Canada]
51467. How to Repair a Scratched Aluminum
Motorcycle Swingarm [Florida] ![]()
51468. I have a 24 carat gold plated
bathroom trashcan inside and out (an inheritance) [Oklahoma]
51469. Possible to plate two finishes onto
one object? [UK]
51470. Can I get hardness of 44-48 hrc all
over EN9 parts [India]
51471. FTMS 141 method 6301.3 vs 6301.2
[Canada]
51472. Salt for salt spray testing
[France]
51473. Analyzing for carbonates in alkaline
copper baths [Mexico]
51474. Using titration to find nickel
concentration in Zn/Ni electrolyte [Singapore]
51475. De Chroming Rims [Texas]
51476. Applying a clear sealer on black
steel [California]
51477. Purpose of bias in PVD process
[Singapore]
51478. Concentration of etching soda for
aluminum [Indonesia]
51479. 316LVM mate grey finishing
[Colombia]
51480. Looking for a source for the
Nitrotec-s process [Illinois]
{3/5/09}
51481. Community needs Bronze Statue
repair [California]
{3/5/09}
51482. Need copper liver finish on aluminum
extrusions [California]
{3/5/09}
51483. Need DMAB for electroless nickel
activation [New Jersey]
{3/5/09}
51484. Powdercoating over anodized
aluminum [Iowa]
51485. Seeking chrome plater to re chrome
my 26 inch chrome wheel [New Jersey]
{3/9/09}
51486. Need shop to do Ematal process for
Aluminium [Singapore]
{3/9/09}
51487. Have plastic (SLA) parts to be
plated [New Hampshire]
{3/9/09}
51488. Need Rodine inhibitor for Sulfamic
acid [Kentucky]
{3/9/09}
51489. Infrared proofing for clothing
[UK]
51490. Nickel Plating Importance
[India]
51491. Need citric acid for cleaning steam
sterilizer [England]
51492. Copper Plating Aluminum - DIY
Possible? [Washington]
51493. CHROME PLATING PROCESS
[Indonesia]
51494. Return steam and vapor off
Diochromate Seal tanks back to liquid form and return it to the tanks
for reuse [Idaho]
51495. How can I remove powder coating in a
localised area [India]
51496. Need a Dielectric coating on
stainless steel [Massachusetts]
51497. Peeling off of galvanised
coating [India]
51498. Titanium coating on SS at low room
temperature [Pakistan]
51499. Electroless Nickel Plating, too dull
on one run [Kentucky]
51500. Plating pricing [Missouri]
51501. Tin plating problem in Ferrostan
Process [India]
51502. Humidity endurance of type 2 class 2
coating [Philippines]
51503. Must have no electrooating in this
area [Michigan]
51504. I'm looking for someone who dips
original motor engine parts to chrome. [Louisiana]
{3/10/09}
51505. Machine Shop needs Black Anodize on
3000 pcs [Florida]
{3/10/09}
51506. Need good price on anodizing and
passivation supplies [Ukraine]
{3/10/09}
51507. Fantachrome and Alsa FX
[Denmark]
51508. What is EZM-2 Treatment?
[Indonesia]
51509. PU Coating or any other clear
organic coating on Aluminium [India]
51510. Glue to adhere S.Steel mesh to
Aluminium plate [Thailand]
51511. Refurbishing Pipe Railing of
Grandstand [Pennsylvania]
51512. Used PET plastic material as powder
coating raw material [Indonesia]
51513. Measuring pH in galvanizing flux
[Scotland]
51514. Nickel Activation - Cathodic or
Anodic? [Malaysia]
51515. Ideal thickness of Cu and Ag to
minimize RF loss [India]
51516. Acid Copper? Pits and imperfections
on Sterling .925 Tray-Can anyone acid copper to fill it? [Texas]
{3/11/09}
51517. Need Metal Front Panel of Oven
Repainted [California]
{3/11/09}
51518. Spec silver plating [Canada]
{3/11/09}
51519. What protective equipment for copper
sulphate experiments [England]
51520. W/w conversion to w/v [Saudi
Arabia]
51521. Chemical etching of steel
[Iran]
51522. Necessary to cross hatch Nikasil
cylinder bores? [Arizona]
51523. Muriatic acid tanks for stripping
galvanize are hard to come by [Michigan]
51524. Stainless and copper pots and pans
scratched from first cleaning [Pennsylvania]
51525. Erasing colors in anodised
titanium? [Colombia]
51526. Cobalt coating of tanzanites
[Thailand]
51527. Brass faucet needs lacquer stripping
and polishing [California]
51528. Burn mark on brand new stainless
steel stove [Australia]
51529. Silver hard soldering on nickel
electroforms - crack problem [India]
51530. Solution for rapid wearing of US10B
finish [Rhode Island]
51531. RAL color code sample card to
Munsell color code sample card [India]
51532. Putting a clear plastic coating of
even thickness over a triple curvature that gets warm [UK]
51533. Zinc Coating [India]
51534. Sweller for Polycarbonate?
[China]
51535. How To Get Grey Anodize To Match
[California]
51536. Need Mil-C-83488 Aluminum Coating
Supplier [Florida]
{3/13/09}
51537. Plumbing fixture (tub spout) needs
refinishing [Indiana]
{3/13/09}
51538. Seeking Ni plating of antique stove
parts [Massachusetts]
{3/13/09}
51539. IAW ASTM B545 Tin plating needed
[Michigan]
{3/13/09}
51540. Need 2024 T3 Test Panels for Salt
Spray [Alabama]
{3/13/09}
51541. Need anodes for lead
electro-winning [Chile]
{3/13/09}
51542. How to make aluminum scratch
resistant? [England]
51543. Concentration of Tin Electroplating
Bath [Malaysia]
51544. Reaction of PMMA with a Gold Cyanide
salt in a citric acid electrolyte ? [California]
51545. How to get factory "wrinkle or
sandstone kind of look" on replacement parts [Australia]
51546. Hexavalent/Trivalent recovery from
Chromic Acid Anodize? [Georgia]
51547. How can I eliminate the orange peel
when e-coating A60 Galvanneal material? [Mexico]
51548. E-coating books [Georgia]
51549. Chemical Process to Brown Auto Parts
and Springs [Pakistan]
51550. Chrome plating ABS Material
[Canada] ![]()
51551. Hard chrome to rebuild internal dia
of cast iron housing? [India]
51552. Heavy sludge dust in phosphating
[India]
51553. Dewatering property of oil
[India]
51554. Need chrome plating of bicycle parts
and nickel plating of sm. toy train parts [New Jersey]
{3/13/09}
51555. Need a plastic piece chromed
[Maryland]
{3/13/09}
51556. Need chandelier replated in gold
[Massachusetts]
{3/13/09}
51557. Peroxide Bombing [England] ![]()
51558. Flow/leveling of metallic
thermoplastic acrylics [Pakistan]
51559. RoHS issue with black oxide on 304
stainless steel [New Jersey]
51560. Crucible materials for zinc
oxide [India]
51561. Automatic Chemical Analysis of
Nickel Sulfamate [Texas]
51562. Nickel plated brass sheet is
staining [France]
51563. Inspection shows pitting in Nickel
Plate QQ-N-290 Class 2 Bright [Massachusetts]
51564. My hard anodize is too fast
[California]
51565. Best method for cleaning oil from
lamination stack before EP-coating [California]
51566. Finishing a galvanized tube
[UK]
51567. Need a sign rechromed [New York]
{3/17/09}
51568. Improving Electroless Nickel on
Copper [Pakistan]
51569. Want Dull finish on Stainless Steel
Kegs [Italy]
51570. Plating Tank - What kind of material
can it be? [Washington]
51571. Swallowing silver plating
[Canada]
51572. Looking for Zinc Sheet Metal look
alike for small table tops [Michigan]
51573. Hard anodizing chiller sizing
[Oklahoma]
51574. High nickel in our wastewater
[Vietnam]
51575. How to hold down Copper Levels in
Ebanol C-Special Bath [New Hampshire]
51576. Etching Ultem Plastic for
Plating [Saudi Arabia]
51577. Hard Anodizing power cost
[India]
51578. Buffing/Polishing Vibration
Monitoring Probe Tracks (4140 shafts) [Saudi Arabia]
51579. Can't achieve AISI #4 base finish on
316L SS tube [Ohio]
51580. Need hot dip tin plated copper wire
used equipment [India]
{3/18/09}
51581. Want warm liquid copper
water-based-paint [Romania]
{3/18/09}
51582. Suggestion for astm-standards of
Zinc and Zinc alloys plating on M.S. [India]
51583. Particle size of powder and role of
DFT [India]
51584. Thermal Deburring Advice please
[UK]
51585. Do they use nickel when plating
sterling silver with rhodium? [Oregon]
51586. Dull Plating in Bright Tin
Plating [India]
51587. Filling in the blanks with super
abrasives [Michigan]
51588. Trouble in black anodizing
[Indonesia]
51589. ASTM 967E Passivation alternative to
chromate? [Maryland]
51590. High temperature glue for Ceramic
and Quartz [Germany]
51591. Colouring stainless steel with
dye [Florida]
51592. Anodizing vs. Powder Coating for
aluminum counter top? [New York]
51593. How to keep abrasion on chrome wheel
from rusting and spreading [Kansas]
51594. Touching up chrome with minor
pitting [Australia]
51595. Industrial anodizing company in
Canada looking for anodizing course [Canada]
51596. Interpretation on EDX spectrum
result [Malaysia]
51597. 5 color printing on stainless steel
- spiral spring [Israel]
51598. Faster, Thicker Silver Plating?
[Pennsylvania]
51599. Plating defects [India]
51600. Anodizing thickness is greater at
bottom of rack than at top [Canada]
51601. Repairing cracks on anodized
surface [Turkey]
51602. CCT-1 test for stainless steel
SS-302 after passivation [India]
51603. Stainless steel electropolishing or
nickel or chrome plating [Vietnam]
51604. Wanted: Precision Plating
Business [Texas]
{3/20/09}
51605. Cyanide oxidation / residual
chlorine [New Mexico]
51606. Post Heat Treat of 416 SS to Avoid
Surface Corrosion [Florida]
51607. Substitute chemical for sodium
dichromate that can be used for the prevention of white rust
formation [Sri Lanka]
51608. The best way to decreasing the
carbonate content in Zn Plating process [Indonesia]
51609. Parting from mandrel [Italy]
51610. Black chromate is Rubbing off
[USA]
51611. Problems with plating brass?
[South Carolina]
51612. Ideal Metal for Cathode (Hanging
Wire Type) [Texas]
51613. RELATIONSHIP BETWEEN Sa value and
micron finish of surface [India]
51614. Need Blue Etch Anodize of very large
parts [Connecticut]
{3/20/09}
51615. Need a ring plated in gold
[Iowa]
{3/20/09}
51616. Steps before rhodium plating 18kt
white gold? [India]
51617. What ways can you strip chrome from
stainless steel? [Oklahoma]
51618. Paint peel off [Kuwait]
51619. E-coat on galvanized steel and non
galvanized at the same time [Mexico]
51620. Can mechanical zinc plating be
applied on smaller pieces in a mass production process?
[India]
51621. Customer's gold plated wheels are
pitting [UK]
51622. Rusting Of Stainless Steel
Railings [United Arab Emirates]
51623. Need jewelry coating for more than 3
years [India]
51624. Absorbent aluminum surface
coating [UK]
51625. Organic dyes for colouring of
aluminum [Pakistan]
51626. Need to remove engraving on a
sterling silver bracelet [England]
51627. Primer for painting stainless
steel [England]
51628. The interior of my microwave is
melting off. [Pennsylvania]
51629. Iphone Gold Plating
[Illinois]
51630. Recovering Silver from Silver
Nitrate [UK]
51631. RV Aluminum Siding Problem
[Washington]
51632. Is unplated Gold worth anything?
[Vermont]
51633. Does AMS or SAE control the
specs? [Florida]
51634. Most resilient/suitable finishing
for outdoor steel benches? [UK]
51635. Gold plating is fading
[India]
51636. How can I test anticipated life of
Gold Plating products? [India]
51637. SATIN NICKEL ON ZINC DIE CAST
[Ohio]
51638. Distinguishing 304 and 316 Stainless
Steel [UK]
51639. Need my Stainless Steel Motorcycle
Exhaust Blackened [Idaho]
{3/23/09}
51640. Need DURAVIN NDG-1V coating on 2-ft
long steel angles [Georgia]
{3/23/09}
51641. Distributor of blue chromating
solutions needed [Mexico]
{3/23/09}
51642. Painting of Stainless Steel Lemur
Tail for themed play area [Washington] ![]()
51643. Translating Ra to "pick count"
[Australia]
51644. Material of construction for
galvanizing baskets [India]
51646. Looking for sources of iron, zinc
and manganese wastes for beneficial use [Missouri]
51647. Pretreatment Process Parameters
[India]
51648. Differences between a No. 3 and a
No. 4 finish on Stainless Steel [Wisconsin]
51649. Solar Water Heaters and
Electrolysis [South Africa]
51650. Cost of hard chrome plating
[Singapore]
{3/24/09}
51651. Need Crankshaft Nitriding
[Canada]
{3/24/09}
51652. Need green antique finish
chemicals [India] ![]()
{3/24/09}
51653. What is the need? What is a good
thesis subject for master degree in electrochemistry?
[Malaysia]
51654. Food safe galvanized metal paint
[Oregon]
51655. 202 Versus 201 Stainless Steel
[Arizona]
51656. Setting up Contractometer to Measure
Stress in Nickel Bath [Scotland]
51657. Need E-Coat standard for automotive
brackets [Michigan]
51658. Suggest the surface treatment for
engine valves [India]
51659. Hydrogen peroxide in flux tank to
reduce dross [India]
51660. Rhodium Sulphate Brightener and
Whitener [India]
51661. Small water mark after plating
[Singapore]
51662. Plating chrome onto a gold layer
[UK]
51663. Reusing hydrogen gas emitted by the
sulfuric anodizing cathodes [Greece]
51664. Effect of porosity in metal
finishing [India]
51665. HR1095 scale removal prior to
plating [New Jersey] (***
51666. What Vibro finishing does to
lengthen salt spray life? [India]
51667. Removing scale from fire water
pipeline [India]
51668. Silver coating is gold in color
instead of silver [Thailand]
51669. Need a service to reduce hardness of
steel parts [Canada]
{3/26/09}
51670. Need chrome removal and Brushed
Nickel finish on $500+ faucet [Illinois]
{3/26/09}
51671. Fastener Manufacturer Needs
Zinc-Nickel plating service [India]
{3/26/09}
51672. Aluminum and stainless steel
anodizing [Ohio]
51673. Installation of galvanized fittings directly to black iron pipe [Georgia]
51674. Need Mil-A-8625, Type III, Class 2 dyed Black (matte), ATF Type 7 License holders preferred [Indiana]
{3/27/09}
51675. Silvering inside a bottle [UK]
51676. Cyanide destruction with peroxide (Cu catalysed) [Ghana]
51677. How to do Blue Galvanizing [China]
51678. Manganese Phosphating on Cast Iron Components [India]
51679. Trivalent Chromate Immersion Times [Maryland]
51680. ENP on Brass Components: No coating build up [India]
51681. How verbose must NADCAP approved work orders be? [Washington]
51682. Where can I get surface finish "texture code"? [California]
51683. Deposit peeling on borders and showing black spots on Watts bath [Colombia]
51684. Need blank Ion Exchange beads [Australia]
{3/27/09}
51685. Enquiry for setting up an Anodizing Plant for Aluminium [India]
{3/27/09}
51686. Corrosion resistance to dilute sulphuric acid [Spain]
51687. Gold plating 15 to 20 microns on watch cases [New York]
51688. If tub is stained with blue, is our water safe to drink? [New Hampshire]
51689. Repairing sun damage to auto plastic with Krylon Fusion [Wisconsin]
51690. Restoring chrome faucets damaged by cleaning fluid [England]
51691. University project: Chrome plating wastewater treatment [Malaysia]
51692. AlTiN stripping solution? [India]
51693. Steel furniture components are till rusting after tool-black surface [Illinois] 52278. Ferritic Nitrocarburizing of machined threads [New York]
51694. How to lessen gold plating roughness? [China]
51695. Formulating a black chromate bath [Iran]
51696. Silky Smooth Rubberized plastic and metal texture coating. [Virginia]
51697. Seeking to have 9 tubular bells brass plated or nickel plated. [Canada]
{3/30/09}
51698. Can you mirror polish an aluminum marine hull or will saltwater dull it? [Canada]
51699. Electrical conductivity of titanium screws used in surgery [Illinois]
51700. Storing a copper electro-form? [New York]
51701. Buffing wheels which one to use [Tennessee]
51702. Paint for plastic inflatable furniture [New Jersey]
51703. I need a material that can transfer image to glass and other surface [Nigeria]
51704. Want high shine plating on AR15 lower receiver [Connecticut]
51705. Raising a destroyed (ground down) Hull I. D. # on an Aluminum boat [Oregon]
51706. Copper treated with bleach, can it be saved? [New York]
51707. Hybrid electroplating plus xerography process [Wisconsin]
51708. Hard chrome plating using chrome anodes [India]
51709. Gold plating an aluminum surface that has chem film [New York]
51710. Outside of beaker shaped part is not Electro Polishing [India]
51711. Formula for Zinc Parkerizing [Malta]
51712. Sandblasted steel rusts immediately after going through iron phosphate pretreatment, Why? [North Carolina]
51713. Need molybdenum coating on soda lime glass [India]
{3/31/09}
51714. Copper sulfate wash as metals colorant [Ohio]
51715. Need to know what type of steel used in electro-galvanized steel [Texas]
51717. Plating to make stainless steel black [India]
51718. Can you safely zinc-plate a weldment that includes a hinge? [Canada]
51719. Need to find someone to do a Black Chrome process to brake canister [Florida]
{3/31/09}
51720. Need Alkaline Tin Plating Process Chemistry [Singapore]
{3/31/09}
51721. What metallographic etchant for 4032 and 4047 aluminm alloy? [Singapore]
51722. Anodizing Problem, part gets thinner instead of thicker. [Ireland]
51723. Jewelry designer needs Black Oxide for stainless steel: dry finish safe for continuous contact with skin [Tennessee]
51724. Hydrogen embrittlement from pickling [India]
51725. Teflon stud bolts and electrical grounding [Texas]
51726. What is the pound per linear foot on 26GA through 14GA Galvanized Metal [Virginia]
51727. Adhesion in Palladium to Palladium electroplating [California]
51728. Blue stains in zinc plating [Mexico]
51729. Problems with Clear Anodizing [UK]
51730. Need to install anodize tank [Oklahoma]
51731. Need anodized aluminium flashing for solar concentrator [Italy]
51732. MIL-C-5541 vs. MIL-STD-5541 [Wisconsin]
51733. Stripping Tin Plating from Cast Bronze [Philippines]
51734. Need Zinc Phosphate Coating Service [Tennessee]
{3/31/09}
51735. Need XRF machine [Virginia]
{4/2/09}
51736. Chromates, dichromates: what purpose in deox/desmut? [Georgia]
51737. Difference between RoHS black zinc and RoHS clear zinc finish [California]
51738. Aluminum casting that "won't take hard anodize" [Missouri]
51739. Concentrate / Recover Zinc Sulphate from waste stream [India]
51740. Need wood-grain powder coating - wood finish transfer stickers [Sri Lanka]
{4/2/09}
51741. NOx Emissions from Titanium NDT Etching? [Canada]
51742. Plating F-125 with electroless nickel [Spain]
51743. Is there any institution who conducts training for electroplating metals? [Philippines]
51744. Need gold plating process chemistry [Hong Kong]
{4/2/09}
51745. What metal needs to be used before silver plating on copper? [Singapore]
51746. Need buffing of a 23" dia. aluminum blanks 0.040 thk. [Massachusetts]
{4/2/09}
51747. Seeking anodizing service for aluminum [Malaysia]
{4/2/09}
51748. Refinishing a Brass Snare Drum [Illinois] ![]()
51749. OABIC, OIA, and BRUT finishes in anodizing [India]
51750. Looking for Arthur Brace's "The Machining of Aluminium" [England]
51751. EDGE PULL BACK WITH HEAVY DEPOSIT HIGH PHOS ELECTROLESS NICKEL [Illinois]
51752. Electroless = Single Element Replacement Process? [California]
51753. Problem with Copper Levels Building in Pyro Bath [New Zealand]
51754. Thermal Expansion Characteristics of a Chrome Plated Component [Ohio]
51755. Can Hardcoat Anodize be done in-house? [Connecticut]
51756. "Iridite" coating analysis question? [Pennsylvania]
51757. Coated aluminium is not withstanding phosphoric acid [Illinois]
51758. Need 150,000 parts hard coat anodized Central Texas area [Texas]
{4/6/09}
51759. Brass tarnishing solutions won't dull my fishing lures as desired [Washington]
51760. Cleaning rust from high tensile steel [Australia]
51761. How to know which metal an antique is made from [N. Ireland]
51762. For antique mirror, start with a mirror or with plain glass? [Lithuania]
51763. Plating a previously used motorcycle exhaust [Washington]
51764. Diamond turning electroless nickel [New York]
51765. Repaint aluminum patio furniture [Florida]
51767. How to do trivalent conversion coating [India]
51768. Reference book about Ni, Pd, Au and Ag plating on copper substrate [Malaysia]
51769. Best metal roof finish for safe rainwater collection [Michigan]
51770. Rough finish in hard chromium plating [India]
51771. Anodized aluminum and road salt [Minnesota]
51772. What is Tri-cationic phosphating? [India]
51773. Heat and Finishes (Galvanneal vs. Electroplating) [Maryland]
51774. Zinc-nickel on Al diecastings (including Enviralloy Ni) [UK]
51775. Removing porcelain from tooling without freezing [Ohio]
51776. Fire Rating on Powder Coating [Florida]
51777. Galvanizing alternative for structural steel staircase [Washington DC]
51778. Zinc trivalent with TOP SEAL to last 480 hrs SST life [Malaysia]
51779. The cost of passivation of implants [Massachusetts]
51780. Acid copper plating bath reaction with PMMA [California]
51781. ElectroGalvanized steel caused salt spray problem [Malaysia]
51782. Chemfilm paint adhesion [Colorado]
51783. Need lusterless black finish per MIL-STD-171 3.4.1 and 3.3.2 [Wisconsin]
{4/7/09}
51784. Difference between Silver Flash and Silver Plating [India]
51785. Why is SS 316 recommended for BSL 3 lab exhaust Dusts? [Pakistan] 52148. QQ-N-290 Ductile Nickel Equals What New SAE AMS Standard? [Texas]
51786. How to remove Jasco Prep and Prime (iron phosphate) spots from galvanized roof [North Carolina]
51787. Hydrogen reactions from vinegar plus sanded nails [Illinois]
51788. Can anyone suggest an alternative to gold plating [Scotland]
51789. Recommended UV/Vis instruments for plating bath analysis? [Washington]
51791. White final finish for fashion jewelry [Pakistan]
51792. Improving the surface finish of PTFE plate [New York]
51793. Nickel Plating Too Shiny! [Idaho]
51794. Bulk curing of painted components [Singapore]
51795. Cannot get the black finish in electrolytic tin method [Mexico]
51796. 5005 or B57? [England]
51797. Selection of plating on metal for wear resistance [India]
51798. Tin Plated Stainless Steel Undercoats [California]
51799. Effect of cadmium plating on aluminum components [Canada]
51800. Process to determine life time of galvanized steel [Sri Lanka]
51801. Need hot dip galvanizing line for fasteners [Netherlands]
{4/9/09}
51802. Need S&W pistol blued [Utah]
{4/9/09}
51803. Want polished brass plating of light fixtures [New Jersey]
{4/9/09}
51804. Properties of Electroless Nickel [India]
51805. Watts Bath Conductivity [India]
51806. Looking for Contractometer [Singapore]
{4/9/09}
51807. Premature white corrosion on trivalent plated hydraulic tubing [North Carolina]
51808. Need Brass Grohe Bathroom Fixtures Refinished [New Jersey]
{4/10/09}
51809. Need to find a company that can coat a metal stamping with NBR-75 rubber coating product [Indiana]
{4/10/09}
51810. Apply Zinc coating weight 275 g/m2 for thickness 2 mm [Egypt]
51811. Instant Black Spot Even Before Drying Process [Indonesia]
51812. Paint blistering on zinc plating - Why? [UK]
51813. Need zinc/aluminum Thermal Spray [Mexico]
{4/10/09}
51814. Need mold material for nickel plating and silicone coating [North Carolina]
{4/10/09}
51815. Cyanide Storage and Gold Electroplating in the 70's [Massachusetts]
51816. I am looking for a sealant for clay pots [Tennessee]
51817. Playbuoy needs facelift [Michigan]
51818. Powder coating over zinc plating [Illinois]
51819. Wanted: Non-conductive clear coating for battery terminals [California]
51820. Blue/black a large steel staircase and shelf units. [Italy]
51821. Coating for small steel parts in continuous outdoor environment [Massachusetts]
51822. Looking to acquire used 24" dip spin machine. [Minnesota]
{4/10/09}
51823. Zincate Bath Life [India]
51824. Seeking hot and cold black oxide finisher [New York]
{4/10/09}
51825. How to get the yellow finish on a restored carburetor [Texas]
51826. Will a burnout kiln melt gold concentrate and/or precipitant [Canada]
51827. Chrome plating on high speed rotating equipment [India]
51828. Electroless nickel is rusting in threaded area [India]
51829. What do I need to anodize my paintball gun [United States]
51830. Can solid, non ionized copper and silver be used to kill microbes in slow-flow water filter? [New York]
51831. Cad Plating in Aviation? [Georgia]
51832. Need EC system to remove As from wastewater [China]
{4/13/09}
51833. Need Micron Thickness Metal Sheet [India]
{4/13/09}
51834. Need non-conductive coating - to hold a static charge [Oregon]
51835. Chromic acid treatment on Magnesium jewelry [Netherlands] ![]()
51836. New to Black Chromate Conversion on Acid Chloride Zinc [Arkansas]
51837. Brass turns to Rust color [New Hampshire]
51838. Need decorative chrome-plating source in my area [Illinois]
{4/13/09}
51839. Gold plating machine [India]
{4/13/09}
51840. Production Zinc Plating to related specifications QQZ325 or ASTMB633 [Utah]
51841. Surface finishing of aluminium sheet for light fixture reflector [India]
51842. Having trouble mirror polishing stainless sheets [India]
51843. Plate Silicon and Tin on amorphous carbon [California]
51844. Where can I find double layered metal [UK]
51845. How can I stop or slow down the corrosion of an aluminum boat? [Texas]
51846. How to produce Galvalume? [Egypt]
51847. Can I dye a light fixture in metal? [New York]
51848. How to remove unwanted galvanic plating from stainless steel valves [Sweden]
51849. How to get the special effects in powder coating [Illinois]
51850. Replace wroght iron railings or restore [Iowa] ![]()
51851. Unknown losses in zinc kettle even with no production [India]
51852. 32% nickel plating on ETP copper wire [India]
51853. Which casting grade of aluminium allows Anodizing and Alodining? [India]
51854. Trivalent chrome passivation operating parameters [India]
51855. How to measure the concentration of heavy metals [Jordan]
51856. Best substrate for Ti-Gold PVD coating [California]
51857. Does zinc plating increases shear strength of screw? [India]
51858. Manganese Phosphating isn't heavy enough [India]
51859. Electroplating companies in NY? [New York]
{4/15/09}
51860. Plating Nickel over Tungsten? [India]
51861. My clothes are grey due to paint worn off of dryer [New York]
51862. Ni elimination from waste water [Israel]
51863. Removing paint spilled on a gold and sapphire ring [England]
51864. Etching steel rings for penny pressing machine dies [Arkansas] ![]()
51865. Using immersion silver plating solution on raw brass? [California]
51866. Creating a dark oil rubbed bronze finish on aluminum [Georgia] ![]()
51867. Identifying 303 stainless vs 304 [Georgia]
51868. Salts are precipitating on our blackened copper electroforms [California]
51869. Look for E-Coater with FFL [Connecticut]
{4/15/09}
51870. Preventing blunting of sharp blades by storage in liquid [Florida]
51871. Aluminium Powder Coating Standards Australia [Papua New Guinea]
51872. Can Racking During Black Oxide Process Cause Thermal Discoloration Appearance? [Michigan]
51873. Grey stain and water marks after anodising [Jamaica]
51874. Need On-site Passivation [Colorado]
{4/15/09}
51875. How to Silver a convex mirror [Canada]
51877. Streaks in aluminium 6063 anodizing [Kenya] ![]()
51878. Applying antique lacquered finish to brass in high volume [UK]
51879. We are facing problem with powder coating [Malaysia]
51880. PVD black and brown on brass components [Hong Kong]
51881. Need to change my vanity faucets from antique brass finish to oil rubbed bronze finish [New Jersey]
{4/17/09}
51882. Need faucets to be gold plated [Tennessee]
{4/17/09}
51883. Need tin alloy platings to withstand high reflow temperature [China]
{4/17/09}
51884. Need automatic hot dip tin copper wire machine [China]
{4/17/09}
51885. Anodizing of aircraft wheel hubs [Fiji]
51886. Materials and Techniques to Plate a Tuba [Canada]
51887. Longevity of blackened or anodized metals [Hawaii]
51888. 316L electrodes are pitting in hydrogen-from-water service [California]
51889. How to make Nickel Plated Brass Keys RoHS compliant [Canada]
51890. Aluminized Epoxy Topcoat was wiped with MPK. Is it harmed? [Arkansas]
51891. Passivation of copper and copper alloy waveguide [Italy]
51892. What is standard E-coat thickness? [Mexico]
51893. Galvanized but unpainted doors rusted in one year [Texas]
51894. Platinum-Clad Anodes for Chrome Plate [Maine]
51895. Need "Structural Examination of Titanium Alloys Etch-Anodize" [Texas]
{4/17/09}
51896. Need gold replating of door hardware [New York]
{4/20/09}
51897. Need Nicotef Plating of type 301SS Sheets [Pennsylvania]
{4/20/09}
51898. Need low-temperature degreaser for anodizing process [Mexico]
{4/20/09}
51899. Aluminum extruder seeks product for reflectivity without anodizing [Pakistan]
{4/20/09}
51900. Need Anode and Cathode For Gold Electrowinning [Iran]
{4/21/09}
51901. Electroless Nickel plating degrades surface finish [New York]
51902. ELECTROPLATING BATH FOR CYANIDE COPPER [India]
51903. Blistering of cadmium plating on stainless steel [India]
51904. Want to plate cerium metal with an inert material like gold [North Carolina]
51905. RECOVERY OF STRIPPING SOLUTION FOR SILVER [India]
51906. Die components are getting pucture holes during anodising [India]
51907. How to find the concentration of nitric acid by volumetric titration? [India]
51908. Polishing naturally pitted [cast] aluminum [Missouri]
51909. Titanium (CP grade 2) cleaning procedure for implantable medical device-similar to pacemaker [California] ![]()
51910. High temp resistant material used as botting on metal surfaces [Lebanon]
51911. Best Coating Material [India]
51912. Is ruthenium or rhodium safe? [Illinois]
51913. Ever heard of hard chrome plating aluminium, via anodizing? [Oklahoma]
51914. Is Alodine 1200S RoHS compliant? [Tennessee]
51915. Magnesium or rare earth additions to hot dip zinc? [UK]
51916. Consumption of iron with hydrochloric acid in galvanizing [France]
51917. Material for container HF 21% v/v [Mexico]
51918. To make mirror finish [Arizona]
51919. Effect of phosphating before heat treatment [India]
51920. Is it possible to have metallic silver shade/color by E.Coat ? [India]
51921. Need brass horse and clock assembly re-brassed [North Carolina]
{4/21/09}
51922. Seeking White Anodize Hardcoat [Oregon]
{4/21/09}
51923. Average life expectancy of just metal [England]
51924. Need consultant for aluminum bright dip setup [Texas]
{4/21/09}
51925. Inert anode for silver plating [Philippines]
51926. Need a pewter color finish for aluminum punch panels [Missouri]
51927. Need white or silver-gray semi-gloss E-coating [Michigan]
{4/21/09}
51928. Finishing on Outboard Motors [South Africa]
51929. Can we still recycle rinsewater after adding inhibitor to pickling acid? [India]
51930. Brush Look for Aluminum [South Dakota] ![]()
51931. Need Mil-Std 171 olive drab plating [Ohio]
{4/23/09}
51932. Want to achieve Dark Electroless Nickel Plating [Colorado]
51933. Extremely Rare 1935 Bugatti Showcar with Magnesium Body Needs "Bright,Silvery" Protective Surface! [California] ![]()
51934. Does Mil-A-8625 require color consistency? [Minnesota]
51935. Making bare aluminum chain match nickel plating? [Texas] ![]()
51936. White rust on bonderized steel [Montana]
51937. Electroplating Finishes for Zamak Parts [South Carolina]
51938. Process for matte black finishing of Stainless Steel [Chile]
51939. Stainless Steel Pretreatments before Powder Coating [Virginia]
51940. Why are chrome plated tools more durable than wheels? [Massachusetts]
51941. Antique horse and clock needs new bronze coating [North Carolina]
{4/23/09}
51942. Black stains on aluminum from shipping [Mexico]
51943. 1950's Kitchen wanted for photoshoot [New York]
51944. Need Titanium Pickling Service [Michigan]
{4/23/09}
51945. Metallic powder coating isn't working [California]
51946. Poor spray paint adhesion on aluminum sheet [India]
51947. Electroplating gold onto copper without gold solution [Australia]
51948. Gray dots on semi-bright nickel plated hull cells [Vietnam]
51949. How to reduce COD from cardboard plant using starch [Jordan]
51951. Tin plating on brass is blistering [India]
51952. Court reporter asks what visual defect on coil coater sounds like "star val B" [Texas]
51953. Which finishing process is better honing or burnishing? [India]
51954. How to dull Galvanized Steel Structures for San Diego Forest and Environment Authoritiy [India]
51955. Need Chrome Plating of small parts for firetruck [Illinois]
{4/24/09}
51956. Excessive Foaming of Black Oxide Bath [New Hampshire]
51957. How do I finish a light fixture in "antique bronze" finish? [South Carolina]
51958. pH measurement at temperatures other than ambient [India]
51959. Texture etching on stainless steel like glass [UAE]
51960. Triple Salt and Quadra Flux Densities? [Egypt]
51961. Titanium Rack for aluminum anodizing turned pink [Colorado]
51962. 4th Grade Science Fair...Fire from a potato [Florida]
51963. Are Corten water features possible? [Australia]
51964. How to use zinc phosphate sludge for the manufacture of bricks [India]
51965. Homeowner needs bronze finish on brass colored plastic trim in jacuzzi tub [Louisiana]
{4/27/09}
51966. What is anolyte, theory of ultra filtration for ED paint, constituents of ED paint? [Iran]
51967. Seeking Plastic Chrome Plating Services [New York]
{4/27/09}
51968. Seeking anodizing 6061 aluminum railings [California]
{4/27/09}
51969. What is Melinite? [Maryland]
51970. Where can I find a printable version of QQ C-320 to purchase? [Iowa]
51971. Ideal zinc temperature for galvanizing [India]
51972. Tungsten composite separation [Texas]
51973. E-coating issue on electrogalvanized material [Illinois]
51974. Chrome Plate of the Brass Ball in a Ball Valve [Rhode Island]
51975. Advantages of platinized titanium anode over lead-tin anode in chrome plating [India]
51976. Nickel plating salt spray failure [India]
51977. Hard copper plating that can be etched best [India]
51978. Carbon steel chisels destroy corrosion resistance of stainless [Illinois]
51979. What grinding wheels are available for sharpening/redressing C B N cutters [Canada]
51980. Bolting Galvanized Structural Steel [Michigan]
51981. Need VW Beeetle bumpers plated [Canada]
{4/27/09}
51982. Impermeable coating for 200 micron diameter alloy spheres [Wisconsin]
51983. Induce Chloride on Aluminium Pad (wafer) [Malaysia]
51984. Adhesion tape and roll for Fed-std-141 method 6301.3 [Canada]
51985. Quick Connects for Rectifier to Anodizing Frame [Colorado]
51986. Ultrasonic Agitation, mixing solution [UK]
51987. Improving adhesion of lacquer on brass zipper teeth for outdoor application? [Italy]
51988. Electroless Nickel versus Zinc Dichromate [Ireland]
51989. What's best prep for 416 SS bars before plating with Electroless Ni/Teflon? [Illinois]
51990. Need help plating 416 Stainless [Tennessee]
51991. Certification of Alodine 1201 to AMS 2473 [Pennsylvania]
51992. Laser mark Alochromed Aluminium [UK]
51993. Zinc finish on tubing (help) [Kansas]
51994. Polishing for circular finishes in ultra high vacuum chambers [Canada]
51995. What is Fluorocarbon coating [China]
51996. TriHydric chrome plating on fasteners [Malaysia]
51997. Stop potassium carbonate buildup in silver cyanide bath or recover silver [India]
51998. Silver plating over silver electroform - decorative articles and figurines [India]
51999. What kind of filter should I use to refine the platinum plating bath? [Iran]