42000. How to tell real chrome from stainless steel [Tennessee]
42001. Hydrochloric Acid and Sulfuric Acid [Illinois]
42002. Analysis methods for mixture of hydrochloric acid and sulfuric acid [Indonesia]
42003. Powder plastification - Orange peel effect on surface [France]
42004. Preplated sheetmetal [California]
42005. Need 10k gold fill of old watch case [California] {8/25/06}
42006. Carbon steel blade in terrible condition! [Arizona]
42007. Can I paint a walk-in cooler? [Texas]
42008. Need spot test solution or other means to test for Chromium on Aluminum [Minnesota]
42009. Sizing of Plating Tanks [Colombia]
42010. Electrode corrosion in anodizing bath [Greece]
42011. Return of conductivity after rinsing [Canada]
42012. Require rust prevention on black oxide part [India]
42013. Hardness of black nickel plating [Malaysia]
42014. Anyone know of Lou Morin or Mor-Industrial in Tarrytown? [New Jersey]
42015. Sn Coating over Aluminium ( Al 6082 ) [Turkey]
42016. Oil resistant plating [India]
42017. Ever notice a buffering effect in a sulfuric anodizing tank? [California]
42018. Pretreatment for powder coating on MS sheet [India]
42019. Unwanted lines in anodising [UK]
42020. Black oxide and skin burns [Michigan]
42021. Need nickel-chrome plater in Asia [Wisconsin] {8/25/06}
42022. Need Replating of Door Hinges [Tennessee] {8/28/06}
42023. Need bumpers plated also pot metal items for 1957 Nash Rambler [North Carolina] {8/28/06}
42024. Need straightener for big bars [Iran] {8/28/06}
42025. Need baths, anodes, chemicals for Tin plating on Copper [UAE] {8/28/06}
42026. Seeking tin coat process for aluminium pistons [Venezuela] {8/28/06}
42027. Recovery of Platinum from Aluminum Oxide Sand [Singapore]
42028. Solubility of CuSO4 in H2SO4 [Washington]
42029. Can trivalent chromate finishes oxidize to hexavalent? [California]
42030. Regeneration cycle: switching from HCl to H2SO4 [Singapore]
42031. Dipping Paint [Indonesia]
42032. Gravimetric test for determination Al and Pb % in Zinc Bath [Egypt]
42033. Chromium Mirror Coating Parameters [India]
42034. Black Oxide on stainless finish WITHOUT sulfur [California]
42035. Bubble chrome structure [Holland]
42036. What cause electroplating bleed out at casting coner edge and how to overcome? [Malaysia]
42037. Why Gold coating over Titanium Nitride turns reddish when touched? [India]
42038. Rusting on trivalent chrome plating [India]
42039. Chrome plate adhesion [Turkey]
42040. How to remove rust on the machined surface without affecting the base metal [Michigan]
42041. Explanation of the Theory of "Vapour Blasting" [Alabama]
42042. Mirror finish on stainless steel surface [India]
42043. Synthetic coating for aluminum alloy [Singapore]
42044. What is the mechanism for the different characteristic odors of metals when handled? [Canada]
42045. Through hole plating of PCBs [Sri Lanka]
42046. Achieving uniform plating thickness in bores/ ID of cylindrical shaped components [India]
42047. How do you use hydrochloric acid to clean brick paving without doing damage to bricks and garden [Australia]
42048. Refinishing old bathtub feet, faucet and shower curtain ring [Nevada]
42049. Recovery of fine gold [Arkansas]
42050. Acid Stripping a Car Body [UK]
42051. Cleaning 1930s heavy brass tray [California]
42052. Zinc plating small motorcycle parts [Florida]
42053. Aluminium Chromatizing with yellow passivation [India]
42055. How to know if a part has been processed with black oxide or black zinc [Costa Rica]
42056. NEED A PLATED CUSTOM GRILLE AND BUMPER DIP, ETC. [Arizona] {8/30/06}
42057. NEED PAINT BOOTH [Virginia] {8/30/06}
42058. Requirement of PVD machines [India] {8/30/06}
42059. Spectrophotometric analysis of silver in jewelry [Philippines]
42060. Alternative inhibitor for tin refining [Canada]
42061. Argentium [Bolivia]
42062. Hex. or tri.? [Missouri]
42063. MIL-P-23377 suitable for Inconel? [Colorado]
42064. Salt Spray Test Exposure Calculation [India]
42065. Blow holes in solder on boards [Maine]
42066. Metal Plating (URGENT)! [California]
42067. Electrochemical machining (stem drilling) [Texas]
42068. Passivation of Phosphorus Bronze [New Jersey]
42069. Need 1974 Nova rear bumper chrome plated [New Jersey] {8/31/06}
42070. Need Price on Hitachi Hot Dip Galvanize unit [Nigeria] {8/31/06}
42071. Silver plating on copper [Colorado]
42072. Copper iridium coin [India]
42073. Bright silver plating on aluminum parts [India]
42074. Corrosion resistance of aluminum polish [Virginia]
42075. Home brewed gun part coating? [Tennessee]
42076. Removing lead based solder from copper? [England]
42077. Black spots on zinc plating with trivalent (clear) chromate [Ohio]
42078. Faraday effect in chroming yields "trouble areas"? [Denmark]
42079. Glass in anodising process [UK]
42080. Titanium pyrophosphate+Na2HPO4 in activation surface [Iran]
42081. Replacement for hexavalent chrome on galvanized steel [Ohio] {9/1/06}
42082. Need PVDF Material [India] {9/1/06}
42083. Start gold plating unit for plating jewelry [Malaysia] {9/1/06}
42084. Need Lord Parlock Primary PM05 [Iran] {9/1/06}
42085. Need stain line conveyor coating [Wisconsin] {9/1/06}
42086. General Aluminum Polishing [Utah]
42087. Discoloration of superalloy part after vacuum heat treatment [Canada]
42088. Does any one know anything about the Cr3+ Yellow chromate? [Florida]
42089. SRTP finishing process [Kansas]
42090. Epoxy coating inside a tube for chlorinated vapours transfer [India]
42091. Mechanical Zinc Plating [Rhode Island]
42092. Low temp. acid copper plating [Wisconsin]
42093. Available processes for surface preparation of titanium for primer [Virginia]
42094. Electro plate aluminum? [Illinois]
42095. Size buildup of manganese phosphate plating on G2 CAST IRON [Pennsylvania]
42096. Cracked plastic chrome grill surround for restored 1968 Buick Gran Sport needs repair [Ohio] {9/1/06}
42097. Need membrane system for caustic recovery from mercersing [India] {9/1/06}
42098. Need system for online marking on tubes [India] {9/1/06}
42099. Electroplating [California]
42100. Remove Antique Finish from Class Ring [Texas]
42101. Screen printing on silver or gold [Lebanon]
42102. Scratch hardness test [India]
42103. Zinc Plating before Powder Coating for Architectural Projects? [Michigan]
42104. Water breaks and ED streak marks [Philippines]
42105. What will E-coat cover [North Dakota]
42106. Prep for painting of "chem-treated" galvanized steel [Texas]
42107. Tin4+ control range in tin bath [Malaysia]
42108. Rhodium Spotting Problems [California]
42109. Matte finish on 316 stainless steel [Oregon]
42110. Chemical Attack on Copper Condenser Coils [England]
42111. Need spray coating of welded AISI 304 box [India] {9/6/06}
42112. Need hot dip galvanizing plant [Iran] {9/6/06}
42113. Dichromating procedure on auto carburetors [Texas] {9/6/06}
42114. Need Alodine 1200A and 1200B [Pakistan] {9/6/06}
42116. Science project on the affect of SALT and water on steel wool [Florida]
42117. Electroplating ZnNi [Jordan]
42118. Cheap conductive coating applied to fuel cell [Portugal]
42119. How to plate Shakudo [Colorado]
42120. Love the metal look to our metal frames...how do we protect it? [New York]
42121. Gold Plate Phone Cover [New Zealand]
42122. Brake rotor coatings...replacements for cadmium, and hexavalent chrome? [Ohio]
42123. Dichromating automobile carburetors [Texas]
42124. RoHS Passivation [Oregon]
42125. Alternative for Tri Chloro Ethylene [India]
42126. Galvanneal/Paint compatibility [Washington]
42127. High Build Epoxy OR 2K Polyurethane [India]
42128. ASTM 153 and 123 [California]
42129. Info about hot deep galvanization [Egypt]
42130. Black/brown oil like contaminant in acid-copper plating solution [Hong Kong]
42131. Pre treatment of aluminum [The Netherlands]
42132. Proveedores de Electropulido [Mexico] {9/6/06}
42133. Need UV powder coat suppliers [Florida] {9/6/06}
42134. Need used titanium, lead lined, or polypro tanks [Michigan] {9/6/06}
42135. Need tools for hard chrome solution bath analysis [Saudi Arabia] {9/6/06}
42136. What does it mean to "Satin Coat Steel" [Canada]
42137. Stainless fasteners for galvanized assembly? [New Jersey]
42138. Pulse rectifier in reel-to-reel plating [India]
42139. Clear anodized aluminum repair. what finish / coating to use? [Ohio]
42140. Stainless or zinc plated a better galvanic couple with aluminum? [Australia]
42141. Seeking retining of inside of copper kettle [Oregon] {9/7/06}
42142. Metal cabinet refinshing [Maryland] {9/7/06}
42143. Plating of platinum on magnesium alloys [South Africa]
42144. THE EFFECTS OF FLUORESCENT LIGHT ON BLACK OXIDE FINISH [Minnesota]
42145. DECRO COATING IS CONDUCTOR OR NOT [India]
42146. Clean in Place - Copper Piping [Minnesota]
42147. Electropolishing issues with Nitinol [Massachusetts]
42148. Personal exposure to Sodium Di(Bi) Chromate [Australia]
42149. Plating a pewter product [Indonesia]
42150. How can we get a homogeneous zinc pot? [Egypt]
42152. Is baking required after hard chrome plating? [Indonesia]
42153. Analysis procedure and bronze oxidation temperature [Indiana]
42154. Electroplating silicon dioxide [Jordan]
42155. Changing a brass finish to a chrome or nickel plated finish [Louisiana]
42156. Jeweler wants sourcing for cyanide [Texas]
42157. Give me a RoHS compliant treatment for brass [Israel]
42158. Need my Infiniti M45 grill plated [New York] {9/8/06}
42159. Looking for someone to refinish / clean my elevator doors [California] {9/8/06}
42160. How do I gold coat inside 1/4" pyrex tube for internal IR reflectance? [California]
42161. What will turn Cast Aluminum Black? [Texas]
42162. Cannot get a consistent pattern in hammertone [India]
42163. Black oxide leaching in clean room [Connecticut]
42164. Iridite 14-2 dry shelf life [Washington]
42165. Aluminum anodize coating failure due to air ionizer? [Massachusetts]
42166. Tin Plating [UAE] {9/8/06}
42167. Chrome plating on alloy (aluminum )wheel [Canada]
42168. Refinished "old style" rims for 1984 380SL Mercedes [California] {9/8/06}
42169. Need Ecoating of fasteners [Michigan] {9/8/06}
42170. Brown colour of gold jewelry [Uzbekistan]
42171. How to paint a car using paintbrush and glossy paints? [Florida]
42172. Information on the restoration of Magnesium Halibrand wheels [Illinois]
42173. Minimum Protection While Metal Finishing [California]
42174. Tarnish and finger prints on machined copper [Massachusetts]
42175. Need assistance on brass patina failures [Washington]
42176. Copper plating on steel [Texas]
42177. Oxalic Acid Anodizing [California]
42178. Need in-situ replating of old bath fittings [California] {9/11/06}
42179. Need Srt8 wheels chromed [Maryland] {9/11/06}
42180. Need an organic dye for hard anodized aluminium [India] {9/11/06}
42181. Thin film adhesion [India]
42182. HCL using in oil well treatment [Kuwait]
42183. TITANIUM ETCHING [India]
42185. Recovery of nickel, chromium, zinc from sludge using biomolecule-siderophore and/biosurfactant [India]
42186. LEAD BATH and ZINC BATH [India]
42187. Nitric acid etching of silver jewelry [New York]
42188. DOES NITRIC ACID WORK ON ALUMINUM ? [Mexico]
42189. Cadillac spoke wheels with bad clear coat [Pennsylvania]
42190. Bluing 20 guage cold rolled steel [Georgia]
42191. Rhodium Plating for .925 Silver [New Jersey]
42192. Recovering factory waste to safe drinking water [India]
42193. Conveyor coating [Wisconsin]
42194. Baking of Electrodeposited Paint Film [India]
42195. Soot and smoke contaminated powder coated aluminum [Malaysia]
42197. IRON PLATE [Mexico]
42198. Blister problem and Salty problem on Chrome parts [Malaysia]
42199. Correct Process Sequence for Tri Passivations [India]
42200. Struggling in cadmium plating [India]
42201. Hard chrome plating replacement in gun barrel bore [Pakistan]
42202. Plating on Sheet Iron Products [India]
42203. Flatness issue about powdercoated parts [Thailand]
42204. Copper and zinc plating (thermal diffusion) [Texas]
42205. Interested in process for diamond like coating [California] {9/12/06}
42206. Need 100 lbs of Cadmium Oxide [West Virginia] {9/12/06}
42207. Spray booth heater [Texas] {9/12/06}
42208. Treating a copper birdbath [Texas]
42209. Can billet aluminum wheels be chrome plated? [New Jersey]
42211. How to evaluate trivalent clear chromate on steel while performing B117? [Iowa]
42212. Safe alternative to Nitric Acid Brite dip tank? [Illinois]
42213. Epoxy powder-coat adhesion to hexavalent and trivalent fasteners [Illinois]
42214. purged
42215. Items nickel coated in barrel process rips after crimping operation [Turkey]
42216. Cottonball and/or Mirror Finish [Canada]
42217. Formicary corrosion in copper tubes for air conditioning systems [Italy]
42218. Welding Coreten Steel [Utah]
42219. Manganese coating [India]
42220. How to tarnish marcasite [New York]
42221. Unpassivated galvanized steel [Canada]
42222. Yellow Bronze Electroplating [Pakistan]
42223. Pretreatment of aluminum diecastings [India]
42224. Amine concentration of chemical deflash [Philippines]
42225. Titanium plating on brass [India] {9/13/06}
42226. HIGH HEAT ENAMEL PAINT [Illinois] {9/13/06}
42227. Barrel plating aluminum (6061-T6)mandrel [New Jersey]
42228. Anodizing with formic or citric acid [England]
42229. Galvanic action around corners? [UK]
42230. Antioxidant for Copper Jewelry Tarnish [Colorado]
42231. Electroplating on Aluminum [India]
42232. Need antique door hardware Tiger strip finished (copper and black) [Maryland] {9/14/06}
42233. Need formed plastic logos chromed [Georgia] {9/14/06}
42234. Sealing a brass sink [Ohio]
42235. Painting over fiber coated roof coating [West Virginia]
42236. Compatibility of copper plating with bronze screws [Delaware]
42237. Galvalume corrugated siding vs galvanized steel corrugated siding [California]
42238. What is the Confidence Interval For MIL-STD-105E? [New York]
42239. Aluminide Coating Stripper [Canada]
42240. Post treatment on CRS metal before plating [Malaysia]
42241. Galling of 316L on 316L [Massachusetts]
42242. LOOKING FOR PVC COATING LINES FOR GALVANIZED WIRES [Turkey] {9/14/06}
42243. Molarity of copper sulfate/sulphate for copper electrolysis [Australia]
42244. Decoating CrN from Al substrate [Italy]
42245. Consistent peeling problem in reel to reel plating [Malaysia]
42246. Dull tin plating [India]
42247. Alodine 1700 or Alodine 1700-1 [Turkey]
42248. What are the differences between Alodine 600 and the Alodine 1132 touch up pen [England]
42249. Aging of urea reactor studs [India]
42250. Ultrasonic cleaning of chromate conversion layer [Arizona]
42251. Chromate conversion coatings [Arizona]
42252. Compatibility of Stainless Steel and Galvanized Steel [California]
42253. Need nichrome wire [North Carolina] {9/14/06}
42254. NEEDED: Serious supplier for a pregalvanized sheet [North Carolina] {9/14/06}
42255. Need nickel plating/coating of plastic [Wisconsin] {9/14/06}
42256. Powder Coat Over Trivalent Chromate [Kentucky]
42257. HYDROGEN EMBRITTLEMENT SPECIFICATION WSSB P17-B1 [Michigan]
42258. Bathing in a galvanized steel tub [California]
42259. Teflon coating a glue roller to keep the glue from sticking? [Texas]
42260. Are there other coatings would be reasonable other than galvanization? [North Carolina]
42261. Stopping copper selenium blackening (gunbluing) from oxidizing [Canada]
42262. Chrome plating for steel fixtures installed in coastal regions [Canada]
42263. Reducing the maintenance of zinc phosphate [Mexico]
42264. Oxide on the stud [Mexico]
42265. Salt water rust corrosion on cast steel chuck [Minnesota]
42266. Metal Etching - Specialty Pattern [Australia] {9/14/06}
42267. Looking for Aluminum Twin Arc Spray Service [Malaysia] {9/14/06}
42268. Powder coat material [Florida] {9/15/06}
42269. Metal Plating [India]
42270. Effects on aluminum forms [India]
42271. Jeweler sized my platinum ring with different metal?! [California]
42272. BIRD BATH PAINTING [Colorado]
42273. Polishing an aluminum yacht hull [Florida]
42274. Powder coating over cadmium plating [California]
42275. Need the best product to protect Cast Iron Cookware that has been stripped to bare metal [Texas]
42276. Surface conductivity of zinc pre-plated steels with organic sealers applied [Colorado]
42277. Walterisation's "Deran C" [UK]
42278. Tough insulating coat for brass [Missouri]
42279. Electrolytic Ni/Au plating on PCB causing low thickness of Cu [Malaysia]
42280. Commercial black chrome [Illinois]
42281. Internal/External Corrosion In Galvanized-Copper Junction [Offshore Gulf of Mexico]
42282. Need my eyeglass frames gold plated [Minnesota] {9/15/06}
42283. Boron Carbide or Diamond Like Coating for Firearms [South Carolina]
42284. Finishing notes on a drawing [Colorado]
42285. Weathering properties of 6061 Al electroless nickel plated outdoors [California]
42286. OPAL FINISHING ON ALUMINUM SURFACE [Malaysia]
42287. Want to purchase non polluting metal treatment equipment to prep for powder coating [Connecticut] {9/15/06}
42288. RHODIUM PROBLEM [India]
42289. Plated contacts on tin oxide coated glass [UK]
42290. Brite dip for aluminum [India]
42291. Passivate finish vs. Cad Plating? [Washington]
42292. Need ZINC FLUX SKIMMING from Galvanizing plant [Taiwan] {9/19/06}
42293. NEED 16" aluminum wheels dipped in chrome [Florida] {9/19/06}
42294. Need consultant for rotary nickel screen manufacturing turn-key plant [Pakistan] {9/19/06}
42295. Why are pennies made of copper not silver like other coins? [Colorado]
42296. Galvanised steel roof [Australia]
42297. Process for high depth etching on STAINLESS STEEL [India]
42298. Gilding techniques [Virginia]
42299. Zinc Plating Specification ASTM A164 [Massachusetts]
42300. How ED paint adheres to zinc phophate layer? [Iran]
42301. Can polystyrene be metallized with silver, and how? [UAE]
42302. Rectifier for chromium plating [Algeria]
42303. Misplating on Parts [Canada]
42304. Mold component (416 stainless steel) [Ohio]
42305. Need 1" x 1" Nickel Inco Canada Nickel [Canada] {9/19/06}
42306. Where can I find a lab that can do a Salt Spray Test [China] {9/20/06}
42307. Looking for imitation enameling supply [Philippines] {9/20/06}
42308. Electroless Ni-P-SiC and Ni-P-Al2O3 [Iran]
42309. Electroplating of inorganic particles such as diamond dust [California]
42310. I want to find an enamel paint for old cabinet doors---I have about 80 of them [Indiana]
42311. Corrosion resistance on a Mexican beach [Canada]
42312. Difference between Zinc Gold Dichromate and Yellow Trivalent [Ohio]
42313. Weatherproofing steel without hot treatments [UK]
42314. Want to know reasons for PIT MARKS on galvanized sheet [India]
42315. How to remove Cl from a chrome tank [Indonesia]
42316. Anodizing vs. powder coating vs. Kynar application for outdoor aluminum extrusions [California]
42317. Peelable Maskant prior to Electroless Nickel Plating (Trike Elimination) [UK]
42318. Anti-corrosion/anti-tarnish coating for metallic fabrics [Philippines]
42319. Seeking Diamond Like Carbon Coating [Indonesia] {9/20/06}
42320. Gold or Copper Electroplating Equipment and Supplies [Ohio] {9/20/06}
42321. Automotive - acceptance criteria after salt spray test [Italy]
42322. Slime in water jet system [Maryland]
42323. Orientation of cylindrical parts in Salt Spray [Connecticut]
42324. ZINC COATING [India]
42325. Galvanizing [Saudi Arabia]
42326. White rust on galvanised steel tubes [Belgium]
42327. Hard Coat Anodize Clear, FDA [Illinois]
42328. Needs to setup titanium anodizing [Pennsylvania]
42329. Rusting of stainless steel grade 302 spring [India]
42330. Need my plastic side covers for Harley Davidson Road King chromed [Canada] {9/22/06}
42331. Chemical Polishing of Inconel 718 [UK]
42332. Etching aluminum leaving aluminum oxide [France]
42333. Effect of phosphoric acid and sulfuric acid in electropolishing of stainless steel [Philippines]
42334. How to make a spray pyrolysis machine ..homemade? [Philippines]
42335. Yellow aluminum siding turning black [Kentucky]
42336. Etching steel doors [Canada]
42337. Painting metal eyeglass frames? [Massachusetts]
42338. Replacement of Chromic Acid for Desmutting Molybdenum [Minnesota]
42339. Chrome plating on plastics [Pakistan]
42340. Welding electrode we should use on ss304 material for yellow passivation? [UAE]
42341. De-ionizing water for use on circuit board washing [Philippines]
42342. Surface treatment for copper alloy [Taiwan]
42343. Furnace / kettle design for the hot-dip galvanizing of garden furniture [Indonesia]
42344. Peeling of galvanized coating [The Netherlands]
42345. Forming titanium nitrate on titanium effect electrical resistance [California]
42346. Electroless nickel plating for food equipment [New Jersey]
42347. Request to get information regarding nickel coating solution [India]
42348. PLATING 12L14 STEEL [Illinois]
42349. Increasing the speed of cyanide zinc plating [India]
42350. Coffee color spots on the zinc plated surface of forged parts [Mexico]
42351. Electroless Copper Tape Mask [New York]
42352. Pit left on the electropolished surface [China]
42353. Stainless steel corrosion [Israel]
42354. Vibratory Ball Burnishing [Michigan]
42355. Chrome Plate Fiberglass and Urethane [Colorado] {9/22/06}
42356. Need electroless nickel plating service [Canada] {9/22/06}
42357. Gold Wash done on Silver in the late 1800's and early 1900's [California]
42358. Removing the melted plastic fan from the cast iron wood burning stove [Nebraska]
42359. What is acid pickling? [Pennsylvania]
42360. Black Oxide on UNS C36000 Brass [California]
42361. Vaccum metalizing [UAE]
42362. CHEMICAL CONVERSION COAT, Grade B? [Missouri]
42363. Bright clear type II anodizing in extrusion profiles [Mexico]
42364. Ryton Composite Material Electroless Ni Plating for EMI and Lightning Protection [California]
42365. Stripping zinc phosphating layer from iron [Iran]
42366. Removal of zinc plating for decorator purposes [Arizona]
42367. Need replated interior classic car pieces [Puerto Rico] {9/22/06}
42368. Need gold replating on several small items [California] {9/22/06}
42369. Need surface finish tester to check honing [India] {9/22/06}
42370. Need satin brushing machine [Jordan] {9/22/06}
42371. What happens when you mix copper wire and silver nitrate? Why? [Kansas]
42372. Is powder coating bad for the environment? [Australia]
42373. Gold plating equipment with pulse technology [Georgia]
42374. Secondary (sealer) treatments on electrical fasteners [Ohio]
42375. We are having high levels of Phenol, 2,4-Dimethylphenol and Chloroform in our waste water stream [Texas]
42376. Brass part oxidized - how to remove it?? [Canada]
42377. Painting problem - Aluminum diecastings [Indonesia]
42378. Nickel plating on sand cast aluminum [India]
42379. Can copper/nickel replace the clear chromate? [Florida]
42380. Improving black on zinc [New Zealand]
42381. Difference between non etch finish and anodizing [India]
42382. Seeking antique bronze refinisher for eyeglasses [New York] {9/25/06}
42383. Need rechroming of chrome wheels [Canada] {9/25/06}
42384. Supporting advertiser needs gold pigment for bar soap [Egypt] {9/25/06}
42385. Need a can of Alodine [California] {9/25/06}
42386. Explaining experimental phenomena observed during electropolishing process [Singapore]
42387. What analysis will help to characterize gold electroplating bath [India]
42389. Extracting gold from copper [Arizona]
42390. Corrosion and wear resistance [South Africa]
42391. Stripping Silver from a substrate (Nickel or Stainless Steel) [Canada]
42392. Nickel brass versus Brass with Nickel plate and Tin plate [Israel]
42393. Necessity of burnouts in heat treat furnaces [Virginia]
42394. What exactly is a non oxidizing furnace on a galvanizing line? [India]
42395. MoS2 with Electroless Nickel [Pakistan]
42396. Platinum Plating on a SiO2/ Si? [Korea]
42397. Contamination on Gold Plated Connector Pins [Singapore]
42398. Cleaning of high silicon aluminum die cast parts for stannate [Pakistan]
42399. Phosphated Pistons [Pakistan]
42400. How to achieve a glass-like finish on flat pieces of gold or silver [Florida]
42401. How to Spec and Quantify a Matte Finish [Texas]
42402. Choosing a decorative finish for seam welded steel cans [Ohio]
42403. Residential Marine Seawall -- Corrosion of Metallic Components [North Carolina]
42404. Seeking flawless brushes [UAE] {9/25/06}
42405. Good adhesion material for Si substrate and Gold?? [Michigan]
42406. Dimensionally Stable Anodes [Florida]
42407. UV testing [Ohio]
42408. Finishing of a highly-polished iron-nickel meteorite finger ring [Wisconsin]
42409. Tips to make chrome last [Philippines]
42410. Ultrasonic cleaning machine tank bottom gets pitting / corrosion [India]
42411. What is the best solution of minor acid spillage [Malaysia]
42412. Remove methylene chloride from a paint stripper [Spain]
42413. Underwater (fountain) black finish for a cast iron kettle [Mississippi]
42414. Powder Over Autodeposition [Utah]
42415. Bubbles in surface of clear powdercoat. Mild steel with no sand blasting. [Texas]
42416. Zincate bath formulation [Iran]
42417. Pinholes in Hard Chrome Plating [Colorado]
42418. Pitting Problems in Silver Plating [New York]
42419. Alternatives to chromate and surface pretreatment [Canada]
42420. Wetting tension testing of aluminum sheet [Illinois]
42422. Clear coat on aluminum [Colorado] {9/27/06}
42423. Using ultrasonics on aluminum parts [Australia]
42424. GOLD RECOVERY RELIGIOUS VESTMENTS ROBES [New Hampshire]
42425. Color plating of chrome vanadium sockets - what is THAT process! [Arizona]
42426. Black Patina for Copper [Michigan]
42427. How Toxic is Liver of Sulpher [Texas]
42428. Volumetrically analysing the level of CHLORIDE in acid tin sulfate plating baths? [India]
42429. Rusting of steel after powder coating removal [England]
42430. How to plate a conductive film inside of a plastic box [Turkey]
42431. Technical information on Nikasil cylinder bores on high tech engines [Texas]
42432. Tin plating problem [India]
42433. Gold plating over stainless steel and brass watches [Turkey]
42434. Chrome conductivity [Canada]
42435. Chromium (VI) alternative? [Denmark]
42436. Rohs Compliant Gold Alodine [Canada]
42437. Laser marking issues with 17-4ph(with passivation) [New Hampshire]
42438. Linished Finish Procedure [UAE]
42439. Need Chroming of Magnesium Wheels [Ohio] {9/27/06}
42440. Looking for a Mexico Powder Coating Co. [California] {9/27/06}
42441. Rechromer Needed in Orange County [California] {9/27/06}
42442. Stripping powder coat from wheels [California] {9/27/06}
42443. Cabinet pulls need refinishing [Illinois] {9/27/06}
42444. Matching Hard Anodizing on 6000 and 7000 Aluminum [Utah] {9/27/06}
42445. Need anti tarnishing chemical for gold [India] {9/27/06}
42446. How can I etch markings on INOX 316 L stainless steel [Belgium]
42447. Electroform sticks to cathode [Canada]
42448. Restoring gloss to E and G gold grill [Florida]
42449. How to achieve Rusty Exterior Cladding [New York]
42450. Preparing aluminum siding [Nebraska]
42451. Renovating bathroom fixtures, faucets/spouts [New Jersey]
42452. Potential for animals to become ill from prolonged licking of galvanized steel pipes [Nevada]
42453. Tannic acid rust conversion primer test method? [Pennsylvania]
42454. Galvanized (Zinc) Steel and EMI problems possibly due to Zinc Oxide? [Pennsylvania]
42455. Fast coppering of steel wire [Chile]
42456. Impurities in Hard Chrome [India]
42457. Zinc plating peeling/blistering off [Singapore]
42458. Micro bubbles on copper plating [Illinois]
42459. Dyeing at room temp [Florida]
42460. Chemical conversion coating on edm surfaces [Massachusetts]
42461. Molybdenum plated Copper wires [India] {9/29/06}
42462. Where to get rims dipped [Texas] {9/29/06}
42463. Seeking a clear coating for titanium [Washington] {9/29/06}
42464. Seeking electrophoretic plating process job shop [New York] {9/29/06}
42465. Temperature effects on latex paint [Florida]
42466. Help, pulsed plating alloy [West Virginia]
42467. 6A14V Titanium and S30V Stainless Steel in a durable flat black finish [Indiana]
42468. Freezer rust [Indiana]
42469. Surface smoothness differences between tri-valent and hexavalent chromate [North Carolina]
42470. Titration procedure for permanganate [Ohio]
42471. Improving CASS life of rims for motorcycles [India]
42472. Hydrogen pick-up test; reaction plan [Michigan]
42473. Replacing trike from a degreasing process [England]
42474. Clear heat proof satin finish for mild steel kiln frame? [California]
42475. Gold passivated zinc vs. galvanizing vs. chemical nickel [Australia]
42476. Cleaning carbon contaminated 316 stainless steel [UK]
42477. Green residue on 410 stainless bolts [Illinois]
42478. Plating on Sintered Metal Parts [Ohio]
42479. Need Rechroming [Bahamas] {10/2/06}
42480. Need brass finish applied to stainless steel doorhandle [California] {10/2/06}
42481. Hot-dipped galvanized nails compared to electro-plated nails for Hardieplank siding [Georgia]
42482. Is phosphate coat on zinc plating RoHS compliant? [California]
42483. Powdercoating conveyor belt rollers [Australia]
42484. Electroless Nickel / Hard Chrome Plating Hardness [Georgia]
42485. Solutions for testing the presence of hard chrome on materials [Oklahoma]
42486. Trivalent Hard Chrome? [South Carolina]
42487. Replating ductile iron [New York]
42488. Need Powder Coating on a 5" dia. X 13 foot long aluminum tube [New Jersey] {10/4/06}
42489. Need anodes for electrowinning of lead [Chile] {10/4/06}
42490. Look for medical coating material [Turkey] {10/4/06}
42491. Why in pvd need vacuum pressure? [Malaysia]
42492. Electroplating of Nickel from NiSO4 solution [Malaysia]
42493. Seeking an electrically conductive aluminum coating [Illinois]
42494. Charcoal filter for sulfamate [California]
42495. I HATE THE COLOR OF MY RIMS! [California]
42496. Where can I buy liquid stone to duplicate my sculpted statues [Pennsylvania]
42497. Cleaning a Galvanized Steel Stock Waterer Used as a Bathtub [Virginia]
42498. Treatment of the side effects of the pretreatment of the aluminum profiles [Sudan]
42499. Removal of thermal spray coatings ( WC-Co ) from Steel plate [Malaysia]
42500. Procedure of powder coating and pre coating correct treatment with time [India]
42501. Plating silver on steel [Rhode Island]
42502. Nickel Underplating Thickness for Gold-Tin Solder Bonding [Singapore]
42503. Electroplating gold with an alloy of copper and silver [India]
42504. Looking for polishing solutions for non-ferrous castings. Outsource? Buy advanced technology? [New York]
42505. Stainless steel blackening relief [Egypt]
42506. Slip and Fall Waiting to Happen - Removing Sealer/Finish from Concrete [South Carolina] 2nd Request
42507. Will an e coating finish resist rust [Pennsylvania]
42508. Need Casket Handle and Bars [Puerto Rico] {10/4/06}
42509. Silverplate a tumbler [Florida] {10/4/06}
42510. Bead Blasting Help [New Hampshire] {10/4/06}
42511. Looking for electroless copper plating on plastic [California] {10/4/06}
42512. Stainless Steel - Cosmetic Finishes [England]
42513. Anticorrosive treatment for MS (CR/HR) telescope covers [India]
42514. Cleaning Stainless Steel Air Pipe [Arizona]
42515. Tin tank standards? [Georgia]
42516. About the dissociation constant of ammonium fluoride [Taiwan]
42517. How to prevent blackening corrosion in head space of tinplate cans [Thailand]
42520. Need dipping of 1949 Tokheim gas pump for rust removal [Iowa] {10/5/06}
42521. Recovery of nickel from nickel oxide [Malaysia]
42522. Wire for wind chimes? [Canada]
42523. Aluminum Hydroxide Polymer Control [Nevada]
42524. Cu over Zn Diecasting causing blistering [South Carolina]
42525. Any suggestion for a suitable Aluminum Etchant for silicon wafers? [India]
42526. Chock of the ball valves after attack by 96% sulphuric acid [Bulgaria]
42527. Swimming pool finishing: Resistance of powder coating to Chloro [Brazil]
42528. Disadvantages of trivalent chrome for hard chrome plating? [Trinidad]
42529. Removing Welding Stinct from SS 316 Boxes [India]
42530. How to do stainless steel satin finishing with HNO3 / HF chemicals? [India]
42531. Removing Oxidation from Kovar [Turkey]
42532. Water based rust inhibitors for lubrication during lapping of 17-4 (modifed 630) SS? [Ohio]
42533. Hydraulic tank materials [Canada]
42534. Need big wheels show chromed [Wisconsin] {10/6/06}
42535. Looking for an Italian chemical plating company [Iran] {10/6/06}
42536. Seeking USA facility / job-shop for aqua regia processing [Ohio] {10/6/06}
42537. Need a good process for chrome-like powdercoating [UK] {10/6/06}
42538. Need a new plating thickness measurement machine [Thailand] {10/6/06}
42539. Plating shop needs White Gold Plating Process [Peru] {10/6/06}
42540. Looking for a plating supplier for brighteners and additives [Iran] {10/6/06}
42541. The Time It Takes to Rust With Contaminants [Georgia]
42542. Gold Electroless Plating on Graphite Composite [New York]
42543. Plating Stainless Steel with Iron [Texas]
42544. Need to paint anodized aluminum [Alabama]
42545. Lacquer chrome [Ireland]
42546. Chrome plating and powder coating [Massachusetts]
42547. Can I polish car steel parts like chrome [Ohio]
42548. Setting up a Gold Plating Company [India]
42549. Stripping Gold and Electroless Nickel from Aluminum Alloys [Missouri]
42550. Zinc Whiskers in a Data Center - Pregalvanized, Hot-dipped Galvanized, Electroplated Zinc? [Ohio]
42551. Relationship between kettle size and capacity? [Iran]
42552. Electroless Nickel Plating Versus Nickel Electroplating [Illinois]
42553. Red rust on chrome plated wire [Tennessee]
42554. Silver anodizing of 16 or 14 gauge wire [Maryland]
42555. Alodine1200 and Steel nutplates [New Jersey]
42556. Need old penn reels to look new for display [Florida] {10/6/06}
42557. SEEKING ANODIZING OF 2024-T351 AL IAW MIL-A-8625 TYPE II CLASS 2 DYED ORANGE 3A [New York] {10/6/06}
42558. I want lacquer for vac. plating [Iran] {10/6/06}
42559. Wanted a brand new vacuum metalising plant from China [India] {10/6/06}
42560. Need 2 tons of nickel anode material [South Africa] {10/6/06}
42561. Need to remove Silicon[e] spray [Florida]
42562. RoHS exemption of Hexavalent Chrome? [China]
42563. What is P16TF3 copper nickel - indium alloy? [Kansas]
42564. Removal of heat scale from annealed electroless nickel deposit [Illinois]
42565. Defective on trivalent yellow [Malaysia]
42566. Alodine 1200S for low resistance coating per AMS 2474 ? [Poland]
42567. Corrosion Pitting Evaluation [Florida]
42568. Masking in PVD process [Connecticut]
42569. QQ-P-35 Type Vl, better or worse than A 967-05 [Missouri]
42570. Who can Nickel Plate to ASTM B607-91? [Tennessee] {10/6/06}
42571. Need equipment to test plating thickness [Missouri] {10/6/06}
42572. Need Barrel Plater for Hex Yellow Chromate Zinc [Missouri] {10/9/06}
42573. Want chrome finish on BMW wheels [Illinois] {10/9/06}
42574. Chrome Replating [New York] {10/9/06}
42575. Need a New Holland 12"x12" Spin dryer [Wisconsin] {10/9/06}
42576. Restoration of old magnesium parts to as new [Illinois]
42577. Need Nadcap approved source for chem film mil-c-5541 class3 the parts are over 120 inches long [New York] {10/10/06}
42578. Building a plating facility in Central America [Guatemala] {10/10/06}
42579. How do I remove rust from hard to reach areas from an outdoor wrought iron rail? [Canada]
42580. Anodized copper sinks [Colorado]
42581. Ebonizing [Tennessee]
42582. M E Q Vs PH [India]
42584. Aluminum dyeing to appear Oil Rubbed Bronze [Colorado]
42585. Request Part number of paint for spec BAC 7144, Y-value 0.73 [UK]
42586. Excessive Aluminum in Zinc [Northern Ireland]
42587. Masking welds prior to Anodize operations [Alabama]
42588. Need German buffing bar for wood finishing [India] {10/10/06}
42589. Denture Electropolishing [Poland]
42590. Determine the concentration of hypophosphorous acid in presence of tin [China]
42591. Large paint dipping tank service needed [California] {10/11/06}
42592. Seeking a Phosphating Supplier [Texas] {10/11/06}
42593. Seeking pickling equipment [Italy] {10/11/06}
42594. Starting a zinc plating shop - need equipment [South Carolina] {10/11/06}
42595. Properties of Chromium [Pennsylvania]
42596. Electropolishing Reaction [Indonesia]
42597. Rust on chrome forged Titleist irons [Canada]
42598. Aluminum additions in zinc kettle [Saudi Arabia]
42599. PdCoAu plating heat treating
42600. HOW TO TREAT PHOSPHATING SLUDGE [India]
42601. Protecting MIL-C-26482 Electrical Connectors from Corrosion [Texas]
42602. Avoiding heat distortion on solid aluminum block [California]
42603. Who can change the finish on stainless item to bronze? [New York] {10/11/06}
42604. What is envolved in dip stripping carbody parts [South Carolina]
42605. Problems with pitting [Scotland]
42606. Dots on the surface after black anodizing [China]
42607. Need the best centrfugal metal finish machine [Washington] {10/12/06}
42608. Brown effect on aluminum degreasing with an alkaline -- WHY?! [UK]
42609. Chemical resistant coating on brass that can withstand 100 deg C [India]
42610. How do I achieve OEM-like paint look on my vintage motorcycles? [California]
42611. Guilding a cast lead object [Virginia]
42612. How do I tarnish stainless steel [Missouri]
42613. Another question for outdoor statue [Indiana]
42614. Stripping baked on paint from aluminum rims [Kentucky]
42615. Phosphoric acid sludge removal [Saudi Arabia]
42616. Chemical effects of Inhibited HCL on Nonmetallic elements (Like Rubber plastic and nylon) [India]
42617. Electrorefining/electrowinning gold [Texas]
42618. Test for Chromate Conversion Coating on Aluminized Steel [New Zealand]
42619. Different angles of measurement and the possible interrelationship [India]
42620. Powder Coating vs Electro-Discharge [Wisconsin]
42621. Galvanneal [Iran]
42622. Need harder electroless nickel on copper [Illinois]
42623. Uneven tin plating thickness (MSA base) [Malaysia]
42624. Zinc chromate finish is rusting (red) very badly at seam [Tennessee]
42625. Remove the etching that occured from concrete splashing against anodized aluminum finish [California]
42626. Corrosion resistance and extra white finish for stainless steel investment castings [India]
42627. Does the electro polishing for cr-co dentures effect the thickness and if yes how? [Jordan]
42628. Will water passing through copper stain stainless steel? [New York]
42629. Leachate treatment [Malaysia]
42630. Automotive crinkle, bubble, splatter finishes on exterior [Georgia]
42631. Ceramic floor etching [Oregon]
42632. Rusty refrigerator [Barbados]
42633. "Finish" specification for 7075 aluminum part [Illinois]
42635. Type II vs Type VIII passivation of 17-7PH SS [Texas]
42636. RA Finish on phosphate and oil parts [Ohio]
42637. Un-phosphating area at metal sheet [Indonesia]
42638. How to increase surface roughness of zinc phosphate? [Taiwan]
42639. Requirement of cataphoretic painting in black color [India] {10/12/06}
42640. Need to find supplier for steel shot media [China] {10/12/06}
42641. Electrolytic Ni/Au [Malaysia]
42642. Chrome wheels damaged by HCl [UK]
42643. Brightening of copper radiator without harming solder [India]
42644. Pinhole problems [Brazil]
42645. Engelhard E-74 Gold Plate Make Up Bath [California]
42646. High brightener content and roughness on rack acid zinc work [England]
42647. HCD area has low tin thickness [Malaysia]
42648. Rusting of cast iron parts [India]
42649. Need Sodium Bichromate [Vietnam] {10/13/06}
42650. Test to indicate ready to chrome plate [Oklahoma]
42651. Want to create a "brushed" metal look on a spray painted lamp [Texas]
42652. The advantage of using trivalent chromate for galvanic protection [Canada]
42653. Need guidance on qualification standards and procedures for a Ni on 303SS plating [Massachusetts]
42654. Aluminium specification code for L110 and L165 [Australia]
42655. Which salt spray method is best? [Michigan]
42656. PVD coating questions [India]
42657. Blisters on ABS Electroplated part after shipment [India]
42658. Thermal vacuum furnace processing of Glass-Metal sealed sensors or switches [Tennessee]
42659. White rust issue [India]
42660. 8625, Type II, Class 2 Black anodize on 2024-T351 alum. rubs off. [Massachusetts]
42661. SS Weld is discolored [India]
42662. Need Din 12476 finish for metal fastener [Illinois] {10/13/06}
42663. Need Chrome Dipping [North Carolina] {10/13/06}
42664. Seeking melonite QPQ process in Far East (China, Taiwan, or Hong Kong) [Florida] {10/13/06}
42665. Need carbon fiber finish on auto parts [Florida] {10/13/06}
42666. Looking for leadframe plating laser mask [Singapore] {10/13/06}
42667. COATING FOR SS FABRICATED TANK [India] {10/13/06}
42668. Need high purity Zinc balls [Louisiana] {10/13/06}
42669. Discoloration of Ti64 after annealing [Florida]
42670. Copper or nickel activation prior to plating [Philippines]
42671. Air agitation for acid chloride zinc plating bath [South Africa]
42672. Metal roofing ground contact [Vermont]
42673. Hard Chroming a Crankshaft [California]
42674. Painting gloss white on bare aluminum [Washington]
42675. Applying colour to small soldered brass components [UK]
42676. Help with Temperature Controllers [Texas]
42677. Separation of Copper from Nickel [India]
42678. Coloring of anodized aluminum [India]
42679. Vapor polishing [North Carolina]
42680. Want retinning of copper pot [New York] {10/16/06}
42681. Seeking powder coat of tubular yacht parts [Michigan] {10/16/06}
42682. Need chrome or nickel plating over anodized aluminum fixtures [Massachusetts] {10/16/06}
42683. Aerospace Surface Treatments (Pickle/Anodise) - India, Bangalore [Scotland] {10/16/06}
42684. Requirement of Phosphating, Degreasing, Blackening, Iron Phosphating formulations know how [India] {10/16/06}
42685. THIXON 422 [Italy] {10/16/06}
42686. ELECTROCOAGULATION FOR TREATMENT TEXTILE WASTEWATER [Indonesia] {10/16/06}
42687. Need a Nickel Acetate Sealer [Virginia] {10/16/06}
42688. ELECTROLYSIS OF A COPPER SULPHATE SOLUTION HELP PLEASE! [UK]
42689. Finding out a weight needed to get 1mg N/L [UK]
42690. Electroplating for a double side PCB in home/college [India]
42691. Please suggest jet black colour with coating other than DLC [India]
42692. How can I clean gold plated wheels or wire spokes? [New York]
42693. How do I prevent fibreglass to attack my styrofoam mold? [South Africa]
42694. REMOVING SILVER FROM OLD SILVERPLATE HOLLOWARE [Washington]
42695. Spiral staircase in copper color paint [Arkansas]
42696. Learning the pH for chemical dipping [California]
42697. Mixed Bed Regeneration: Effluent Water [India]
42698. Helicopter Pad, appropriate paint [UAE]
42699. Adhesive for aluminum to aluminum or steel to aluminum? [Spain]
42700. White rust on HDG sheet metal parts [Alabama]
42701. Need procedure to plate antique pewter part [Iowa]
42702. How-to for abrasion and corrosion resistant aluminum machine part? [Missouri]
42703. Which chemical is used for etching of stainless steel? [Oman]
42704. Need bath faucet replated in place [Connecticut] {10/19/06}
42705. Need magnesium alloy test panels for automotive application [New Jersey] {10/19/06}
42706. Need Aluminium Anodizing Equipment [India] {10/19/06}
42707. Anodes for wood nickel strike [Colorado] {10/19/06}
42708. Iron nail in magnesium sulfate and vinegar [Philippines]
42709. Best Electroplating Experiment [Illinois]
42710. Electroless and Electrolytic Copper Plating on Ceramic [Malaysia]
42711. Anodizing of 2219 aluminum alloy [Pakistan]
42712. Silver items [Texas]
42713. Electroplating rhodium on silver plate [New Jersey]
42714. How to strip and recover Silver from Alloy 42 parts [India]
42716. Tribostatic/electrostatic technology [North Carolina]
42717. Coating thickness variations at fluidized bed coatings [Turkey]
42719. Hard chrome plating in parallel [India]
42720. Electrical difference between Nickel Flash and Silver Flash [Connecticut]
42721. High Speed Chrome Plating [India]
42722. Zinc Chromate Plating Surface Corrosion [Texas]
42723. Passivating stainless steel tanks [Washington]
42724. Hair line finishing on Stainless Steel [India]
42725. SS cut wire shot blasting to SS surface [India]
42726. Methodology for sandblasting to SSPC Sa 2.5 [Philippines]
42727. Need to replate jacuzzi hardware in polished nickel [New Jersey] {10/19/06}
42728. Will end of life directive go to the spare autoparts and replacement autoparts? [Mexico]
42729. Chrome Grohe Tub Filler needs refinishing [Utah] {10/23/06}
42730. Scratches in brass belt buckle! [Florida]
42731. Producing a pattern of deep and complex cuts into mild steel and bronze through etching [California]
42732. Conforming anodes and pumping through of electrolyte [California]
42733. My trumpet [South Carolina]
42734. Sublimation Coating (Mugs) [Brazil]
42735. Corrosion resistant plating for spring battery contacts requiring submersion [Iowa] 43404. EN plating applications [India]
42736. How do I plate to obtain a antique gold finish/matt gold finish and matt silver finish? [China]
42737. Zinc plating heat treated steel [Idaho]
42738. Alodine help for a rookie [Wisconsin]
42739. Dark smut on conversion coated cast aluminum parts [California]
42740. Iron Phosphate on Zinc Electro-Deposition? [North Carolina]
42741. Ceramic Epoxy versus Hard Chrome [Georgia]
42742. Need chrome plating of fiberglass hubcap [Puerto Rico] {10/23/06}
42743. Does anyone know of any gold and silver recovery services? [Texas] {10/23/06}
42744. Need copper pot retinned [New York] {10/23/06}
42745. NEED SILVER PLATING ON STAINLESS STEEL AND PROTECTION [India] {10/23/06}
42746. Platinum Plating Electrodes for Fuel Cell use [Florida]
42747. Is hard anodizing influenced by size factor of component? [India]
42748. I need the definition of chrome layer (chemical film).... thanks a lot! [Taiwan]
42749. Standard peeling test for copper plated with Sn (after bending for surface mount devices) [Taiwan]
42750. Is there any chances of bed separation if bed is in idle condition for 3 to 4 days? [India]
42751. Powder coating spec info needed [Massachusetts]
42752. How long does galvanized plating last? [Florida]
42753. Black Hardcoat Knurled Handle [Rhode Island]
42754. Hard anodize 7075 surface finish [Idaho]
42755. Making microchannels on stainless steel [India]
42756. What is the method for chemical etching [Thailand]
42757. Soft Iron Anode info [UK]
42758. Need gold dipping of marble statue [India] {10/23/06}
42759. Looking to restore chrome luggage rack for vintage car [Wisconsin] {10/24/06}
42760. Need SUS 304 No. 8 Mirror finish and Shot finish - Colour: Neues Sputtering Gold [Singapore] {10/24/06}
42761. Wanted polyurethane floor coating technology [India] {10/24/06}
42763. Removing small scratches in chromed billet Harley part [Michigan]
42764. Bleach stained galvanised metal equipment [Florida]
42765. Confused about "acid test" for silver and other precious metals [Florida]
42766. How to smooth/eliminate scratches on stainless steel farberware frying pan [Washington]
42767. Oxidizing or patinizing steel to matte gray [Michigan]
42768. Removing paint from an old brass fire extinguisher [Australia]
42769. Needing info on chroming business [Florida]
42770. Heat treating air quench contamination - NH3 (ammonia) [Illinois]
42771. Interpretation of ISO 10555 "corrosion" [Ireland]
42772. Antiquing solution for brass plating and silver plating [Philippines]
42773. Direct coating on brass substrate in vacuum chamber [India]
42775. Conductive paint [Missouri]
42776. Add additional thickness on anodized layer [Malaysia]
42777. Black tiny patches on the anodized aluminum sections [Iran]
42778. How to prepare passivation solution for SS304 fabricated parts to avoid rust [UAE]
42779. Stainless Steel Crevice Corrosion Problem [Australia]
42780. Thickness measurement for hard anodising and zinc nickel alloy plating [India] {10/24/06}
42781. 'Tiger Stripe' phenomenon in Black Anodize Electrolytic Coloring [Singapore]
42782. Need acid dipping of '56 Ford truck [California] {10/24/06}
42783. Need a stainless steel kitchen hood refinished [Pennsylvania] {10/24/06}
42784. Looking for electropolishing training software [Ohio] {10/24/06}
42785. How to use ferric chloride to clean water [California]
42786. Stainless steel oxidizing with porcelain dishes, stoneware, etc. [Connecticut]
42787. Titration procedure for oxalic acid anodizing bath [Sweden]
42788. Chemical etching of molds [India]
42789. Nickel vs Bright nickel and its affect on DCR [Florida]
42790. Required imformation regarding teflon fep [Pakistan] {10/24/06}
42791. How to remove oxidation from galvanized metal [Oklahoma]
42792. Logo printing on polypropylene bag [Illinois]
42793. Need a contact for a company who copper plate leaves [Maryland] {10/25/06}
42794. Want recovery equipment for reuse of spent pickle liquor [India] {10/25/06}
42795. Anomalous anode dissolution in tin electrorefining [Canada]
42796. Tank material selection for 200 deg F chromic acid [Oklahoma]
42797. Aluminum Alloy B-535.2 Hard Anodize Surface Treatment (Seawater App) [Arizona]
42798. Need motorcycle side cover chrome plated [Arizona] {10/27/06}
42799. Homemade brass cleaning polish/cream [India]
42800. Mirror Finishing on Low Carbon Mild Steel Galvanized Wire [India]
42801. Need Ti Passivation service [Georgia] {10/28/06}
42802. Automatic machine for silver recovery from waste [India] {10/27/06}
42803. Black spots on Zn-Ni plated parts [South Carolina]
42804. Titration of silver nitrate [India]
42805. Aluminum/Masonry damage to Anodized Aluminum [California]
42806. Paint removal on chrome rims [Tennessee]
42807. Painting my BMW 528i in Mirrachrome [Illinois]
42808. Need to know viscosity of Nickel Sulfamate [New York]
42809. Stripping silver plate from nickel silver [Connecticut]
42810. Using titanium chips to remove contamination from a vacuum furnace [Arizona]
42811. Silkscreen mesh line appear on printed surface [Canada]
42812. Bulk lacquering process for fish hooks [India]
42813. Rust on inner diameter (Surface Area) [Philippines]
42814. Platinum Electroplate on Molybdenum [Oregon]
42815. How to remove sodium carbonate from aluminum [Florida]
42816. Black Passivate 303 Stainless Part [Connecticut] {10/30/06}
42817. Need machinery for gold and chrome plating [India] {10/30/06}
42818. Friction material with high coefficient of friction [Missouri] {10/30/06}
42819. Discoloration of Titanium Nitride (TiN) coating on stainless steel substrate [Hong Kong]
42820. What are contents of the 7.5% in silver jewelery [New Jersey]
42821. Silver etching [Florida]
42822. Hot Rod Restoration [Illinois]
42823. Brass fittings on antique cars and tarnishing [Canada]
42824. Ford plating spec [Ohio]
42825. Scrubber on top of fumehood [Singpaore]
42826. Tarnished copper parts [Mexico]
42827. Shock Absorber Springs Powder Coating [India]
42828. Required Glass Beeds/Shot Blasting/other finishing equipment for Aluminum Die castings [India]
42829. Carbon removal [Indiana]
42830. Pitting problem in 316L reactor [Georgia]
42831. Corrosion of the interface between a brass stud screwed into an aluminium body. DC Electrical Current carrying. [Australia]
42832. Requirement of Insulation material between Galvanised Steel and Aluminum [Saudi Arabia]
42833. Need 99.99 % pure iridium powder [India] {10/31/06}
42834. Need used automotive paint booth [Florida] {10/31/06}
42835. Need Dioxane chemical solvent [Greece] {10/31/06}
42836. Need help with small scale electropolishing of stainless steel [Florida]
42837. Relationship between thickness of oxide layer and time/ voltage for anodizing Al-Alloys [Pakistan]
42838. Wish to clean black residue from harrow disk after electrolysis removal of rust [Oregon]
42839. Muriatic acid used in a lavac toilet [Texas]
42840. Gun blueing at home [Texas]
42841. Powder coating: galvanneal vs. straight cold rolled [Illinois]
42842. Rusted hot dip galvanized bolt and nuts [Malaysia]
42843. Nickel plating on large/flat brass surfaces trouble [California]
42844. Sealing problem after anodising [India]
42845. Want automotive body paint stripping [Rhode Island] {11/1/06}
42846. Need plating (not anodizing) of aluminum extrusions [California] {11/1/06}
42847. Want to Rent or Buy Used Small Oven for Refining Gold [Germany] {11/1/06}
42848. Acetylene as Semi Bright Nickel Plating additive [Pakistan]
42849. Bubble traces observed in electropolishing copper [Hong Kong]
42850. Chrome 6 (Hexavalent Chrome) Passivation Lifetime [Malta]
42851. RoHS verification [New Jersey]
42852. Cleaning and rinsing filtration systems [Florida]
42853. Curing Test on IZS Primer and Adhesion Test on IZS+Silicon Acrylic System [UAE]
42854. Interface adhesion for coupling iron shaft - zinc galvanized iron sheet [Italy]
42855. Lead-cadmium in electroless nickel [India]
42856. Electroless nickel plaing - effect on fatigue strength [UK]
42857. Sodium Dichromate Dihydrate contamination in Cadmium plating vat [UK]
42858. Reoxidizing trivalent chrome to hexavalent [Michigan]
42859. Passivation Fluid Testing and Criteria [Indiana]
42860. Pre commissioning process for stainless steel tank [Iran]
42861. Etching of steel without etching ZnO [USA]
42862. Suitable adhesive for steel fiber [Malaysia]
42863. In need of a custom plater for abs plastic application small to low volume parts [Indiana] {11/2/06}
42864. Manufacturing acid stains [Florida]
42865. Refinish White Cast Iron Bed [New Jersey]
42866. Is chrome clear? [Illinois]
42867. Boric acid analysis [Hong Kong]
42868. Powder Coating on Aluminum Castings [Pakistan]
42869. Cycle Times for Anodizing, Bright Chroming and Electropolishing [Michigan]
42870. Aluminum alloy etching process [India]
42871. Will 316 SS corrode/rust when immersed in hard water environment? [Singapore]
42872. Need Sheradized Coating [China] {11/2/06}
42873. Need polyurea application in the Philippines [China] {11/2/06}
42874. Need Micro Plating System [India] {11/2/06}
42875. Suspending iron objects in copper wastewater [Michigan]
42876. Oxidation from Tin II to Tin IV [Canada]
42877. Cloudy Bright Nickel Plate [California]
42878. Reduction reaction causing pitting in 316L reactor [Georgia]
42879. Stainless surface prep [California]
42880. Zinc compatible with copper [Missouri]
42881. Is a zinc handle considered rust-proof? [California]
42882. Need System for Powder Coating of Fastener Heads [Australia] {11/2/06}
42883. Can you colour platinum [UK]
42884. Need a copy of Lockheed PB78-509 [California]
42885. Pin Holes In Compressor Guard [India]
42886. How to do quick electroplating of shoe molds? [Missouri]
42887. Plating Tin-Nickel on Magnesium Alloy [China]
42888. Thickness vs. Time for Barrel Plating System [Brazil]
42890. Oil free stainless? [New York]
42891. Corrosion of surface condenser in seawater [Iran]
42892. Need machine to sputter coat razor blades [Iran] {11/2/06}
42893. How can I age brass to uniform dark finish [Texas]
42894. Wrought iron acid wash [Mexico]
42895. Liquid Metal Embrittlement issues with rolled steel shapes [Virginia]
42896. Need dipping of factory rims [Florida] {11/3/06}
42897. Seeking platinum electroplating on plastic [Wisconsin] {11/3/06}
42898. I need my factory 03 Navigator grill assembly chromed [Ohio] {11/3/06}
42899. Alumina oxides electroplated on a aluminum fin [Texas]
42900. Restore antique gun metal finish that was mistakenly "cleaned" off [Missouri]
42901. Are the fumes from dipping metal in zinc galvanizing dangerous [Nebraska]
42902. Digesting A Wastewater Sample [Pennsylvania]
42903. Automatic Passivation Equipment - and control of [Iowa]
42904. Rust issues using Manganese Phosphate. The parts are 4130 cold drawn steel. [Tennessee]
42905. Distribution profile of current density in oblique barrel plating [India]
42906. Reduce COD level [Pakistan]
42907. Brown stains on nickel plated materials [Philippines]
42908. Need Brass Plating Shop [Illinois] {11/7/06}
42909. Looking for a continius hot dip galvanizing line [Turkey] {11/7/06}
42910. Need electronic SILVER / GOLD purity tester [Thailand] {11/7/06}
42911. Need State-of-the-art Metal Finishing / Plating Shop [India] {11/7/06}
42912. Looking for test method [South Africa]
42913. Copper filling of 20-25 um PTH [Philippines]
42914. 1-3 Meg-Ohm-cm water needed for plating line? [Colorado]
42915. Zinc-Nickel Electroplating of Fasteners [Canada]
42916. Yellow patches in finished coatings of alkaline noncyanide zinc plating [India]
42917. CHROME OR RHODIUM PLATING ALUMINUM [Canada]
42918. Rinse maintenance [Mexico]
42919. Conductivity control [Australia]
42920. Dining chairs need rechroming before reupholstering [California] {11/8/06}
42921. Nickel S Round [India] {11/8/06}
42922. Paste or gel etchant for stainless steel before NDT inspection [Canada] {11/8/06}
42923. Looking for In Mould Coating formula in PU industry [China] {11/8/06}
42924. Siderophore production [India]
42925. Aluminum brazing compound [New Jersey]
42926. Brown Black color on 1018 steel for interior display [Maine]
42927. Aluminium Window Corrosion [Gibraltar]
42928. Clear coat Breaking up [North Carolina]
42929. Fresh machined aluminum looks like its galvanized? [South Carolina]
42930. ASTM B633-98 std: Electrodeposited coating of Zinc [Singapore]
42932. SILICA REMOVAL IN LIME SODA SOFTENING [India]
42933. Powder coating vs anodising on engine room deck plates [The Netherlands]
42934. Can we get jet black colour with CrCN coating [India]
42935. LAMINATED PEEL OFF PROBLEM IN TRINICKEL PLATING [India]
42936. Surface treatment for 4736 mg Alloy [Turkey]
42937. Concrete filling of aluminum columns [Florida]
42938. Rust on 300 series SS [New York]
42939. Need Internal Hard Chrome Plating of Shotgun Barrels [South Dakota] {11/8/06}
42940. Want to know plating company that does plating and electroforming using aluminum [South Korea] {11/8/06}
42941. Nickel Plating of Antique Car Clock Parts [Pennsylvania] {11/8/06}
42942. Need a 90" diameter Ring Coated for Composites Manufacturing [Michigan] {11/8/06}
42943. Need Black Chrome Plating [Wisconsin] {11/8/06}
42944. Need quotation for zinc ingots 99.995% for galvanizing [Saudi Arabia] {11/8/06}
42945. Request antifingerprint coating chemicals [China] {11/8/06}
42946. Cost of Decorative Chrome Plating [UK]
42947. Specification ZNIA3L-Silver for Coating? [India]
42948. Gold Plating of Seashells [California]
42949. About the chromate conversion of zinc plating [India]
42950. About the automatic line of zinc plating [India]
42951. Remedy for Hydrogen Embrittlement [India]
42952. Deposit on the Anode [India]
42953. Aluminum galling [Florida]
42954. Spray to find the Stainless Steel Grades [Saudi Arabia]
42955. Need Bluing of Welded Frames [Oregon] {11/8/06}
42956. Zinc Anode for Metal Railings [New Hampshire]
42957. Looking for a chemical reagent that can help in an ultrasonic cleaning of CoCr (L605) alloy [New York]
42958. Looking for a titration method for ferric chloride [New York]
42959. SCREEN PRINTING ON BARE ALUMINUM [Ohio]
42960. Can you selectively plate plastics by overshooting areas with a non plateable grade resin? [Michigan]
42961. Blisters in Hard Coated 7075 [New Jersey]
42962. Recommend a Finish for AISI 1095 Carbon Steel [California]
42963. Need powder coating of aluminum tubes [California] {11/10/06}
42964. Aluminum surface treatment for marine use after anodization process [Hong Kong] {11/10/06}
42965. Need to substitute stainless steel for plated or coated carbon steel [Connecticut] {11/10/06}
42966. Need 2 - 5000 and 1 - 500 gallon tanks [Wyoming] {11/10/06}
42967. Need nonconductive high emissivity coat/paint, that can be easily removed [Arizona] {11/10/06}
42968. Nickel strike on Glidcop and brazing [Switzerland]
42969. Plating Process Area Sprinkler Risk Analysis [Iowa]
42970. Mechanical plating large components [India]
42971. Coloration of Nitride Parts [Colorado]
42972. Brown staining on electroless nickel plating [South Africa]
42973. Plating Machined ABS [Massachusetts]
42974. Cloudy zinc, after heat is applied [Canada]
42975. Trivalent Chromium Plating [India]
42976. Noncoloring conversion coating on edges [Korea]
42977. Need a pair of child's shoes metallised [England] {11/10/06}
42978. What aluminum finish on 70s Coke machine? [North Carolina]
42979. Removing surface rust from blasted Camaro [Louisiana]
42980. Electroless Black Nickel [Malaysia]
42981. Metal plating cost calculation based on A/dm" (or A/sqft) [Brazil]
42982. How do you accomplish a us 26 finish [Wisconsin]
42983. Need a powder coating plant [UAE] {11/10/06}
42984. Need 5mm Bar suitable for sea water [England] {11/10/06}
42985. Copper plating an aluminum heatsink [India]
42986. Removal of paint from 6061-T6 Aluminum Bike Frame [Arizona]
42987. Patination or darkening of aluminum leaf [UK]
42988. Need Brushed Nickel or Look-alike Spray Paint [California]
42989. What's the best material for 23% H2SO4 + 23% FeSO4, temperature 95C [India]
42990. Galvanized steel for diesel application [Malaysia]
42991. Conversion coating appearance [Korea]
42992. Need price on chrome plating my magnesium motorcycle rims [New York] {11/14/06}
42993. Seeking someone to refinish copper cooking pots [Connecticut] {11/14/06}
42994. Need Casket Handle and Bars [Nigeria] {11/14/06}
42995. Need anodizing of titanium [Malaysia] {11/14/06}
42996. Seeking Bright Dip for 24' Alum. Extrusions [California] {11/14/06}
42997. Need rhodium plating solution [Australia] {11/14/06}
42998. WANT TO BUY PLATING / STRIP LINE TANKS AND BARRELS [Florida] {11/14/06}
42999. Need Reciprocators/painting automation [India] {11/14/06}


The finishing.com Hotline has been on the Internet since '95 and includes more than 40,000 threads about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to: start at our home page, view the most recent letters, or search the site.


© finishing.com, inc., 1995-2007