The finishing.com Hotline has been on the Internet since '95 and includes more than 50,000 threads about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to start at our home page, view the most recent letters, or search the site.


26000. Alternative to acid cleaning of brass parts to avoid oil sticking on the part [India]
26001. Procedure for mirror finishing naval brass for 99.9% reflection [India]
26002. Applying gauge lines on a hypodermic needle [Mexico]
26003. Stainless steel tanks for fruit washing corroded by 50 ppm chlorine [Australia]
26004. Marine repairer needs chrome plater for brass-bronze parts [New Jersey] {12/01/03}
26006. Want license or consultant for Degreasing/Cleaning formulations [India] {12/01/03}
26008. Health risk of galvanized metal used under a wok used for cooking [Oregon]
26009. Does my vendor's COLD passivation process for 300 series stainless steel meet the specs? [Tennessee]
26010. Help, mirror finishing titanium in tumblers [Argentina]
26011. Need plastic parts of Harley V-rod chromed [Nebraska] {12/01/03}
26013. Seeking advice on repainting anodized window/door frames [Florida]
26014. Protection of brass/brown war plaque [New Zealand]
26015. How is pvdf coating done? [India]
26016. PCB trainee asks difference between black oxide process and natural oxidation of copper [Philippines]
26017. Cleaning of Aluminum without Degreasing [Israel]
26018. Suitable tube material for sea water condenser [Iran]
26019. Sensor installation needs austenitic steels that are 100% non-magnetic [New Zealand]
26020. Need titanium wire [India] {12/01/03}
26021. The process by which pennies get their copper coating [Canada]
26022. Automotive metal corrosion testing [Arizona]
26023. Sealant for copper to keep it from tarnishing [New Hampshire]
26024. Shop refinishing steel sleeves with TIN [Maryland]
26025. Seeking thin dense chrome [New York] {12/01/03}
26026. Seeking Dow Corning RTV compounds for mold making [India] {12/01/03}
26027. Need source for Magna-coat by Magnus Chem or equivalent [New York] {12/01/03}
26028. Seeking surface coating to protect chrome plating [Hong Kong]
26029. Tungsten carbide inserts get brown patches from cleaning [India]
26030. Need 33' aluminum trailer polished [Florida] {12/02/03}
26031. Need my plastic speedometer bezel rechromed [Iowa] {12/02/03}
26032. Changing appearance of brass to satin chrome without plating? [California]
26033. Need Gabe's article "Hard-Anodizing" [Connecticut]
26034. Extending the life of steel galvanizing kettle [India]
26035. Materials Engineering student investigating AC anodising [England]
26036. What does E-300 mean in the passivation process? [California]
26037. Thick (.001") nickel plating using a barrel plater or alternative [Canada]
26038. Seeking plating/spray finish for investment casting [UK] {12/02/03}
26039. Problem with high contact resistance with pure tin [Hong Kong]
26040. Is plating or blackodizing better on spring washers [India]
26041. Need brass plating on wood as chandelier repair [Virginia] {12/02/03}
26042. HOW TO TELL PAINT FROM POWDERCOAT [Tennessee]
26043. Musical instrument lacquers [Indiana] {12/02/03}
26044. Contractor needs Chemglaze Z306 [The Netherlands] {12/03/03}
26045. Use of SS 304 vs SS316 vs SS 316L in a phenolic environment [India]
26046. Knife sharpener mfgr. needs diamond composite plating [South Africa] {12/03/03}
26047. Passivating steel danglers [India]
26048. Alternate finish needed for blued spring clips [Illinois]
26049. Thin Electroless Nickel low stress films [Missouri]
26050. Nickel plating vs zinc on air/oil separators [Massachusetts]
26051. Our chrome plated mufflers have some spot or stain [Colombia]
26052. Electropolishing titanium for the medical industry [Ireland]
26053. Rust problem on cooling tower tubular fan shafts [California]
26054. Manufacturing process and related costs pertaining to 3"x3" Zinc T-Plate [Canada]
26055. Reducing sulfur content of nickel deposits [Canada]
26056. Effect of caustic gel on food grade stainless steel? [Canada]
26057. What is the difference between galvanize and metalize? [California]
26058. Need durable clear coat for steel sculpture details placed outside [Illinois]
26059. Need Delta-Seal SWF 11.129 [Poland] {12/03/03}
26060. Changing light blue anodized seat post to black [Michigan]
26061. Need brazing material /filler that can be electroplated [Indonesia]
26062. Powder peels from aluminum rims at bolt area [Malaysia]
26063. How to detect if Trivalent Chromate is on parts? [Tennessee]
26064. Need protection oil / pickling oil for outdoor storage [Pennsylvania] {12/04/03}
26065. Need gold plating of my charm [Florida] {12/04/03}
26066. Need clear alodine [Florida] {12/04/03}
26067. Chrome plating of fasteners for motorcycles [New York]
26068. Cleaning carpets of green copper corrosion drippings [Ohio]
26069. Browning versus bluing of firearms [Pennsylvania]
26070. Stripping silver and nickel from PCBs [Utah]
26071. Seeking firm to strip rubber from metal parts [Pennsylvania] {12/04/03}
26072. 100 hunting equipment components need red powder coating [California] {12/04/03}
26073. Need a used plasma unit (Metco MC7 or MC9) [Texas] {12/04/03}
26074. "Galvanizing" with zinc ozide and butternut squash [Arizona]
26075. Spent Treatment [India]
26076. Cyanide-free silver plating solutions [Scotland]
26077. Semicon mfgr. wants comparison of the various mold release coatings [Philippines]
26078. Motorparts supplier wants chrome spray for plastics [UK] {12/04/03}
26079. Magnetic Fields Prevent Car Crashes [Illinois]
26080. Reduction and Precipitating of Copper from its salt solutions without using electricity [UK]
26081. Can't repeat a nice black EN coating on silver [Turkey]
26082. Removing nickel carbonate from EN surface [California]
26083. Chrome Removal from Aluminum [Oklahoma]
26084. Effectiveness of passivation test kits? [California]
26085. Need consultant to redesign baking oven and recovery [India] {12/05/03}
26087. Firearm maker wants info on Nitriding/Carbo nitriding [Wisconsin]
26088. Heating Process [Colombia]
26089. How do I harden cold rolled steel? [Alabama]
26090. Painting soft "foil" like ductwork [Georgia]
26091. Aluminum oxide for paint [South Carolina]
26092. Galvanic corrosion prevention in medical equipment [Florida]
26093. Kitchenwares mfgr. finds 302SS tarnishes in dishwasher [New York]
26094. Copper post treatment [Louisiana]
26095. Plating Muscle Wire (titanium-nickel) [England]
26096. Help with bamboo floors with aluminum oxide urethane finish [Maryland]
26097. Automotive designer needs S-N curve for AlMg3 [Germany]
26098. Non stick coating on SS Tube ID [India]
26099. What powder coating thickness for aluminum workstations? [India]
26100. Need info on applying Nylon 12 E-Coatings [Georgia]
26101. Need to improve salt spray duration of zinc plating [India]
26102. Improving our citric acid passivation process [Turkey]
26103. Needed: High wear/no maintenance black finish for hand cuffs [Illinois] {12/08/03} 
26104. Electroplating rhodium using rhodium iii chloride hydrate, 99.999% [England]
26105. Need the details of electroless nickel plating steps [Hong Kong]
26107. Restoring a black & copper "japanned" antique finish [Texas]
26108. How do I repair the scratched powdercoating on my chopper's frame? [Arkansas]
26109. Fatigue strength and Hardness of EN 6060, T66 - F22 [Michigan]
26110. European directives vs. Tin Whiskers & Tin Pest [Oregon]
26111. Architect wants brushed aluminum finish on suspended ceiling [Texas]
26112. Need info about Bright Dipping [California]
26113. White streaks in anodizing due to uneven blasting? [Arizona]
26114. Seeking brass polishing and lacquering [Maine] {12/08/03}
26115. Need supplier of nickel anodes, 10 tons/year [Egypt] {12/08/03}
26116. The effects of changing from solid anodes to anode buttons/balls [Philippines]
26117. Space duty requires high conductivity plating for aluminum [California]
26118. Need coating to protect freshly blasted aluminum from future stains [So. Carolina]
26119. Modifying the appearance of a shiny chrome finish [Ohio]
26120. Is hexavalent chrome dangerous after plated on a part? [Ontario]
26121. Failure of railway compartment springs [India]
26122. Powder Coating for non-metal products [Jordan] {12/08/03}
26123. Need mag sleeve coatings and machine to apply them [Malaysia] {12/08/03}
26124. Need electroless Ni-B plating bath for silver [Australia] {12/08/03}
26125. Need Stalagnometers [Australia] {12/08/03}
26126. Activation of aluminum film surfaces on silicon [Texas]
26127. How can one preserve their chrome rims in Aruba? [New York]
26128. Does Electroless Ni require post treatment? [Israel]
26129. Economically getting chrome adhesion on Hastelloy & stainless [Australia]
26130. Pickling verification for internals of contactor tower [Nigeria]
26131. Need info on degreasing prior to plating [Lebanon]
26132. Hard Coating Process Information [India]
26133. Need for a Metascope / Steelscope [India] {12/08/03}
26134. Specific gravity of anodize solution and how to measure it [New Zealand]
26135. Busbar factory seeks installation of a silver plating facility [Thailand] {12/08/03}
26136. Alternatives to decorative chrome plating [Alabama]
26138. Need platinum black thin film deposited into metal sponge [North Carolina] {12/09/03}
26139. Need bumpers plated and other parts on 1955 Packard [Florida] {12/09/03}
26140. Architect needs 18' bar nickel plated [Connecticut] {12/09/03}
26141. Finishing shop is looking for test panels [California] {12/09/03}
26142. Need small hot dip galvanizing plant [India] {12/09/03}
26143. SURPLUS PAINT of aluminium extrusions - what to do [Indonesia]
26144. Theory and application of vci (paper and film) [India]
26145. Safety of the use of alum in water to be used for consumption [New York]
26146. Zhan cup vs EZ ZHan cup [Canada]
26147. Autophoretic coating tank needs excessive dumping [Australia]
26148. Tiny bore Nicasil application [Michigan]
26149. Yellowish stain on Sn-PB connector pin [Singapore]
26150. Aluminum sludge build up/removal from caustic tank [Texas]
26151. De-burring and polishing Inconel [Australia]
26152. Creating oxidation film on copper to retard erosion [Colorado]
26153. Need black anti corrosion finishing for steel screws [Israel]
26154. What is sermalube; is it a stock product? [New York] {12/10/03}
26155. Need small chrome line for motorcycle parts [North Carolina] {12/10/03}
26156. Need trivalent chrome or chrome free conversion coatings for aluminum [Canada]
26157. Hardcoat anodizing dust toxicity [Minnesota]
26158. Looking for Cosmetic Specification for Gold Alodine [California]
26159. Chrome plate my lineman's pliers for less then $50? [New York] {12/10/03}
26160. TV production firm has questions on Miller chlorination process for gold [Virginia]
26161. Work piece geometry that hinders CCC rinsing [Maryland]
26162. Please comment on our procedure for stripping of nickel-cadmium plate [Serbia]
26163. Need mil-spec CCC, epoxy primer, and polyurethane on 140 aluminum parts [Florida] {12/10/03}
26164. Choosing electro vs. mechanically deposited cad [Connecticut]
26165. Corrosion protection of 6061 AL, electroless nickel or anodizing? [California]
26166. Improving breakdown voltage for hard anodized cast aluminum [California]
26167. Comparison of electroplated vs. chemical grafted components [Canada]
26168. Deionized water cause aluminum oxide film contamination on parts [Indiana]
26169. Need used coil coating line aluminum Venetian blinds [India] {12/10/03}
26170. Want to buy copper sulphate [China] {12/10/03}
26171. Need My DOHC Valve Cover Chromed [Nevada] {12/12/03}
26172. Seeking Zinc Nickel Trivalent Chromate Plater [Illinois] {12/12/03}
26173. Need a Hanging Hull Cell [Massachusetts] {12/12/03}
26174. Why does copper turn green? [Iowa]
26175. Etchant to reveal nitriding of aluminum by plasma? [Brazil]
26176. Steel/Metal Desk Restoration Tips Needed [California]
26177. Disposal of "Universal Waste" from plating shops [Oklahoma]
26178. Treatment of cyanide with hypochlorite: cooling of the reactor [Spain]
26179. Want selective etch for Ni in Ni-Germanide [Belgium]
26180. Recoating pvc steel [Virginia]
26181. Pinholes in epoxy powder coating on grey castings [Tennessee]
26182. How to reduce concentration of sulphuric acid from 93% to 13% [Illinois]
26183. Can our aluminum fishing reels be titanium coated? [California]
26184. "Plasma Electroplating" is it a myth? [Hong Kong]
26185. Problems with silver cyanide bath [Massachusetts]
26186. Degreasing LM6 Aluminium in hot water [England]
26187. NaOH is attacking 316 Stainless Steel tank [North Carolina]
26188. Stainless Steel Abrasive Finish Standards [Washington]
26189. Dangerous Corrosion of Embedded Aluminum Posts in Hi-Rises [Florida]
26190. Is dry galvanic corrosion possible? [Washington]
26191. Chromate to nickel galvanic incompatibility? [Ohio]
26192. Galvanize flakes building up on rollform rollers [Delaware]
26193. Artist inquiry about gold-plating [Kansas]
26194. Need black oxide for large stainless steel panels -- treatment or or tanks [China] {12/12/03}
26195. Need Chrome Plating on Aluminum flasks - Ongoing [Illinois] {12/12/03}
26196. Etching solution for MgF2 on GaAS [Taiwan]
26197. "Galvanizing" steel with mercury vapor in an oven [Arizona]
26198. Bumper restoration: filling a gouge [Canada]
26199. Black anodize is flaking [Ohio]
26200. Conforming Anodes in Nickel Sulfamate? [Michigan]
26202. Powder coating peel off [Malaysia]
26203. Using fruits and vegetables to produce electricity [California]
26204. How to apply lacquer to polished brass? [Arizona]
26205. What does cadmium smell like? [Massachusetts]
26206. Same pretreat for powder coating steel or aluminum? [Wisconsin]
26207. Pretty finish close to cost and protection of anodizing AL380 [Arizona]
26208. Aluminum or Stainless for swim platform on Houseboat ? [California]
26209. Maintaining biocompatibility at nitinol to SS joint [Germany]
26210. Early yellowing of clear anodized architectural extrusions [Canada]
26211. EN won't adhere to Molybdenum [Czech Republic]
26212. Quality problem in zinc plating [India]
26213. Electroplating copper articles with either gold or silver [India]
26214. Chemically removing plasma cutting slag from mild steel [Montana]
26215. Need 1 Maplight Assembly Chromed [Indiana] {12/15/03}
26216. Need for hydrogen de-embrittlement [India]
26217. Shelf life of ZnSO4 and NiSO4 plating electrolytes [Louisiana]
26218. Black spots on zinc plated valves after repeated washing [Michigan]
26219. Need black chrome coated copper sheet [Michigan] {12/15/03}
26220. Looking for a silver plater [New York] {12/15/03}
26221. Want h.d. motorcycle plastic sidecovers electro-plated [Michigan] {12/15/03}
26222. Need fishing jigs chrome plated [North Carolina] {12/15/03}
26223. Need mil-spec chrome plating of 2024 aluminum [Texas] {12/15/03}
26224. Need electro deposition lacquer [India] {12/15/03}
26225. Need an electroplating additive made from dyestuff [China] {12/15/03}
26226. Polyester coating for dye sublimation [California] {12/15/03}
26227. Brightener and booster for alkaline zinc plating [UK]
26228. How to: Build a salt spray chamber, need plans and B.O.M. [Florida]
26229. What is H2SO4 [England]
26230. Scratches and stains in stainless steel cabinet doors [Florida]
26231. How to mount and build aluminum openings [Mauritius]
26232. Recipe to electro polish stainless at home [New York]
26233. E-coat is bleeding [Michigan]
26234. Zinc Alloy Plating chipping over carbon nitrided steel [Ohio]
26235. Pink, Crazed, Cadmium Plating [Illinois]
26236. Rusting in Zinc plating parts [India]
26237. Chem film color vs. electrical resistance [New Zealand]
26238. Sodium Hydroxide for parts cleaning? [Michigan]
26239. Ideas for non-conductive coating on locating pins for spot welding [Michigan]
26240. Need fabrication of chrome hand grips [New Jersey] {12/15/03}
26241. Want to open a shop chroming plastic and aluminum [Indonesia]
26242. Refinishing wrought iron furniture [Texas]
26243. Re-anodizing or oxidizing silver jewelry [Illinois]
26244. How to do Brushed Steel look [Vermont]
26245. Recoloring alloy ski poles as a hobby? [Illinois]
26246. Problems in Passivated Zinc deposit [India]
26247. Yellow Passivation color change [India]
26248. Requirements for type III anodizing with a type II setup [Tennessee]
26249. Translucent dark grey anodizing on 6061 heavy plate [New York]
26250. Burrs causing undersize holes [Texas]
26251. Polishing of Zirconium Metal [Pakistan]
26252. Need preanodized aluminum sheet [New Jersey] {12/16/03}
26253. Chrome plating steel drum musical instruments [Maryland] {12/16/03}
26254. Seeking anodized aluminum for floodlight reflectors [Iran] {12/16/03}
26255. Seeking Nedox HTR alternatives [Michigan] {12/16/03}
26256. Help finding Christmas gift [Florida] {12/16/03}
26257. General query on powder coating [England]
26258. Must stones be removed to rhodium plate? [Connecticut]
26259. Need coating for snowmobile exhaust [Michigan]
26260. Type of silverplate and refinishing possibilities [Florida]
26261. Improving my rust blueing of guns [England]
26262. Selective Tin-Lead Plate over ENIG [Utah]
26263. How to achieve deep black on 356 castings? [Connecticut]
26264. Surface tratment for stenter chain elements [India]
26265. Best post-treat for galvanneal [Michigan]
26266. Need handles, etc. rechromed on '68 Firebird [Arkansas] {12/16/03}
26267. Need plater, polisher, caster in S.E. to produce my accessory line [So. Carolina] {12/16/03}
26268. Need high current contact saddles for our anodizing line in China. URGENT! [North America] {12/16/03}
26269. Etching of al 5083 [India]
26270. Selective brush plating of billet aluminum [North Carolina]
26271. Salt Spray specs. ASTM vs. JIS [Brazil]
26272. Using mechanical plating process for plating sheets? [Iran]
26273. Pre Care of metal components used in high vacuum tubes [India]
26274. Is bromine better than chlorine in nickel sulphamate baths? [India]
26275. Can platinized titanium anodes be used in hard chrome plating [India]
26276. Compatibility of rubber lined mild steel tank with 98% sulphuric acid [India]
26277. Gold plating of jewelry--2800 medals [California] {12/17/03}
26279. Zinc Plating Roll Formed Shapes [Pennsylvania] {12/17/03}
26280. Need anodising kits, small amounts of dyes [Australia] {12/17/03}
26281. Looking for very small quantity of copper sealer [California] {12/17/03}
26282. Need used salt spray cabinet [Illinois] {12/17/03}
26283. Need a way to clean saddles from catwalk [Kentucky]
26284. Powder Coat over anodized aluminum [Colombia]
26285. Chromatization on zinc diecast parts [India]
26286. Chromating Problem [Thailand]
26287. Bright Brushed Anodized Sheet .063" [Georgia] {12/17/03}
26288. Need small Copper Etching line [Massachusetts] {12/17/03}
26289. Need "adhesion layer" for Gold on Aluminum [New York]
26290. Cadmium growth - whiskers, crazing, or just corrosion [Florida]
26291. Plating aluminum electrical contacts [New York]
26292. How is it possible to re-hard coat anodize without stripping? [Washington]
26293. Anodized aluminum is turning yellow [Canada]
26294. Measuring rust, chemical formula for rust [Wisconsin]
26295. Removing rust stains on anodized aluminum [Hong Kong]
26296. 1995 ZX-6R Frame Polish info needed [Louisiana]
26297. Increase whiteness of rhodium plating / Need a rectifier [Pakistan]
26298. Bubbles after black chromium [Portugal]
26299. Will the installation of dielectric unions stop electrolysis in this situation? [Texas]
26300. Need 6000 closet-pole flanges stripped and powder coated [New York] {12/18/03}
26301. Need Silver Plating of Pyrex Tube [New Jersey] {12/18/03}
26302. Clear coating aluminum wheels [Louisiana]
26303. Possible corrosion of metal in damp state [Illinois]
26304. Yellow gold jewelry has turned maroon [North Carolina]
26305. Salt spray testing of 4140 and acceleration factor [Florida]
26306. Reclaiming silver from our vacuum capacitors [Ohio]
26307. Can nickel/nickel chrome replace electro zinc plating? [Alabama]
26308. Cured application of alodine 1200 passivate new coat of 1000 [Washington]
26309. MIL-C-5541 class 1A vsd class 3 [New Hampshire]
26310. Cor-Ten Roofing / Halting Rust Process [Colorado]
26311. Gold inorganic pigment for silk screening [Yugoslavia] {12/18/03}
26312. Need a UV Glue Chemiseal U-1546B [China] {12/18/03}
26313. HOW DO I MIRROR FINISH STAINLESS STEEL [Louisiana]
26314. Carburetor [Texas]
26315. How can I obtain a copy of mil-a-8625f? [Hong Kong]
26316. ADHESIVE FOR TEFLON [India]
26317. AMS 2488 [Denmark]
26318. Surface prep. for 446 S.S. prior to platinum plating [North Carolina]
26319. Challenges with Passivation 303S [Texas]
26320. SS 316 PIPES and H2SO4 [Saudi Arabia]
26321. Need "Super seal finish" / Tor Cad [Ohio] {12/19/03}
26322. Need NH35 corrosion coating on magnesium [Colorado] {12/19/03}
26323. Robotic grinding, buffing, and polishing equipment suppliers [Wisconsin] {12/19/03}
26324. Gold plating from start to finish [Indiana]
26325. Portable chrome-free chroming? [Hawaii]
26326. DI or Distilled Water Re: detoxification of my body? [Wisconsin]
26327. MD asks skin toxicity of ammonium bifluoride [Massachusetts]
26328. Heat Resistant finish for gas lanterns [Texas]
26329. Need Tech Know-how for manufacture of OPC Drums [India] {12/19/03}
26330. Need power supply for anodizing in home workshop [Arizona] {12/19/03}
26331. Interesting questions [Turkey]
26332. Need Metal Finishing Guidebook [Louisiana]
26333. Antique Finish on Brass Zip Fasteners [India]
26334. Did we "over-passivate" our tubing? [Malaysia]
26335. Effects of chlorine dioxide on 316 stainless steel [England]
26336. Passivation of fasteners [India]
26337. Picratic Acids In General [Oklahoma]
26338. Artist endeavors to turn 304SS a mottled blue [Alabama]
26339. Plateable filler metal for steel [New Jersey]
26340. What is ANSI #7 for stainless steel [Minnesota]
26341. Fading Method of Metal Colorizing in Gold Plating [Indonesia]
26342. Black Chrome my Cycle Wheels [Minnesota] {12/22/03}
26343. Need Gold refining equipment [Columbia] {12/22/03}
26344. I need motorcycle parts chromed [Massachusetts] {12/23/03}
26345. Re-anodizing and Re-chroming fishing reel parts [Canada] {12/23/03}
26346. Seeking black oxide finish on putter heads [California] {12/23/03}
26348. PROTECTIVE LACQUER/MASKING LIQUID FOR USE DURING ANODIZING [India] {12/23/03}
26349. Electroplating copper onto titanium [Spain]
26350. Chrome-like finish on the back side of clear plastic [North Carolina]
26351. Hardness of different gold alloys [New Jersey]
26352. Pitting on brass since we moved [Canada]
26353. Gold cleaning [Canada]
26354. Stripping gold to restore silver dollar [Ohio]
26355. Question about the durability of artificially induced patina on brass [New York]
26356. ACID PORTING HEADS AND INTAKE MANIFOLDS [Minnesota]
26357. Artificially Aging Brass [Texas]
26358. Vapor hone or sand blasting (is there a difference?) [Minnesota]
26359. Chlorine contact/contamination of aluminium water tanks [UK]
26360. What is the exact process of anodizing aluminum? [Missouri]
26361. Polishing cast aluminum covers to look like chrome [Texas]
26362. ABS Nickel-Chrome plating [California]
26363. NEED CHOCOLATE BROWN FINISH ON COPPER BATH ACCESSORIES [South Africa]
26364. Black Patch problem on DOM tube surface [India]
26365. Improving zinc phosphate formulation [Mexico]
26366. PASSIVATION OF 201 WIRE RODS [India]
26367. Chroming a copper radio chassis [New Jersey] {12/24/03}
26368. Credit-card equipment refurbisher need finishing of plastic machine cases [Florida] {12/24/03}
26369. Cyanide-free silver plating process for Martensitic Steel [Scotland] {12/24/03}
26370. Artist seeks silver gel [Montana]
26371. World-wide equivalent to 380 die cast aluminum [Wisconsin]
26372. Tacky anodized parts [Connecticut]
26373. Prevent Stainless Steel Tarnish During Vulcanization [Kansas]
26374. Dielectric coating for assembly [Ohio]
26375. Need 18-megohm D.I. water system [Philippines] {12/24/03}
26376. Looking for technical know-how to coat selenium copier drums [Singapore] {12/24/03}
26377. How to clean spots off brass lantern lights [North Carolina]
26378. Paint textured appliance surface [California]
26379. GM spec. WPPGLA on Powder Coat [Michigan]
26380. Etch acid for Inconel 718 and 903 [Kansas]
26381. How to obtain light blue colour with alkali zinc plating [Turkey]
26382. Aluminum oxide [Australia]
26383. Need gold testing machines [India] {12/24/03}
26384. Electrical conductivity of plating materials [Vermont]
26385. Need one wheel rechromed [Alabama] {12/24/03}
26386. Need Plastisoling equipment and materials [Canada] {12/24/03}
26387. Need high quality stems for discharge lamps, tubes [India] {12/24/03}
26388. Roofer needs Teflon coating on aluminum as release [West Virginia]
26389. Theatre group Desire a Streetcar to be rusty [Arizona]
26390. Hydrogen Embrittlement in HSLA Steels [Michigan]
26391. Best activation for EN plating of a complex shape 400 SS part [Mexico]
26392. Problems bonding to anodized aluminum [South Africa]
26393. Will Copper-Aluminum corrosion occur in heat exchanger [Belgium]
26394. Redipping facemasks for football helmets [Oklahoma] {12/29/03}
26395. Antique auto needs media blasting [Florida] {12/29/03}
26396. Seeking acid dipping [New Jersey] {12/29/03}
26397. Refinishing antique Coke machines [Michigan] {12/29/03}
26398. Seeking refinishing of vintage cast iron tubs [Texas] {12/29/03}
26399. Seeking Chrome Plating of Black Plastic Honda CRV/Pilot Grills [Massachusetts] {12/29/03}
26400. SEEKING ENDURION COATING [Massachusetts] {12/29/03}
26401. Equipment for nickel silicon plating [India] {12/29/03}
26402. Need holographic hot stamping foil [Pakistan] {12/29/03}
26403. Need hand-held coating thickness gauge [India] {12/29/03}
26404. Cable factory needs copper cathode sheet [Malaysia] {12/29/03}
26405. Want gold refined from materials on hand [Tennessee] {12/29/03}
26406. Need an automated passivation and ultrasonic cleaning system [Ohio] {12/29/03}
26407. Rust prevention for 10-year-old's project [Michigan]
26408. Dissolving coins so salts can be analyzed [India]
26409. To rust and trust [Texas]
26410. Improving corrosion resistance of nitrocarburized metals [Iran]
26411. Electrodeposition of Pt as a fuel-cell catalyst [Michigan]
26412. Electropolishing of coronary stent [India]
26413. Getting large rust off '57 Willeys [Washington]
26414. Need to restore shine to weathered brass door hardware [Texas]
26415. Chrome paint [Canada]
26416. Cleaning paint from galvanized metal [Arkansas]
26417. True gold anodizing spray paint? [Colorado]
26418. New European Council recommendations for chromate coating [Taiwan]
26419. Anodize standard [India]
26420. Hanger marks [India]
26421. What paint stripper for epoxy? [India]
26422. Adhesive for bonding ultem2300 before plating [California]
26423. Black rings from stamper [India]
26424. What is the proper cutoff for 3.2 Ra finish? [Ohio]
26425. Reducing wear, tear and friction on yarn spinning traveller [India]
26426. Improve quality of a Hologram Master [India]
26427. Need my GTO bumper replated [Maryland] {12/30/03}
26428. Need plating for antique Fiat restoration [California] {12/30/03}
26429. Salt Spray Chamber per ASTM B 117 [India] {12/30/03}
26430. Chemistry question [Canada]
26431. Paint removal from antique pipes of church organ [New York]
26432. Refinishing of wood cook stove [North Carolina]
26433. Cracking problem of Ni-Cr plating on plastic auto parts after Thermal cycle test [India]
26434. Sealing a space between two attached disks for plating [California]
26435. Seeking shop to refinish firearms via Norrell's process [South Carolina] {12/30/03}
26436. Need a solution for masking-finishing emblems [Iowa] {12/30/03}
26437. Seeking silicone pull plug [India] {12/30/03}
26438. Electroplating theory [Oklahoma]
26439. Coloring stainless steel [North Carolina]
26440. How to keep copper roof non tarnishing [New York]
26441. Copper countertops [Ohio]
26442. Our galvanized parts are dull [India]
26443. Options for zinc-plating steel [New Hampshire]
26444. Pre Treatment [India]
26445. Restoration and rechroming of wire shower caddy [Pennsylvania] {12/30/03}
26446. Chrome plating of motorcycle parts [California] {12/30/03}
26447. Silverware oxidation has been lost [Tennessee]
26448. Post Treatment [India]
26449. Long or Short Profile Anodizing? [New York]
26450. Aluminum finishing and bushing material [California]
26451. Polishing stainless steel muffler end caps [New Zealand]
26452. Non-Destructive Testing of Nickel Thickness [Arkansas]
26453. Recycling of chrome plating sludge [South Africa]
26454. COMPATIBILITY OF CERAMIC COATING FOR TRI-N-BUTYL PHOSPHATE [India]
26455. Proper analytical method for free fluoride in acidic solution [India]
26456. Zinc sheet structure [Vietnam]
26457. Need powder coating powder [Russia] {12/31/03}
26458. What chemical is used to make zinc plate black [Vietnam]
26459. Need Module-V for Thermax powder coating equipment [India] {12/31/03}
26460. Exhaust fan [Texas] {12/31/03}
26461. Galvanized Plater for Fasteners [Tennessee] {12/31/03}
26462. Looking for a lead, tin, copper plater [Wisconsin] {12/31/03}
26463. Rechrome my 1962 Olds parts [Tennessee] {12/31/03}
26464. Electoplating brush plating kit wanted [Pennsylvania] {12/31/03}
26465. Need chroming of my Accura wheels [Virginia] {12/31/03}
26466. Softness of platinum vs yellow and white gold [California]
26467. Reducing Total Dissolved Solids in Rinse Water [Iowa]
26468. Acidic Atmosphere in Our Anodizing Department [Idaho]
26469. ZINC OR COPPER FILTER CAKES [Georgia]
26470. Searching for method to measure anodized layer thickness [Singapore]
26471. Corrosion Improvement Properties of Anodized Aluminum [Michigan]
26472. Punch And Die Surface Finishing [Singapore]
26473. Seeking baby shoe finishing suppliers [West Virginia] {12/31/03}
26474. What is new in thermo reactive deposition method [Iran]
26475. Chalky white residue left from dripping taps [Australia]
26476. Need vinyl dipping of spring steel [Florida] {12/31/03}
26477. Need tin electroplating of copper plates for marine use [California] {12/31/03}
26478. Urgent need for anodized aluminium sheet for floodlights [Iran] {12/31/03}
26479. Need microetchant procedure [Turkey]
26480. Special coloured anodized finish on aluminum extrusion [Turkey]
26481. Custom guitar builder looking for someone to plate parts [Florida] {12/31/03}
26482. Need refinishing of Stiffel lamp [New York] {12/31/03}
26483. Etching nickel [North Carolina]
26484. Inventor needs nickel plating on tungsten wire [New York] {1/02/04}
26485. Want to Purchase Nickel Anodes [U.A.E.] {1/02/04}
26486. How to treat rash caused by nickel or stainless steel jewelry? [California]
26487. Electrowinning Problems [Arizona]
26488. Need high speed lead-free Electroless Nickel [Korea] {1/05/04}
26489. Need specialized adhesive tapes [India] {1/05/04}
26490. Effect of coating on fatigue life of components [Pakistan]
26491. Solidification/stabilization technology for heavy metal laden waste [India]
26492. Need to know the "skin pass standard" [Vietnam]
26493. Help identify metal poisoning [Montana]
26494. Amount of Sulfur Dioxide Generated by Sodium Metabisulfite in Acidic Solutions [Georgia]
26495. Formula for preparing NC Thinner and Auto Thinner [Sri Lanka]
26496. Repairing 12L14 pitted by stripping [Minnesota]
26497. Descaling of Cobalt-Chromium Alloy (L-605) [India]
26498. Non-conductive coating for Class III Be-Cu [Ohio]
26499. Need dents fixed, then rims chrome plated [Texas] {1/05/04}
26500. FACILITY FOR PIN AND Cr N PVD COATING [India] {1/05/03}
26501. Artist needs copper and gold electroplated leaves [Oregon] {1/05/04}
26502. Need chrome plating of my '54 Chevy parts [Maryland] {1/05/04}
26503. Re-finish my range backsplash [Washington] {1/05/04}
26504. Wholesaler needs electroplating of seashells [Texas] {1/05/03}
26505. Seeking colloidal tin or aluminum [Pennsylvania] {1/05/04}
26506. Acid and Can Reactions [Maryland]
26507. Want table to rust quickly [Massachusetts]
26508. Preparation of Phenyle and Acids [India]
26509. Aluminum Truck Body Cleaner [New Jersey]
26510. Gasoline and Ospho [North Carolina]
26512. Skin discoloration [Kansas]
26513. Polishing brass buckle [Arizona]
26514. Preventing chrome from rusting [UK]
26515. Brush finishing stainless steel [Arizona]
26516. Need pointers on coating polished brass or copper [Pennsylvania]
26517. Plate finish for copper sheet [Pennsylvania]
26518. Problem using ti applicator for high lead solder [Singapore]
26519. Tomato canner wants printing on filled cans [California]
26520. Mechanical Galvanized Coating Thickness [Canada]
26521. I need some color on stainless [Washington]
26522. Coating an aluminum airboat hull [Finland]
26523. Need brass bed cleaned and sealed [Florida] {1/05/04}
26524. Does Platinum metal have memory? [California]
26525. Copper Head Golf Clubs [Oregon]
26526. Help making stainless steel magnetic [Florida]
26527. Patchy electroplating of palladium onto nickel [Texas]
26528. Looking to have my car rims and other items black chromed [Minnesota] {1/06/04}
26529. Need my Mopar bumpers and plastic parts chromed [Ohio] {1/06/04}
26530. My wheels needs to be re-chromed [Florida] {1/06/04}
26531. Non-profit org needs sublimation coating materials [India] {1/06/04}
26532. Electropolishing of the interior of 316 stainless steel tanks [China] {1/06/04}
26533. Help dad help son with copper plating project [Texas]
26534. HOW TO MAKE POROSITY IN ALUMINA [India]
26535. Nubbing or white spot formation [South Africa]
26536. Solar selective coatings in the lab [Pakistan]
26537. Replating silver at home [New York]
26538. Teflon removal [Florida]
26539. Residential contractor wants copper cleaning/clearcoating products [Mississippi] {1/06/04}
26540. Need a passel of reflective glass beads [China] {1/06/04}
26542. Lacquer coating on alum foil [U.A.E.] {1/06/04}
26543. Need electrostatic guns and control panel [Saudi Arabia] {1/06/04}
26544. Is Dry Phosphate Treatment available in the USA [Indiana] {1/06/04}
26546. Stripping chrome plating from thin aluminum [California]
26547. M-nitrobenzene sulphonic acid sodium salt [China]
26548. Stripping Gold Braze [Texas]
26549. Fishing reel mfgr having problems bonding Teflon to anodized aluminum [South Africa]
26550. Tell me something about flux solution [Vietnam]
26551. HOW TO REDUCE TRI CHROME CONTENT [Pakistan]
26553. Bumper rechroming [Illinois] {1/07/04}
26554. Need '72 Chevy truck grill plated [Indiana] {1/07/04}
26555. PROCESSING SMALL ORE FINDS [Illinois]
26556. Nickel plating Science Project Help [Tennessee]
26557. RMS conversion to anchor profile depth [Texas]
26558. Need my '72 Skylark bumper chromed [New York] {1/07/04}
26559. Need brushed aluminum or service to brush aluminum [Minnesota] {1/07/04}
26560. Ni-Plating for small gas cylinder (one-hole) [Pennsylvania] {1/07/04}
26561. Need Nickel Anodes for Plating [Iran] {1/07/04}
26562. Acidity of iron rusting [Colorado]
26563. Effect of crystal orientation on polishing and grinding [China]
26564. Obtaining flame colors on copper [Colorado]
26565. Need pictures of different metal finishes [Hong Kong]
26566. HASTALLOY STRAINER BASKET FOR USE IN HYDROCHLORIC ACID [Michigan]
26567. Actual years reflect a 48, 96 or 192 Hr of Salt Spray Test [Israel]
26568. Need Silver etchant that does not attack Copper [Singapore]
26569. Titanium rack coating [Taiwan]
26570. Electroplating on PPSU [India]
26571. Inconsistent Copper Hardness [Pakistan]
26572. Tumble polishing stainless steel [Canada]
26573. Need bumpers chrome plated [Illinois] {1/07/04}
26574. Need glass crusher to make abrasives from windshields [Canada] {1/07/04}
26575. Thermal conductivity of oxide layer [Germany]
26576. Powder coating over Tin and Silver plated Buss bars [Illinois]
26578. Cost of aluminide coatings [Iran] {1/08/04}
26579. Portable crankshaft polisher needed in Italy [Connecticut] {1/08/04}
26580. Seeking Polyethylene Powder [Bangladesh] {1/08/04}
26581. Electroplating a key for science project [Colorado]
26583. Which BEVERAGE cleans pennies best? [Maine]
26584. Pd-Ag electropolishing for OIM studies [Canada]
26585. Electroplating for alternative, non-silver photography [Wyoming]
26586. Chemical Polish of Jewelry with Thiourea [Colombia]
26587. Removing scratches in stainless steel elevator walls [California]
26588. Rechroming items at home [England]
26589. Boric Acid Titration problems [Pennsylvania]
26590. Removing hard chromium [Turkey]
26591. Quantify increased hardness of adding hard chrome [Ohio]
26592. Nickel plating appearance specification [Iowa]
26593. Reinforcement of a Hard Chrome Solution [Pakistan]
26594. Problem with nickel bath [Canada]
26595. Sulphuric aniodized turning yellow [India]
26596. DI water seal temps [California]
26597. Is anodizing FDA or USDA approved? [Texas]
26598. Galvanic Action of D-I Water and Stainless Steel [New Hampshire]
26599. Rust on 304 ss bits and riding equipment [India]
26600. Need zinc chromate on steel plate 48 x 56 x 1 [Alabama] {1/08/04}
26601. 6061 Aluminum Coatings and Material Compatability [Canada]
26602. CHROMING EQUIPMENT [South Africa] {1/08/04}
26603. New Epoxy Powder Coating System [Saudi Arabia] {1/08/04}
26604. Polishing and buffing [Pakistan]
26605. Looking for Manganese Phosphate supplier [Canada] {1/9/04}
26606. Seeking Copper Coating for threads [Canada] {1/9/04}
26607. Chrome dipping of 4 rims [Tennessee] {1/09/04}
26608. Need my swingarm plated [Indiana] {1/09/04}
26609. Need Porcelain Powdercoating service [Missouri] {1/9/04}
26610. Trivalent aluminum chromating [India] {1/09/04}
26612. Everslik 1301 High Performance Coating [Nigeria] {1/09/04}
26613. Extraction of silver from silver nitrate solution [England]
26614. Pollution of Marikina River [Philippines]
26615. What is the difference between hot press, cold press, and galvanized sheet metal [Colorado]
26616. Making a mirror [Malaysia]
26617. NEED HELP WITH REBLUEING PREPARATION [Florida]
26618. Rhodium/re-rhodium plating a white gold ring with engraved detail [Rhode Island]
26619. Temperature at which steel is hardened [South Carolina]
26620. Cooling tower run off at old Navy site, soon to be a school [California]
26621. Zn plate quality in blind threads [Israel]
26622. White rust formation on plated surface [India]
26623. Acid copper is blistering [Wisconsin]
26625. Difference between a 2B and 2F finish? [Tennessee]
26626. Does deionised water prevent galvanic corrosion? [Singapore]
26627. Need Zinc Nickel Plating on springs [Ohio] {1/9/04}
26628. Chrome Plating Shop Needed [Florida] {1/09/04}
26629. MFZn2-C [Ohio]
26630. British and American equivalent raw materials and specifications [Illinois]
26631. Why pot metal blistering? [Illinois]
26632. Black nickel plate parts made of titanium [Massachusetts] {1/9/04}
26633. Chrome my alloy wheels [Pennsylvania] {1/09/04}
26634. Need bike part rechromed [New York] {1/09/04}
26635. Need sailboat chains re-galvanized [Florida] {1/09/04}
26636. Chroming steel legs [New York] {1/9/04}
26637. SILVER RECOVERY EQUIPMENT [Bahrain] {1/09/04}
26638. Manufacturing red lead and zinc oxide [Egypt] {1/09/04}
26639. Reqd Technical Collaborator for Nikasil / Nickel silicon carbide coating [India] {1/09/04}
26640. Yellow chromate conversion coating [Vietnam] {1/09/04}
26641. Need used Truck Paint Booth fast! [Pennsylvania] {1/09/04}
26642. Why did powdered aluminum become an adhesive? [Canada]
26643. Scaling of heating coil [India]
26644. Removing paint from bumpers [Canada]
26645. Water marks/stain marks on turned aluminum components [India]
26646. Substituting silver for immersion gold on PWBs [Malaysia]
26647. Need Assistance to learn electroplating [Mexico]
26648. RA surface finish compared to lap surface finish [South Carolina]
26649. Need car e-coated [Texas] {1/12/04}
26651. Cathodic protection [Indonesia]
26652. Titanium vs. platinum wedding bands [Ohio]
26653. White Gold turning yellow [Florida]
26654. Polishing chrome bumpers [Pennsylvania]
26655. Soldering Zinc Die Cast Housing [Florida]
26656. Need exhaust pipe nickel plated for dirt bike [Florida] {1/12/04}
26657. Etchants for W and NiSi [North Carolina]
26658. Need help smoothing porous brass so I can shine it [Ohio]
26659. Wholesaler needs gold plated records and cds [Georgia] {1/12/04}
26660. Automotive brightwork goes dull when anodized [Canada]
26661. Aluminum Polished Skin Process Specifications [The Netherlands]
26662. TiB2 coating on graphite [India]
26663. Rusting of Electroless Nickel plated parts [India]
26664. Need powder paint line [Arizona] {1/12/04}
26665. Where does auto dealer go to get powder coating done [BC, Canada] {1/12/04}
26666. Need Consumables for Buffing and Painting [India] {1/12/04}
26667. We need more answers [Mississippi]
26668. Need potassium cyanide for pest control [California] {1/12/04}
26669. Repairing anodized Al chassis of Lotus Elise [Oregon]
26670. Student needing help with plating copper onto quarters [Washington]
26671. Where can you find the rusting metals I need? [California]
26672. Trouble hiding fasteners under powder coating [California]
26673. MATTE BLACKENING STEEL AND STAINLESS FASTENERS [Maryland] {1/12/04}
26674. Aluminum Hydroxide corrosion with anodized Al356 [Michigan]
26675. Low cure zinc rich coatings [Ohio]
26676. Very large item to be chromed [North Carolina] {1/12/04}
26677. Nickel plating [Texas]
26678. Need help about hard chrome [Bolivia]
26679. PAINTING TRUCK FRAME [Canada]
26680. Effect of coating on fatigue life of components [Pakistan]
26681. Seeking technical know-how for paint manufacture [Washington, DC]
26682. Looking for process for coating brush bar [California]
26683. Remove Monogram on Dirilyte [Indiana] {1/13/04}
26684. Which cleaning products contain phosphoric acid [Pennsylvania]
26685. Rust replacing metal [Wisconsin]
26686. Ion selective electrode for fluoride [Colorado]
26687. Electrostatic organic coating on glassware substrates [Turkey]
26688. Ivadizing on aluminum fasteners [India] {1/13/04}
26689. GOLD REFINING MACHINERY [India] {1/13/04}
26690. Electroless copper plating research areas [India]
26691. No adhesion of top coat to etch primered aluminum [India]
26692. Filtration system for satin nickel plating [India]
26693. Premature failure of Tri Nickel Coating on Welded joints [India]
26694. Red Cast on Manganese Phosphate Components [New York]
26695. Zinc and Yellow Chromate Protective Finish [Vermont] {1/13/04}
26696. Need powder coating with Mil-approved resistance to chem warfare agents [England] {1/13/04}
26697. Seeking antiquating copper chemical [Nevada] {1/13/04}
26698. Reworking powder coating [Mexico]
26699. Powder coating thickness [Indiana]
26700. Max. chromating temperature? [The Netherlands]
26701. What if Alodine surface is left unpainted? [Florida]
26702. Chrome plating a cast-plastic sculpture [Canada] {1/13/04}
26703. Titanium Nitride all chrome on H-D Road King [Connecticut] {1/13/04}
26704. Need production plating of bumpers [Illinois] {1/13/04}
26705. How does the electroplating occur [Canada]
26707. Galvanized water mains [UK]
26708. Developer needs to paint anodized aluminum storefront [Illinois]
26709. Alodine or anodize my designer sunglasses [Texas]
26710. Removing oxidation/corrosion from any metal in general [Tennessee]
26711. Dull spotted finish [Ohio]
26712. Powder coat my exhaust system [Texas] {1/14/04}
26713. Details about Hydrogen De-embrittlement [India]
26714. Yellow stains on post-heat treat stainless steel parts [California]
26715. Silver Flaking [Ohio]
26716. Seeking RECYCLING of USED PICKLE OIL [Michigan]
26717. Emission calculation from gold refinery reactions [UAE]
26718. Anodizing fading in color [Illinois]
26719. Restoring Mauviel skillet from very bad abuse [Virginia]
26720. Restoring Antique Wrought Iron Bed [California]
26721. Nitriding of Steel [Malaysia]
26722. Super Finishing By Honing [India]
26724. French standards for steel finish [Israel]
26725. Remove Sn from lead frame (Ni) [Malaysia]
26726. Ag from Cu plating [Malaysia]
26727. Alkaline heavy rust remover [Tennessee]
26728. GALVANOX [New York] {1/14/04}
26729. Restoring museum doors [Washington]
26730. John Deere green high heat paint [Missouri] {1/14/04}
26732. Occupational safety and health issues during stainless steel passivation of MS bolts [India]
26733. Need galvanizing wipe pads and to measure pickling acid concentration [Pakistan] {1/14/04}
26734. How do you paint brass? [Kansas]
26735. Pitting on cast aluminum after electroless nickel [Arizona]
26736. Aluminum Pretreatment for Powdercoating [Michigan]
26737. Looking for BLACK T specs [Israel] {1/14/04}
26738. Silver Plating bright bath help [Uruguay]
26739. Making a Refrigerator Colorful [Massachusetts]
26740. Coating glass capillary tubes with Ag [Nebraska]
26741. Rust on iron [Wisconsin]
26742. Units of Ductility [UK]
26743. Help with the cleaning of my sword [Texas]
26744. Cast and forged aluminum, how to chemically strip and refinish? [Texas]
26745. F-401 DS Type II [California]
26746. Chrome Burning [Wisconsin]
26747. Cleaning and finishing procedures for bone screws [Venezuela]
26748. DETAIL ABOUT PULSE RECTIFIER AND ITS APPLICATIONS [India] {1/15/04}
26749. Artist wants to do gold electroforming [Sri Lanka] {1/15/04}
26750. Need: Chrome FX, Cosmichrome, or FantaChrome system [Texas] {1/15/04}
26751. Galvanneal steel vs. aluminum buses [Louisiana]
26752. Looking for a product that will reliably stain aluminum [Georgia]
26753. How to paint polished aluminum bumper inserts for my car? [Nebraska]
26754. Metal Golf Head Refinishing Techniques and Equipment [California]
26755. Nickel color stability: yellowing [California]
26756. Dark metallic nickel-free plating for costume jewelry [Canada]
26757. Cleaning without de-anodizing [Philippines]
26758. Which coating to use on motor shafts? [India]
26759. Vinyl coated steel doors [Georgia] {1/15/04}
26760. Electrically conductive plating on plastic conduit connectors [Ohio] {1/15/04}
26761. Seeking glass beads for paint [Pennsylvania] {1/15/04}
26763. Titanium shell with micro structures [Wisconsin]
26764. Artist inquiry about the use of body fillers on aluminum [New York]
26765. Dichromate substitute [Michigan]
26766. Potential hazard of cleaning phosphatized wire [Pennsylvania]
26767. Analysis for Ferric Sulphate [Scotland]
26768. Paint peel off from cast iron object [Pakistan]
26769. Paint peel off on gp sheets [India]
26770. Thread standards for parts to be zinc plated [Wisconsin]
26771. Alodine 1132 compatibility with RP-1 Fuel [Colorado]
26772. What does 'mill finish' of aluminum mean? [Canada]
26773. Problem in sand blasting prosthesis [Turkey]
26774. Need replacements for canceled 'Bright dip' and 'Chromate' chemicals [UK] {1/16/04}
26775. Looking for a UK PVD coating equipment manufacturer [UK] {1/16/04}
26776. The right settings to electropolish aluminum alloy and stainless steel [Malaysia]
26777. Painting over chrome [Georgia]
26778. Mineral spirits vs NC thinner [UAE]
26779. Stainless steel jewelry questions [California]
26780. STEEL PROPERTIES [France]
26781. Poor adhesion of Electroless Ni with PTFE coating onto MIM parts [Kentucky]
26782. Corrosion resistant coating for magnesium [Germany]
26783. Cathodes for Chromic Anodize [Connecticut]
26784. Alodine 1500 Versus MIL-C-5541 [France]
26785. "Score" marks on electropolished 316 [Spain]
26787. Seeking Source for Powder Coating [Mississippi] {1/16/04}
26788. Teflon coating losing adhesion under a dry steam environment [Illinois] {1/16/04}
26789. Color Codes--How to determine what they are specifying [Arizona]
26790. Muriatic acid stains on stainless steel [Florida]
26791. How-tos of dechroming [Oklahoma]
26792. Rusting problem [India]
26793. Galvanic corrosion of weld near Au plated area [California]
26794. Need process (and filter?) for Satin Nickel plating [India] {1/16/04}
26795. Surface characterization of stainless steel substrate [The Netherlands]
26796. Optical properties of liquid copper [New York]
26797. Polymer solubility search [Scotland]
26798. Electroless copper for PCB (PTH) [Iran]
26799. Trivalent chrome plating [India]
26800. Nickel on steel, rust problem [England]
26801. Solving a potential electrolysis problem in home plumbing [Texas]
26802. Feritic nitrocarburizing [Wisconsin]
26803. Sherardizing [UK]
26804. General information about zinc electroplating [Bulgaria]
26805. Difference between Alodine 1200 and Alodine 1132 touch-N-Prep [Switzerland]
26806. Seeking Colorful Steel Coating -- Economical and Durable [Wisconsin] {1/19/04}
26807. Chuch steeple needs durable clear coating for multiple metals [New Hampshire] {1/19/04}
26808. Powder coating aluminum wheels [Texas]
26809. AMS2416 nickel-cadmium effect on alloy steels [Illinois]
26810. Testing virgin powder [Mexico]
26811. Furniture maker needs quick rusting of metal on log beds [Utah]
26812. Seeking anodizing for one piece of aluminum tubing [Illinois] {1/19/04}
26813. Titanium coatings [Indiana]
26814. E-coat on bare steel and weld nuts [Mexico]
26815. Nickel Plating of Aluminum [Maryland] {1/20/04}
26817. I need motorcycle parts plated [New York] {1/20/04}
26818. Cleaning old bolts for reuse (min 1 ton) [Australia] {1/20/04}
26819. Paints for glass bottles [Eritrea] {1/20/04}
26820. Need low emissivity high temperature paint [Canada] {1/20/04}
26821. Clear coat for copper protection [Ohio] {1/20/04}
26822. Synthetic diamonds [U.A.E.] {1/20/04}
26823. Germanium etchant [Pennsylvania]
26824. I want to come into metal finishing business can you help? [UK]
26825. Carb electroplating problems [North Dakota]
26826. Starting a Chrome Shop [Connecticut]
26827. Surface rust on stainless underhood parts of collectible car [Louisiana]
26828. Non heat treat cad plating [Georgia]
26829. What is the industry std for powder coating thickness [India]
26830. Troubles in Chloride Zinc Plating [Brazil]
26831. Electroplating situation in Canada [China]
26832. Cold process for pretreatment of metal [India]
26833. How to use sandpaper for sharp hairline on 430 stainless [Taiwan]
26834. Coating the anodes for high power laser cavity [Oregon]
26835. Acid corrosion of metals [Missouri]
26836. Metal Finishing Guidebook and Directory [Ohio]
26837. Ways to restore magnesium casting from white corrosion [India]
26838. Need a source for brass plating [California] {1/20/04}
26839. Cleaning of stainless steel pipes [Pakistan]
26840. Gold Electroplate on Rocks [Canada]
26841. Sandblasting media for cast aluminum [Canada]
26842. Metal blackener [Kansas]
26844. Why does silver tarnish? [Pennsylvania]
26845. Need paint for stove top [South Carolina]
26846. Muriatic Acid [Minnesota]
26847. Black oxide blueing [Ohio]
26848. Chroming an antique Corvette [Pennsylvania] {1/20/04}
26849. Need metal hammer parts brass coated [Missouri] {1/20/04}
26850. SEEKING A NEW CADMIUM PLATER [Massachusetts] {1/20/04}
26851. Need nickel chloride, nickel sulfate [Kentucky] {1/20/04}
26852. Need a Model 25TD air solenoid valve for Thorid, RAJ-2000 Filter Unit [Indiana] {1/20/04}
26853. Composite electroless nickel-PTFE [France]
26854. Electroplating tools using diamond [Mexico]
26855. Preparation of guns for nickel plating [Kentucky]
26856. Brightening of Immersion plated Tin surfaces on Printed Circuit Boards [Pakistan]
26857. Finishing wrought iron furniture [Canada]
26858. Copper patina finish on table [Illinois]
26859. Using and Cleaning an Overheated Pan [Virginia]
26860. MIL-C-26074 B grade A Class 1 [Ohio]
26861. Stripping Process for Immersion Gold [Arizona]
26862. Composition of Alballoy [Florida]
26863. Spec'ing black zinc plating [Ohio]
26864. Hydrogen Sulfide [Ecuador]
26865. Magnetic Properties induced into stainless steel thru cold work [Massachusetts]
26866. Aluminum transmission case badly corroded [Pennsylvania]
26867. Energion ECD [Germany] {1/21/04}
26868. Science fair project to plate screws [Canada]
26869. Need to find a Zn plating factory with production capacity [Taiwan] {1/21/04}
26870. Activating old nickel plate [Florida]
26871. Zinc vs Stainless vs Galvanized Fasteners [Texas]
26872. Removal of "plated" finish on brass [UK]
26873. Surface Treatment Procedure On Mild Steel [Malaysia]
26874. Demineralization of Water [South Africa]
26875. Need help with lot verification or passivation testing [Indiana]
26876. Chroming of Auto-Wheels [Michigan]
26877. Restoring lacquer finish to solid copper platter [Arizona]
26878. Plating onto titanium substrates [Texas]
26879. Incralac [Canada] {1/21/04}
26880. Seeking black chrome/nickel plating [California] {1/21/04}
26881. Chemicals for nickel plating too hard to find [Ohio]
26882. How do I restore shine to galvanized finish [Florida]
26883. Increased tensile strength through metal whiskering [South Africa]
26884. Painting a steel roof [New York]
26885. Problem with white rust on zinc dichromate surfaces [Missouri]
26886. Chemicals for testing zinc plating [Ohio]
26887. Stainless Steel Polishing [Alaska] {1/21/04}
26888. EVERLUBE 10026 lubricant [India] {1/21/04}
26889. Need a Teflon Coating Process for Anodised aluminium parts [Ireland] {1/21/04}
26890. Chroming: lamellar nickel and the columner nickel [Ohio]
26891. Chrome removal from plastic auto grill [Hawaii]
26892. Removing aluminum from a base metal [Michigan]
26893. Release coating for steel pultrusion die surface [Australia]
26894. Cold Sealing - Greenish Problem - 20micron [Saudi Arabia]
26895. Working With Transparent Conductive Coatings [Texas]
26896. Stripping bad silver plate [Kansas] {1/22/04}
26897. Need sissy bar chromed [Louisiana] {1/22/04}
26898. Need my rims refinished [California] {1/22/04}
26899. What metals rust the fastest (steel, copper, bronze) [North Carolina]
26900. Chrome plating plastic [Ohio]
26901. Options for Regenerating Phosphating Operation Chemicals [Texas]
26902. Laser marking of passivated parts [Pennsylvania]
26903. POLISHING OUT DIFFERENTIAL COVER [California]
26904. Nitric Acid percent to specific gravity [California]
26905. Dirty blind threads [New Jersey]
26906. Oxide Coating for Stainless Steel [Massachusetts]
26907. Coatings for fasteners [Hawaii]
26908. What is electrolytic reduction? [Philippines]
26909. Reconditioning Nikasil Clyinders [North Carolina]
26910. How good is EIS? [Ohio]
26911. Smoother finish on 304 SS [Texas]
26912. Shrinkage Control Machine [Pakistan] {1/22/04}
26913. Printing on precoated aluminum [UK]
26915. GLIDE COATING [India] {1/22/04}
26916. Re-enameling 1920 sink [Ohio] {1/22/04}
26917. Looking for a cleaning product for stainless [New York] {1/22/04}
26918. Removing concrete from aluminum finish [Indiana]
26919. Question about Stovepipes [Canada]
26920. Cleaning surface rust on stainless steel grade 304 and 316 [UK]
26921. Need electrophoretic lacquer [India] {1/23/04}
26922. Standards for diffusible or residual hydrogen [Cuba]
26923. Painting Nickel Plated Fishing Lures [New York]
26924. Platinum / Iridium 90/10 sputtering [Minnesota] {1/23/04}
26925. Goldpaint on shells/copperised leaves for jewelry [The Netherlands]
26926. Can coating of plating rack/jig could contaminate plating solution? [Philippines]
26927. Cleaning slate with muratic acid [Pennsylvania]
26928. Carburetor mfgr. needs very small size forgings [England] {1/23/04}
26929. Zinc nickel suppliers [Australia] {1/23/04}
26930. Seeking Decorative Electro Plater [New Jersey or California] {1/23/04}
26931. Need Copper trace element analysis service [India] {1/23/04}
26932. U.S.10-b finish on brass sheet [Connecticut] {1/23/04}
26933. Motorcycle shops seeks chrome plating services [Alabama] {1/23/04}
26934. Need machine for silver recovery [Bulgaria] {1/23/04}
26935. Specs for Chrome plating on Zinc Alloys [Spain]
26936. ANALYSIS OF A CYANIDE BATH [New Mexico]
26937. MIL-E-11195 dry time and hardness problems [Oklahoma]
26938. Powder etching primer [Malta]
26939. Effect of QPQ on thread strength [Canada]
26940. Sursulf Processing? [England]
26941. Will MIL-C5541 alter aluminum extrusion surface finish? [California]
26942. Removing the impurities from a stainless sheet [India]
26943. Rust Prevention of Sintered Components [India]
26944. Protective Coatings for Effluent Treatment Plant [India]
26945. Teflon Ty II, Green any information or contacts [Maryland] {1/26/04}
26946. Need one set of 16" rims chromed [England] {1/26/04}
26947. Acid dipping of an auto body [Maryland] {1/26/04}
26948. Vacuum metallizing plastic body panels [Canada] {1/26/04}
26949. Need gold and silver leafing service urgently [India] {1/26/04}
26950. Seeking chrome plater [California] {1/26/04}
26951. Cleaning Copper Roof [Texas] {1/26/04}
26952. Plastic media blaster wanted [Illinois] {1/26/04}
26953. What can cause the stains on the white gold jewelry and how they can be removed [Florida]
26954. Transfer of hydrocarbons via galvanized piping [Louisiana]
26955. Vibrations in zinc pot for galvanizing line [Romania]
26956. How do I remove color from PVD brass? [California]
26957. Nickel free brass plating process [India]
26958. White Passivation [India]
26959. Titanium Passivation in citric acid [Connecticut]
26960. Fine chips not washing out [Ohio]
26961. Selecting the correct Blast Media [California]
26962. Chrome Dip My Mazda Rims [Texas] {1/26/04}
26963. Seeking job working company for DACRO coating on fasteners and springs, press parts [India] {1/26/04}
26964. Wrinkle paint [California] {1/26/04}
26965. Need a 300 amp rectifier [Missouri] {1/26/04}
26966. Need DACRO Coating equipment for fasteners, press parts, springs [India] {1/26/04}
26967. Electropolishing rhenium and ruthenium surfaces [Spain]
26968. Properties of 2024 T351 [Washington]
26969. Anion supporting salt common-ion effect [Canada]
26970. Fixing a bumper dent [Florida]
26971. Aluminum Buffing [Alaska]
26972. Raw deal with the raw steel [California]
26974. Disposal of unused muriatic(hydrochloric) acid [Delaware]
26975. How To Begin Electroforming [Australia]
26976. How to remove nickel oxide [The Netherlands]
26977. Silverplating problems [India]
26978. Removing chloride from silver KCN bath [Thailand]
26979. Can you anodize in bright yellow [England]
26980. Sanitary finish on tanks [England]
26981. Corrosion preventive compound / MIL-C-16173 [Pennsylvania] {1/27/04}
26982. Anodized aluminum welding [Massachusetts]
26983. Lightweight shaft for air bearing [England]
26984. Gold plating parameters [England]
26985. Is silver jewelry being chrome plated? [Germany]
26986. Difference between tin-lead and tin-bismuth? [Philippines]
26987. Student project about polyacrylic acid and aluminum [Iran]
26988. Chemical reaction between salt and sulfamic acid [Wisconsin]
26989. How to form a ball on the end of a stamping [England]
26990. What is the number of computers to make one ounce of gold? [Minnesota]
26991. How is a Euro coin like a wet cell? [California]
26992. Anodizing over Teflon [Illinois]
26993. Teflon coatings for rubber [South Carolina]
26994. Removal of gold plate/wash from sterling silver jewelry [Connecticut]
26995. Need manganese phosphating service [India] {1/27/04}
26996. Touching up anodizing that is void of color [Australia]
26997. UV coatings for FRP profiles [India] {1/27/04}
26998. Information on brush plating technology [India] {1/27/04}
26999. Suspected sulfide related cracking of CF8M pump casing - Soda ash industry [India]

The finishing.com Hotline has been on the Internet since '95 and includes more than 50,000 threads about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to start at our home page, view the most recent letters, or search the site.


© finishing.com, inc., 1995-2009