13000. Rusty SUS303
13001. Coating on copper to save from molten zinc
13002. Treatment of hollow core steel window frames
13003. What is DIN 50960 plating?
13004. CORROSION OF SS BY CHLORIDE IONS
13005. Refinishing old wrought iron furniture
13006. Atmospheric evaporators/zinc chloride
13007. Cyanide Zincate
13008. Nickel Strike
13009. Black Chem Film or Conductive Finish
13010. Passivation-Abrasive Blasted Stainless Steel
13011. Sludge removal from Zinc Cyanide tank
13012. Seeking X-RAY Fluorescence measurement [Singapore] {2/15/02}
13013. Rate constant of HCl+FeO reaction
13014. Nickel electroplating
13015. Use of Galvanize Metal in Heated Environment
13016. Electroplating equipment and supplies information
13017. "Cratering" after cataphoretic painting on galvanealed steel
13018. 12 ct. HARD PLATING OVER COPPER ITEM
13019. Stamping(Etching) on Stainless Steel
13020. Does ASTM A967 Practice D apply to age hardened 17-4 ph stainless steel?
13021. 420 corrodes around laser etching
13022. Stainless Steel Finish Specification
13023. Plastisol vs. powder coating
13024. Electroless copper
13025. Seeking source for application of Deltaseal Coating [Taiwan or China] {2/18/02}
13026. Graphite coating
13027. Seeking hot oil reflow on tin [Illinois] {3/05/02} 2nd Request
13028. Seeking sources for plated roses [California] {2/19/02}
13029. Salt Spray Corrosion Comparison
13030. Bright color for anodizing aluminum
13031. Amount of per side surface removed by anodizing
13032. Seeking Powder Coating Machine [India] {2/19/02}
13033. Seeking 6063 cathodes [Illinois] {2/19/02}
13034. SEEKING HYDROCHLORIC ACID INHIBITOR [JORDAN] {2/19/02}
13035. What's the history of industrial electroplating
13036. Electrodeposition of Alumina
13037. Reclaim Gold from Electronics
13038. Brick Stripping (external)
13039. Polishing Harley disc brake
13040. Determination of silver in fixer solution
13041. How do I age steel quickly?
13042. Dip Clean For Old Aluminium Carbs
13043. Gold plating over lead
13044. Separating mercury from gold jewelry
13045. HMIS ratings
13046. Stripping of hooks
13047. ZINC PLATING AND OLIVE BLACK PASSIVATION (CHROMATING)
13048. QA INSPECTION
13049. Best Protection for Parking Meter
13050. Surface finishing... galling of 410 against 440C stainless steel
13051. Iron Build-up in Acid Copper Bath
13052. Etching on Iron
13053. Pickling before chrome plating
13054. Ra 0.4 finishing requirement for small part of tool steel
13055. Nickel plating flaking from revolver - would like to remove plating
13056. Seeking coloring resin [China] {2/20/02}
13057. Seeking circumferential surface measurement [England] {2/20/02}
13058. Aluminum 6061T3 and 7075 Alloy
13059. Rusting a wedge
13060. Rack stripper
13061. Black passivation process
13062. Electroless coating
13063. Conductive paints for electroforming onto non-metallic items
13064. Blister Problem
13065. Solvents and Alodine conversion coating
13066. SEEKING STRESS RING [Singapore] {2/20/02}
13067. Coating questions
13068. Is electroplated hard chrome corrosion-resistant at all?
13069. Seeking Ashing-off Diamond-like-carbon coating on Tungsten Carbide surface [South Carolina] {2/20/02}
13070. Seeking checker plate [Scotland] {2/20/02}
13071. Seeking suppliers to expand plating supplies business [Canada] {2/20/02}
13074. Remove tin plate and lead solder from copper vessel?
13075. Chrome removal advice
13076. Future/upcoming Cd regulations
13077. Ion exchange resin regeneration
13079. 2024-T3 Spec for Iridite / Alocrom test panels
13080. Nitric vs Phosphoric Acid Based 316L SS Passivation
13081. Copper aluminum problem
13082. Industrial anodizing
13083. Knife maker seeking help
13084. Seeking Platinum Oxide Coated Titanium Sheet [Australia] {2/20/02}
13085. RECOVERY OF PLATINUM GROUP METALS
13086. Cleaning after PCT test
13087. Optical properties of surfaces with Alodine treatment
13088. Copper coating
13089. Cadmium vs. Zinc vs. Nickel Plating Comparison
13090. Seeking metal lacquer [New York] {2/20/02}
13091. Wire Rod Defects
13092. SEEKING ZINC PLATING ON STEEL SHEET 7/8"THICK X 66" X 72" [Pennsylvania] {2/20/02}
13093. Seeking scratch resistance top coat for high vacuum metallization [Turkey] {2/20/02}
13094. Preparing gold potassium cyanide
13095. Techniques to process gold and silver
13096. Gold underplating
13097. Black Oxide problem
13098. Stannate Process
13099. Hard Coat Penetration
13100. Vibratory tumbler/tumbler process and machine
13101. Seeking Low IR Reflectance Primer\Coating [California] {2/21/02}
13102. WHICH SOLUTION WILL CHANGE THE COLOR OF A PENNY THE QUICKEST? WHY?
13103. Thin film gold or platinum on polymer spheres
13104. Post-welding Heat Treatment of Aluminum
13105. Removing brass plating
13108. Hard chroming process
13109. Electropolishing copper by using phosphoric acid
13113. Electrocoagulation
13114. BLACK OXIDE SET-UP
13115. PVD gold color matching
13116. Nodulation
13117. Formulas for nickel plating solution
13118. Preparing bismuth for plating (or blackening)
13119. Heavy Duty Hardware Corrosion Protection
13120. Antiquing brass hardware
13121. Aluminum clear coat removal
13122. INTERNAL FINISH ON WAVEGUIDE (COPPER)
13123. Sludge production in the treatment process
13124. Chemical conversion coating degradation under heat and water
13125. Trouble rinsing small dia tube with one end closed for black hardcoat
13126. Passivation with Citric Acid+Sodium Dichromate
13127. Effect of Brushing on Hardness of Stainless Steel Sheet
13128. Aluminum corrosion problem by copper
13129. Anodize/plating for Al to resist bromides
13130. Solenoid armature
13131. Nickel growing planarly
13132. White gold or Rhodium plated confusion or deception
13133. Testing for Hydrogen Embrittlement
13134. Galvanized coating problem
13135. Help for a small fishing tackle company
13136. Will a citrus-based cleaner replace MCF for immersion patina?
13137. Seeking hot dip tinning [Massachusetts] {2/22/02}
13138. How is this kind of chromium plating working?
13139. Flexible + durable finish on expanded polyethylene foam
13140. Cleaning solutions for copper antique products
13141. Ni recovery by electrolysis
13142. Coating for ferrous metals
13143. Glass bead blasting of hardened steel causing hydrogen embrittlement
13144. Seeking tape for tape pull test [California] {2/22/02}
13145. Temperature for stainless steel to become magnetic
13146. Marine stress and corrosion on underwater bolts
13147. Wrinkle/Texture Paint for Metal
13148. Light scratch in stainless steel counter top
13149. Aluminum went cloudy!
13150. Clear coat for mid-century steel desk
13151. White gold dilemma
13152. CLEANER TITRATION REQUESTED
13153. PALLADIUM STRIPPER FOR CERAMIC CAPACITORS
13154. Ink adhesion on anti-finger print coatings
13155. Why is aluminum sputter not shining even after leak check and sample cleaned
13156. SEEKING SMALL ALUMINUM PART FINISHING [Texas] {2/22/02}
13157. Studying Copper
13158. Stainless Steel Elevator Door Refinishing
13159. Faux antique mirror
13160. Permalloy detection
13161. Brightening Hard Chrome Surfaces
13162. Gold plater rinse water reclaim
13163. Seeking DRY BONDED LUBRICANTS FOR MILITARY WEAPONS [India] {2/22/02}
13164. Seeking black endurion [France] {2/22/02}
13165. Seeking ion implantation of 410 stainless steel parts [Georgia] {2/22/02}
13166. Seeking VCI chemicals and process method [Turkey] {2/22/02}
13167. NYBCO spray paint
13168. Copper Kitchen Counters
13169. Final Polishing-1/4"Wooden Pegs or Walnut Shell Fine Grit 20/30
13170. How to make bronze medals from a model in gypsum
13171. Burnt Plating
13172. Silicon mark
13173. Seeking Platinum Coating (Liquid) [India] {2/22/02}
13174. Black Diamond Coating [California] {2/22/02}
13175. How do you retin a copper pan
13176. Wire coating thickness instrument
13177. Seeking methyl methacrylate (dura flex) final surface prep [Oregon] {2/25/02}
13178. Seeking equipment for bronze plating [New York] {2/25/02}
13179. Seeking easily available sources of hypo solutions for silver extraction [India] {2/25/02}
13180. Seeking welding machine for mineral insulated wires [U.A.E.] {2/25/02}
13181. Seeking gold stripping solution [California] {2/25/02}
13182. Metal finishing wastes treatment methods
13183. Information about polysulfide resin
13184. Advantages and disadvantages of carburizing
13185. Help, permanent thick film on si
13186. Metallurgical Lab
13187. Can I use a cast-iron/ baked enamel bathtub for saltwater fish?
13188. New 18k white gold ring changes color
13189. Non-conductive
13190. Lead
13191. What's the best way to remove tarnish from solid bronze hardware?
13192. Green stuff on brass
13193. Anodized finish removal from aluminum
13194. Rusting Garage Doors
13195. Seeking wrinkle black paint [Connecticut] {2/25/02}
13196. Refinishing wooden counter top
13197. Coloring titanium
13198. Help with a military finish spec
13199. Definition of MIL-C-10578 spec
13200. Relative 'corrosivity' of pH adjusting acids in aqueous waste streams on black iron grease trap components
13201. Waste Water Troubles
13202. 316SS MIM Part Galling Problem
13203. SS stripper solution
13204. Bright Annealing Stainless Steel Sheets
13205. Corrosion protection on grey cast iron
13206. Yellow iridescent chromating of castings
13208. How To Prepare Mill Finish Aluminum for a One Part Acrylic Lacquer?
13209. AMS vs MIL Specs
13210. Biomaterials
13211. Electrolytic cleaning
13212. Sandblasting versus 7 tank prior to powder coating
13213. Abrasive finishing technique
13214. Inconsistent Rusting on 316L Welds
13215. Seeking AR-1500 metal rustproofing [Florida] {2/27/02}
13216. Silver questions
13217. On an anode bags importance
13218. RESTORE WOOD COOKSTOVE
13219. Kitchen cupboard hardware
13220. Clearcoat finished zinc-coating for metal doors
13221. Seeking bronze protective coatings [Bahamas] {2/27/02}
13222. Copper electro plating
13223. Chrome Removal Question
13224. Coating anti-scratch
13225. Olive drab (green) passivation of aluminium alloy items
13226. Seeking machines for razor blades, safety blades [India] {2/27/02}
13227. Seeking wheel polisher [Canada] {2/27/02}
13228. Brightening chrome surface without polishing
13229. Preventing copper tarnishing
13230. Seeking copper plating supplier [North Carolina] {2/27/02}
13231. Al etching operating conditions?
13232. Corrosion resistance of different colored dichromate coatings over zinc
13233. Nickel Plating
13234. Bromate deoxidizer for aluminum
13235. Plating Copper in a Steel Pickling Line?
13236. Electroplating organic material
13237. 3 micron titanium etch
13238. Coating the inside of a hourglass shaped object
13239. HDMP dry lubricant
13240. Type of metal for anode cages
13241. Do Stainless Steel and CLO2 Mix?
13242. Plating plastic helmet....
13243. Fiberglass boat oxidation
13244. Zinc or Galvanized Poisoning Symptoms
13245. Need material most suitable for chrome plating fixtures
13246. Seeking electroforming machines [Jordan] {2/27/02}
13247. Seeking silver paint and electroless polishing [Indonesia] {2/27/02}
13248. Seeking nichrome wire [Pakistan] {2/27/02}
13249. Seeking Zn/Fe alloy sheet [Canada] {2/27/02}
13250. Composition of coins
13251. Expt procedures (EN on Al)
13252. Chrome plating adhesion standard
13253. PVC compound
13254. Chrome plating titanium
13255. Stainless steel pipe for sea water
13256. Infra Red Reflectivity
13257. Seeking industrial Peptone [UK] {2/28/02}
13258. Seeking rims dipped in chrome [Louisiana] {2/28/02}
13259. Weld or bond polyethylene?
13260. Simple Metal Plating
13261. Soda acidic
13262. Stainless Steel Flatware
13263. Gold zinc with yellow chromites
13264. Clorox bleach test procedure
13265. HOW TO STRIP HARD CROMIUM FROM ALUMINUM
13266. Hex chrome on pregalvanized steel coils
13267. Cold dip black oxides
13268. Oxalic Acid in Type II Anodize
13269. Poor color of anodized material
13270. Laser cut parts
13271. Corrosion of "pure" aluminum
13272. Spring corrosion resistance
13274. Seeking heat treat protective coating, 2100F, steel parts [Missouri] {2/28/02}
13275. Weight Of Organ Pipes
13276. Cost comparison galvannealed/aluminium/FRP
13277. How long does it take for natural gas to corrode copper pipes?
13278. Standard for chromating zinc die cast components
13279. Nickel electroforming, join with steel
13280. Sn-Co alloy coating
13281. How to plate lead
13282. How can I passivate stainless steel part without destroying silver solder joints
13283. Seeking rims polished [North Carolina] {2/28/02}
13284. Nitinol Parts Soldering
13285. Seeking dye passivation of stainless parts [Canada] {3/01/02}
13286. Seeking source for air drying plastisol [Georgia] {3/01/02}
13287. Coefficient of Friction for AMS-C-5541 Coated Surfaces
13288. Stains and stress marks on clear anodized
13289. What cleans a metal(copper, iron, gold, bronze, etc.) chemically? What process?
13290. PrePlate Processes
13291. SALT SPRAY RESULTS?
13292. Shining anodized aluminum
13293. Chromate Conversion Coatings
13294. Polishing of punches
13295. Acid Types in Autophoretic Process
13296. Cleaning fingerprints off electroplated tin and zinc finishes
13297. The effects of anti-static packaging on electro-plated zinc finishes
13298. Seeking yellow iridite pens [Virginia] {3/04/02}
13299. Seeking finishing help on bronze letters [Minnesota] {3/04/02}
13300. Shape of Anodizing Rack Clips
13301. Seeking Cobalt Alloy Gyro shafts [Australia] {3/04/02}
13302. Seeking Hologram materials and equipment [India] {3/04/02}
13303. Colored concrete treatment
13304. Rust removal and inhibition for a refrigerator on a saltwater boat
13305. Ospho Refinishing
13306. How do I put a design/pattern on a stainless steel tabletop?
13307. Seeking electroforming of cavity insert of worm gear [Singapore] {3/04/02}
13308. S and B standard for MS Plates
13309. Charcoal Blue Info Needed
13310. Seeking Muriate of Potash [West Europe] {3/04/02}
13311. Seeking Transparent Conductive Film or Ink [California] {3/04/02}
13312. COST OF IRIDIUM
13313. Seeking equipment for making Gold Potassium Cyanide [China] {3/04/02}
13314. Broad Spectrum Transparent Glass
13315. What is fusion bonded epoxy?
13316. Seeking gold plating unit [India] {3/04/02}
13317. Electrolytic steel derusting
13318. Seeking powder coat 30,000 screws [Texas] {3/04/02}
13319. Reblueing guidelines
13320. How do I remove RUST from car before paint touch up
13321. Etching titanium
13322. Polishing circlips or jumplinks
13323. Manufacturing problems on stainless pipe (industrial and ornamental)
13324. Seeking metal wire electroplating equipment [Saudi Arabia] {3/05/02}
13325. Seeking chromium-look paint or powder [India] {3/05/02}
13326. Searching for antique elevator door pictures
13327. Seeking equipment to mfg. Gold Potassium Cyanide [Indonesia] {3/05/02}
13328. Seeking supplier to electroplate iron on metallic surfaces [California] {3/05/02}
13329. Finishing of Antique Cast Iron Book Press
13330. VERY Large Clear Anodizing Tank
13331. Cleaning chrome
13332. ENAMELING PLANT FOR CAST IRON BATHTUBS
13333. Acid Choice for Cleaning Aluminum Alloys
13334. Metal Finishing Question From Non-Professional
13335. Seeking electroless nickel plating for steel [Australia] {3/05/02}
13336. Treatment for used water in plating process
13337. How to reduce dross generation?
13338. How to build a small galvanization line
13339. Seeking Rh plating over Cu [Utah] {3/05/02}
13340. D.I.Y. bronze casting- Ceramic Shell technique
13341. Info Required about Drying Curves
13342. Etchant for Aluminum 5xxx series welds
13343. Mo-Cr Plating
13344. Laser surface conditioning of aluminium aero alloys to increase bonding
13345. Spirits of nitre
13346. Alodine: Is there a difference?
13347. Chromate Environmental Concerns
13348. Galvalume (OR Aluminum-zinc coating)
13349. Chromate for hot zinc galvanizing
13350. Color variations/spotting problems
13351. Suggested ASF for hardcoat anodizing
13352. Risk in passivating cres 416
13353. Chem Milling, what to do
13354. How to finish brass
13355. Stability of 420F Stainless
13356. Zinc plating of case hardened steel
13357. Best Malleable (Non-Flaking) Finish for 12L14
13358. Seeking gold plating bath [Italy] {3/06/02}
13359. Aluminum can printing
13360. Steel chemical cleaning
13361. Acid required to etch aluminum
13362. Data on NYLON PA12
13363. Alternative for dichromate as separation layer for silver
13364. Chairs
13365. Electrically Conductive Coating for Aluminum
13366. Problem in zinc phosphate
13367. Passivation of Stainless Steels and Titanium
13368. Surface finishing handbooks
13369. Stained stainless in elevator cab
13370. Potassium and cyanide content in plated silver
13371. Removing old anodizing
13372. Nylon coating
13373. Seeking water base lacquer for jewelry products [Pakistan] {3/06/02}
13374. Gold plating reaction
13375. Gas flow through irregularities in surface finish
13376. Salt Spray inquiry
13377. Nickel plating molds
13378. Corrosion of stainless steel tank
13379. Surface finish
13380. What is the formula for surface finish ratings?
13381. Coating/Treatments for a Hydrochloric environment
13382. Seeking chemicals [Iran] {3/07/02}
13383. Splash Anodizing
13384. Knoop Hardness
13385. Corrosion resistance to 1000+ hours
13386. Plating safety training program
13387. Titanium finish on mechanical hardwares
13388. Galvanized roofing for bathroom walls
13389. Reliable coating weight procedure for Alodine+SA on Al needed
13390. Leldo por favor
13391. Seeking suppliers of bluing chemicals and process details [India] {3/07/02}
13392. Seeking machinery for powdercoating [India] {3/07/02}
13393. Preparing sea shells for crafts or display
13394. Advantages of treating water for drinking by electro coagulation
13395. Geometry Riddle
13396. How to Clean Brass Beds
13397. Wood Plating
13398. Cleaning copper... FAST
13399. Electric properties of black zinc surfaces
13400. Zinc Plating Platinum
13401. To Remove Zinc from Nickel Sulphate Solution
13402. Pickling and passivation for preventing rust on stainless
13403. Seeking hard finish on steel for use at 850 deg F [Wisconsin] {3/08/02}
13404. Remove galvanic stains from a polished steel (cast steel, cast iron) table surface
13405. How to polish and clean Hastelloy for ultrahigh purity
13406. SURFACE FINSH CHART
13408. Hydrogen Embrittlement of Brass Pins
13409. Seeking chrome re-dipping for my rims [Massachusetts] {3/08/02}
13410. Seeking aluminum burnishing or brushing equipment [South Carolina] {3/08/02}
13411. Plating too thin
13412. Seeking BLACK CHROMATE metal finishing [California] {3/08/02}
13413. Seeking conductive coating for glass that can accept 120VAC [Pennsylvania] {3/08/02}
13414. Pre-anodized aluminium
13415. Removing zinc from an iron galvanized nail
13416. Using liver of sulphur on bronze
13417. Nickel/chrome plating of pewter toys
13418. 304 stainless steel
13419. Clear passivation of copper and effects on electrical conduction
13420. Graphite suspension to coat over organic films
13421. Challenger Two
13422. Gold electroless plating solution
13423. Problem with chrome coming off
13424. Copper bar top, need adhesive
13425. Seeking E-ni plus Solder Dipping [California] {3/09/02}
13426. Need Plated Plastic Car Dash for magazine shoot [N.J.] {3/10/02}
13427. Seeking anodizing of bumper and nerf bars [N.C.] {3/10/02}
13428. Seeking powdercoating [N.J.]{3/10/02}
13429. Suppliers for Oxygen Scavengers for Boiler Feed Water [India] {3/10/02}
13431. Electroplating problems with my science fair project
13432. Etching titanium without Hydrofluoric acid
13433. I need info for my chemistry assignment
13434. Colored Anodized Aluminum Information
13435. Availability of spray teflon?
13436. Polishing Formica and brushed aluminum
13437. Copper Anodized Aluminum
13438. S/S to Steel Electrolysis and Corrosion
13439. Fine etch for aluminium
13440. Require copper antique coating process [India] {3/10/02}
13441. Aluminium-plated paper Wanted [China] {3/10/02}
13442. Clear resin floor tiles need strong wear resistant coating
13443. References to help explain why citric acids clean pennies best
13444. Staining, coating and adhesives for metals
13445. Metal Finishing Questions from Non-Professional
13446. Anodize type III class 2 in color?
13447. Finish for Al-Alloy to Meet Corrosion and Contact Resistance
13448. Hard Chrome vs Electroless Nickel and Nitriding
13449. Need help setting up Hologram industry [India] {3/11/02}
13450. Wanted Suppliers for Ruthenium Oxide [India] {3/11/02}
13451. Process, Equipment & Chemicals For Multicolour [India] {3/11/02}
13452. Repair of surface scratches in plastic laminate counter top
13453. Hot bluing problem
13454. Caustic Recovery
13455. ASTM B117 duration - real time correlation
13456. Plating on titanium
13457. Cleaning Nickel on Banjo [Tennesee]
13458. Seeking black anodize of some aluminum castings [Calif.] {3/11/02}
13459. Al Cast plating for high humidity and drinking water contact [New York City]
13461. Researching Automotive Spray Booths [New York]
13462. DI water on Tin plated Copper coils [Louisiana]
13463. Chromate conversion coating in lieu of anodizing? [California]
13464. Reactive Sputtering target material? [Australia]
13465. Faded zinc plating protection by washing process [Brazil]
13466. Cathodes for phosphoric acid anodize [Ohio]
13467. Treatment of aluminium brightening effluent [U.K.]
13468. Al Etchant [Singapore]
13469. How to select suitable IR Heater [India]
13470. Gold Alloys [Mexico]
13472. Steel ball polishing [India]
13473. Finishing to Inhibit Corrosion of Aluminum [Kansas]
13474. QA ENG - Solderability testing [Israel]
13476. Electroplating basic steel [Finland]
13477. Properties of anodizing film for cooking wok [Singapore]
13478. ASTM B633 Appearance standards [California]
13479. Salt Spray Test on Clear Chem Film [California]
13480. CLEANING ANODIZED SURFACES [Illinois]
13481. Can't find a suitable Power Supply / Rectifier [N.J.] {3/13/02}
13482. Paintball Aluminum Plating [Connecticut]
13483. Electrowinning of Chrome Questions [Massachusetts]
13484. Need U.V. Curing oven for glass-to-metal seals [India] {3/13/02}
13485. Seeking process equipment to make Gold Potassium Cyanide [Hong Kong] {3/13/02}
13486. Stripping Nickel from Brass [Ontario, Canada]
13487. Alumina coating [India]
13488. Looking for help with more complex high school plating experiments [UK]
13489. Gold Potassium Cyanide Market [France]
13490. ALUMINIUM CORROSION- stannate [France]
13491. Seeking powder coating system [Libya] {3/14/02}
13492. Electropolishing equipment [Norway] {3/14/02}
13493. Looking for sprayable selective plating mask [Calif.] {3/14/02}
13494. Effect of scratch width in salts spray test on painted galvanized steel [Belgium]
13495. Need cyanide-free silver plating solution [Texas] {3/14/02}
13496. Plating on Fiberglass Bumpers [California]
13497. Powder adhesion problems on MIG welds [Indiana]
13499. Need cleaner for scale from alkaline etch process [Washington] {3/14/02}
13500. Mechanical student seeking help [South Africa]
13501. Electrolytic and electroless plating as well as mirror finished Ni plate [California]
13502. Restoring surfaces in 1964 Porsche engine [Texas]
13503. Counterflow rinsing design [Australia]
13504. Blistering of Powder Coat on a Yellow Zinc Plated surface [Massachusetts]
13505. Quality control of functional PVD layers based in solar absorber for thermal collectors [Portugal]
13506. Electroforming molds question [Mexico]
13507. Leaching on one of two batches of components Zn3A + JS500 plated [U.K.]
13508. Black Chrome Information [Rhode Island]
13509. Aesthetic conductive metal finishing [California]
13510. Need a Soluble Anode of Co or FeCo [New Jersey] {3/15/02}
13511. Placa litografica de compuesto de asfalto y aceite de lavanda experiencia [Peru]
13512. Need pretreatment chemicals for aluminum [India] {3/16/02}
13513. Uniformity of depositions [Texas]
13514. Plating of lead for stained glass [Florida]
13515. Applied basics of sodium cyanide case hardening for steel [Mexico]
13517. Electrolytic Paste [Columbia]
13518. Hardcoat Acid Concentration? [Ohio]
13519. Cleaning White Gold... help please [Oregon]
13520. Surface finish values [Illinois]
13524. Need Silver Plating process for engineering purposes [Iran]
13525. Brass Cash Register Nickel Removal [Indiana]
13526. Basic Plating Help [Florida]
13527. Coating a hole with carbon black or other electroless plate [California]
13528. Tolerable conc. of copper for cyanide zinc baths [Iran]
13529. Burnt product in the electro plating tank [Singapore]
13531. Masking ink questions [Israel]
13532. Best steel type for galvanizing? [India]
13533. Seeking 52100 bearing material [Toronto, Canada] {3/18/02}
13534. Powder or liquid painting aluminum [Argentina]
13535. Seeking clear coating for copper [UK] {3/18/02}
13536. Chemistry assignment [Australia]
13537. Getting into chrome dipping [Louisiana]
13538. Finding zinc plate [Minnesota]
13539. Painting wrought iron furniture [Ohio]
13540. How to oxidize galvanized steel for home craft project [Illinois]
13541. Guidance for bright finishing of SS parts [India]
13542. Metal prep on a lathe [Ohio]
13543. Metallurgical science [Australia]
13544. Effect of temperature on copper deposition [Scotland]
13545. Search for etchant of aluminium for reflow mask [France]
13546. Making stainless steel 304 nonmagnetic [India]
13547. Finish for exterior steel sculpture [New Mexico]
13548. Velour nickel headache [South Africa]
13550. Rinses and water usage [Washington]
13551. Advice on QPQ [New York]
13553. SEEKING FIRETUBE BOILER 800 BHP [Columbia] {3/19/02}
13554. Eliminating silver tarnish from antique silver pictures (daguerreotypes) [Maryland]
13555. Welding Yellow Chromate vs. Clear [Michigan]
13556. Alloy Specific Salt Spray Failure of Sulfuric Anodize [Idaho]
13557. Passivation of AISI 431 [India]
13558. How to restore a rescued iron bed frame [Georgia]
13560. Seeking high-speed reel to reel equipment [China] {3/19/02}
13561. Answer to these word equations [England]
13562. Outside wood finish [Georgia]
13563. Chemical labeling [New Jersey]
13564. Prescription electroless nickel plating [Holland]
13565. 925 silver plating [China]
13566. Restoring polished aluminum finish [England]
13567. Life age of Dacrotizing process [Taiwan]
13569. Er2O3 coating [The Netherlands]
13571. Restoring old side bys [Florida]
13572. Coating for stainless 304 - where hydrochloric acid fumes are present [Ohio]
13573. PHOSPHATING [India]
13574. Restoring Brass Fixtures [Missouri]
13575. Restoring old wood exterior doors [Missouri]
13576. Request for information to obtain FED-STD-595 [Texas]
13577. Automatic pH measurement in nickel electroplating tank [Tennessee]
13578. Electropolish questions [Ohio]
13579. Is powder coated galvanized steel a good exterior finish [Texas]
13580. Die cast magnesium (AZ91D) coating for FDA compliance [Australia]
13581. Burnt stain on brass fireplace screen [Maryland]
13582. Blunt Blade [Australia]
13583. Tinplating or Aluminum [Wisconsin]
13584. Electrodialysis for aluminum removal from caustic solution [Australia]
13585. Alkaline anodising [India]
13586. Ways for removing oxidized Ni [Israel]
13587. Electropolishing Inquiry [India]
13588. Effect of potassium formate on Zn-Ni plating [Michigan]
13589. Unit for copper plating [India]
13590. SEEKING CATAPHORESIS SYSTEM [Turkey] {3/21/02}
13591. Composite Diamond Coating [Indonesia]
13593. Seeking gold electroforming and plating equipment [India] {3/21/02}
13594. Painting a brass bed [Virginia]
13595. Copper counter tops [Nebraska]
13596. Polishing titanium bike frame [New York]
13597. Sheet metal counter top [Texas]
13598. Nickel plating stripping method [Pennsylvania]
13599. Make palladium in the channel of porous Alumina for catalyst use [Pennsylvania]
13600. Steel kettle or tile lined concrete [Saudi Arabia]
13601. Burning on end of steel tubes (Copper plating) [California]
13602. Neutral cyanide gold bath [U.A.E.]
13603. Chip Burning during plating process [Malaysia]
13604. Plating silver on stainless steel [Virgin Islands]
13605. Why does the hard chrome on nickel fail [India]
13606. Anodizing zinc [Wisconsin]
13607. Stainless coloring [Texas]
13609. Why use cadmium plated fasteners in the aeronautical field [England]
13610. Copper paint/finish [Colorado]
13611. Hub Coating [California]
13612. Surface Finish Specifications [Ohio]
13613. Corrosion Problem on Ductile Iron Castings [Canada]
13614. Aluminum corrosion preventative [Pennsylvania]
13615. Burnish/Hone [Wisconsin]
13619. Seeking conductive paint for anodes [Singapore] {3/22/02}
13620. SEEKING TITANIUM MATERIAL SUPPLIERS IN ORTHOPEDICS AND FINISHERS TO TITANIUM METAL [India] {3/22/02}
13621. Seeking very durable and protective finish for large quantity of brass handrails [Indiana] {3/22/02}
13622. Seeking electropolishing equipment-Used or New [Quebec, Canada] {3/22/02}
13623. Wetting problem [Illinois]
13624. Searching for supply/muric acid [Hawaii]
13625. Safety requirements [China]
13626. HCN concentrations in plating baths [Washington]
13627. Degreasing of 300 and 400 series stainless steel [India]
13628. Passivation and mirror polish [India]
13629. Best coating for rust resistance for valves [Pennsylvania]
13632. Copper Sulphate and Trout [New Zealand]
13633. How do refrigerator magnets work [New York]
13634. How do I customize a mirror [Michigan]
13635. Plating over 18k yellow gold [Pennsylvania]
13636. Gold plating temperature resistance [Canada]
13637. Seeking Teflon coating for car [India] {3/25/02}
13638. Seeking UV Spectrophotometer [India] {3/25/02}
13639. Seeking liquid compound to polish stainless steel plates [India] {3/25/02}
13640. Mechanical properties of 4340 steel [Australia]
13641. Coating of slurry thin layer on a 3D surface [Singapore]
13642. Aluminum tray from 40's needs touch up paint [Georgia]
13643. How to find Mil spec [Thailand]
13645. Seeking Polystone/Polyresin/Polyurethene for statue molding [India] {3/25/02}
13646. Water stains in wood [Virginia]
13647. Motorcycle aluminum problems [Kansas]
13648. Painting an aluminum outdrive [Ohio]
13649. Insulating a metal sheet to render it non-conductive with spray paint [Canada]
13650. Nickel Plating Brass [Canada]
13651. Dealing with rust on clawfoot tub [Kansas]
13654. Seeking used screw type, noiseless air compressor [Illinois] {3/25/02}
13655. Seeking Semi-Automatic Electroplating Machinery [U.A.E.] {3/25/02}
13656. Carbon steel counter top [Texas]
13657. Can I color rusted cast iron [Pennsylvania]
13658. Etching Ti-Nb and V-Nb micro-alloyed steels [Louisiana]
13659. Titanium Anodized Custom Implant [New Zealand]
13660. Sealing problem [Canada]
13662. Seeking platinum coated titanium electrodes [Sri Lanka] {3/25/02}
13663. Seeking powder coating facility for steel [California] {3/26/02}
13664. Seeking Dust Collector System [Michigan] {3/26/02}
13665. Seeking titanium tubing [Indonesia] {3/26/02}
13667. Making sodium hypochlorite [India]
13668. DIE CASTING PROBLEM [Lebanon]
13669. Black paint/low reflectivity [Texas]
13670. Matte black metal finishing; White gold + rhodium [Sweden]
13671. To Blue or not to blue that is the kanundrum [Florida]
13672. Wrought Iron Restoration [North Carolina]
13673. Referenced color systems [Canada]
13674. Nodules in Nickel Plating [Massachusetts]
13675. Passivation of the Titanium [New York]
13676. Petreament for titanium [Sweden]
13677. Solar Loading [Pennsylvania]
13678. Seeking supplier for Nikasil prototype coating for automotive application [New York] {3/27/02}
13679. Seeking silver plating thickness tester [India] {3/27/02}
13680. Seeking Teflon coated water heater coils [India] {3/27/02}
13681. Acid Concentrations in slow-rust formula [Denmark]
13682. Passivation of stainless steel [Latvia]
13683. Superiority of SS410 over ENP [India]
13684. Hard Anodized Aluminum [New Jersey]
13686. Electropolishing Cobalt Chromium [South Africa]
13687. De-silvering Mirrors [Michigan]
13689. Seeking diamond particles for EN Diamond Composites [Indonesia] {3/27/02}
13690. Sputtering Copper onto Platinum [UK]
13691. Nodules on Silver Plated Copper Substrates [Massachusetts]
13692. Preserving copper brightener [Washington]
13693. Zinc corrosion resistance vs. Cadmium [Pennsylvania]
13694. Seeking chroming of magnesium [Rhode Island] {3/27/02}
13695. Etching steel before painting and endurance [California]
13696. Ring question, gold to silver [Minnesota]
13697. Recommendation for Current Density [Malaysia]
13698. Phosphate Treatment of Compressed Air Pipes (Internal) [Australia]
13699. Bonding rubber to titanium [India]
13700. Zinc cobalt alloy electroplate chromating [Iran]
13701. Iron coating [India]
13702. Seeking supplies for electrochemical etch marking of titanium [Czech Republic] {3/28/02}
13703. Simple torque wrench calibration [Georgia]
13704. SEEKING ALLOY WHEEL LATHE [Ohio] {3/28/02}
13706. EN-Teflon for Food Applications [New Jersey]
13707. Wood stain removal [England]
13708. Gold Plating Brass Pins for High-Temp Soldering [Texas]
13709. Autophoretic paint adhesion problems [England]
13710. Seeking Glassophor [Indiana] {3/28/02}
13711. Increasing corrosion resistance for 316 stainless steel. How? [Florida]
13712. Cleaning oxidized copper [India]
13713. How to clean antique brass fixtures epoxy finish [California]
13714. Seeking chroming of fishing lures [New Jersey] {3/28/02}
13715. Need black hardware that won't rust [Virginia]
13716. Running New Powder Coating Plant [Canada]
13717. Blackening process for Al metal? Methods to improve resin bonding with Al? [Arizona]
13718. Plasma nitriding procedure [Ireland]
13719. RE-POLISH ALUMINUM MOTORCYCLE FRAME [Texas]
13720. Coloring of silver [India]
13721. Scratched Chrome Rim [Pennsylvania]
13722. Finish coating for zinc electroplated products [Italy]
13723. Stains from baked on tape adhesive [New York]
13724. Patina for steel [Canada]
13725. Rocheltex [Alabama]
13726. Dissolved Oxygen+Residual Hydrazine [India]
13727. Light Color Antistatic Powder Coating [China]
13728. Hard anodising electrical insulation at sharp edge [Macau]
13729. Kolsterising yellowish discoloration spots on 316l [New Jersey]
13730. Small hole deburring/polishing [China]
13731. Black finish on bare steel [Canada]
13732. PARTS COME OUT FROM THE CHROME AT LCD MILKY (WHITE) [Michigan]
13733. Need help polishing aluminum wheels [Indiana]
13734. SULFUROUS ACID [Australia]
13735. Buffing mark problems in finished product anodized aluminum [Michigan]
13736. Anodizing to limit EMI/RFI Issues [Texas]
13737. Various Surface Finishes on Stainless Steel [Oregon]
13738. Plating question [Ohio]
13739. Seeking Plating Iron onto Aluminum [Texas] {3/29/02}
13740. Seeking titanium bags or foils for protection from oxidation [Ohio] {3/29/02}
13741. Seeking protection of aesthetic plastic components against scratch marks [India] {3/29/02}
13743. Mild Steel [Canada]
13744. Information on removing paint from brass needed [Florida]
13745. Standard Nickel Strike Composition [Greece]
13746. Hard chrome plating on cast iron [India]
13747. Alodine Precoating as Metal Finishing [Texas]
13748. Carbon and titanium oxide removal of extrusion components [Ohio]
13749. Need help polishing anodized surface [California]
13750. Sludge problem in phosphating [Pakistan]
13751. FDA approved coating for stainless steel cleaned with chlorine [Virginia]
13753. Recycling water [Malaysia]
13754. Copper washer identification [India]
13755. Pearlescent Automotive Paint and Coatings [North Carolina]
13756. Brazing / Soldering copper [New York]
13757. Finishing Problem [India]
13758. Seeking small plastic clip manufacturer [New York] {4/01/02}
13759. Investigate the metallurgical interface between zirconium and stainless steel 304 [UK]
13760. Faradays Law [South Africa]
13761. Repairing dents in aluminum [Georgia]
13762. DOES CHROMED ALUMINUM RUST [Illinois]
13763. Titanium Nitride Coating by nitriding titanium [Pakistan]
13764. Seeking to recycle the effluent [Malaysia] {4/01/02}
13765. Seeking automated plating plant [India] {4/01/02}
13766. Results on magnesium reacting with hydrochloric acid in the form of a graph [England]
13767. Seeking Trivalent plating processing [Massachusetts] {4/01/02}
13768. Restoring a copper tea set [Illinois]
13769. Seeking Alodine 1201 or equivalent [Hong Kong] {4/01/02}
13770. Seeking 1500A Pulse Rectifier [India] {4/02/02}
13771. Seeking 1-3-6 napthalene trisulphonic acid trisodium salt [Canada] {4/02/02}
13772. Health issue regarding domestic water heater [Portugal]
13773. Removing old plating and adding new (to pewter) [Georgia]
13774. Black Chromate [Indiana]
13775. Alodining Secondary Aluminum Alloys [North Carolina]
13776. How do you apply galvanneal [Massachusetts]
13777. Citric Acid vs. Nitric Acid Passivation for 440C steel? [California]
13779. Seeking stainless steel nails [Australia] {4/02/02}
13780. Etching solution for brass [Australia]
13781. How to make aluminum wheels shine [Canada]
13782. Filing an edge on a chromium plated ring [Washington]
13783. Surface texture of anodized aluminum [Missouri]
13784. How to polish inconel [Arizona]
13785. Electroless nickel [U.A.E.]
13786. Difficulty adhering paint to polyethylene surface [New Jersey]
13787. Powder coating scratch protection [Connecticut]
13788. Galvannealed vs. Zinc with Clear Chromate Conversion [Massachusetts]
13789. Effective hard anodize mask sought [England]
13790. Environmentally safe electrolytes [California]
13791. Seeking paint that looks like nickel plate [California] {4/03/02}
13792. Need info on bromate/free bromine waste treatment [California]
13793. Information about anodizing [Bahrain]
13794. Aluminiun sheet [Georgia]
13795. Plating w/out hazardous chemicals [New York]
13796. Mix Bleach with Guanidine Thiocyanate [California]
13797. Black Oxide/Chromic Dip [Arizona]
13798. Nickel strike bath [California]
13799. Seeking VERTICAL POWDER COATING LINE [Turkey] {4/03/02}
13800. Affordable paint to color rocks [New Jersey]
13801. POSICION ARANCELARIA [Colombia]
13802. Stripping copper [Oregon]
13803. Seeking salt spray testing of our galvanized material [Saudi Arabia] {4/04/02}
13804. School electroplating project (zinc onto a penny) [New Hampshire]
13805. Pulse hard chroming [UK]
13806. Deionized water vs. Distilled water in heat exchanger for Yag Lazer [Massachusetts]
13807. High Friction Material [Spain]
13808. Achieving class 3 chromate conversion coatings [UK]
13809. Anodising color loss and restoration [Australia]
13810. Requested study on the reaction between hot dip zinc and cadmium and wax plating [New Hampshire]
13811. Hexavalent Chrome. Why does it inhibit corrosion? [Ohio]
13812. Seeking kitchen cupboard wood doors powder coated [Michigan] {4/04/02}
13813. Gold coin patina restoration [Oregon]
13814. Creating a distressed mirror [Virginia]
13815. Copper sealer for counter tops [Texas]
13816. Getting a chrome like finish on exhaust pipes after being Jet-Hot coated [Pennsylvania]
13818. Identify s chromium plat eating utensils [Washington]
13819. Disposal of copper ion [Pennsylvania]
13820. Dye application on 302 stainless [Texas]
13821. Selectively conductive plating on plastics [Maryland]
13822. Al vs 316L Cathodes [Idaho]
13823. Aluminum casting burrs / flash / lamination [Indiana]
13824. Seeking sublimation surface coating [Ohio] {4/05/02}
13825. Rhodium removal from silver [Florida]
13826. Thin wall copper tube finishing [Illinois]
13827. Brass plating [India]
13828. Anodizing BeAl [Singapore]
13829. Yellow patches after passivation [India]
13830. Tumbling process [India]
13831. Seeking good polish for wheels and tanks [Kentucky] {4/05/02}
13832. Seeking Training to Iridite/Alodine Aluminum [Maryland] {4/05/02}
13833. Minimum solubility [Indonesia]
13834. Plastisol Primer/Undercoat [UK]
13835. Precipitation of wastewater [Indonesia]
13836. Embrittlement Sensitivity of Diffused Nickel Cadmium Coatings [Florida]
13837. Problems in electroforming [Argentina]
13838. Zinc content increase [Malaysia]
13839. Alodine or Anodize for corrosion protection of Al casting [Utah]
13840. Seeking Phosphoric Acid Anodize of Alum [Kansas] {4/05/02}
13841. Seeking Low Friction Plating [Canada] {4/05/02}
13842. Nickel finish over brass [New York]
13843. REQUEST FOR PROCESS INFORMATION [India]
13844. 40 cfr 433 passivation [Arizona]
13845. Re-passivation of coated stainless steel [Virginia]
13846. Need a durable weather resistant black finish for stainless steel [California]
13847. Problems with discoloration on nickel plating [Minnesota]
13848. Seeking color anodized tubing [Illinois] {4/05/02}
13849. Seeking polycrystalline cobalt plating [Pennsylvania] {4/05/02}
13850. Seeking line to manufacture nickel foil [India] {4/05/02}
13851. Seeking vacuum evaporator [Poland] {4/05/02}
13852. Seeking 1000 tons cresold urgently [China] {4/05/02}
13853. Pennies [Ohio]
13854. Needed: source for copper sheeting [Michigan]
13855. Stainless steel, scratch [Ohio]
13856. Surface smoothness measurement [Minnesota]
13857. Powdercoating MDF vs. vinyl vacuum wrap [Indiana]
13858. Silverplating [Alabama]
13859. Diamond additive [Oregon]
13860. Making up a chrome bath [Singapore]
13861. Haze film on Sterling Silver [Rhode Island]
13862. IRON CONTENT IN HCl PICKLING [India]
13863. Fastening torque changes due to surface treatment [India]
13864. Corrosion resistance of zinc on steel [UK]
13865. Reducing stress in plated Permalloy [California]
13866. Seeking Vacuum Metallizing Services [Canada or West Coast USA] {4/08/02}
13867. Seeking info and equipment for Ceramic and Powder Coating Process [Ohio] {4/08/02}
13868. End forming of needle [India]
13869. Help me with black oxidizing [USA]
13870. Calcium carbonate as an extender in paint production [Jamaica]
13871. Remover for dyes [Jordan]
13872. Scam of iridium copper coins [India]
13873. How do I get the shine back? [Virginia]
13874. Polished Aluminum [California]
13875. Galvanizing [Canada]
13876. Need heat resistant antique brass paint [Oklahoma]
13877. Fire Protection for Powder Coating Booths [Nebraska]
13878. Braze Furnace Maintenance [Kentucky]
13879. Tie-coat: paint to polypropylene [Florida]
13880. Suitability of mechanical zinc with sems screws [Ohio]
13881. Cathode Plate Thickness in Dummy Plating [Algeria]
13882. Finishing operation in manufacturing circular punches [Wisconsin]
13883. Science Fair - "The Truth About Toothpaste"
13884. Stainless steel refinishing [Tennessee]
13885. Need help with offline tin dissolution unit for MSA wire tinning [Massachusetts]
13886. Brass cleaning of antiques [England]
13887. Seeking PTFE (Teflon) coating of aluminum strips and roll-forming into round bushings [Virginia] {4/09/02}
13888. Seeking materials for refinishing bathtubs [UK] {4/09/02}
13889. Seeking 120MT/mo. of Boric Acid [Russia] {4/09/02}
13890. Seeking electrode for old salt water chlorinator [South Africa] {4/09/02}
13891. Stained tub [Illinois]
13892. Waste water treatment [Malaysia]
13893. A suggestion for removing gold from chrome [Canada]
13894. How do I finish my metal brushing exercises [California]
13895. Diffusion Dialysis Membranes [Australia]
13896. Masking problems [India]
13897. Passivation for 420SS [Minnesota]
13898. Seeking decorative black chrome [Maryland] {4/09/02}
13899. Seeking chrome plating [Arkansas] {4/09/02}
13900. Seeking BLUED TITANIUM [Iowa] {4/09/02}
13901. Coal combustion [India]
13902. 304 at High Temperatures [South Carolina]
13903. Electroplate Silver [North Dakota]
13904. Stainless steel more corrosive in the sea water than steel [Saudi Arabia]
13905. Home electroplating [Australia]
13907. Help for Antique Car [West Virginia]
13908. Status of QQ-P-35 [Connecticut]
13909. Salt spray correlation [Connecticut]
13910. Copper finishing - natural [Bahamas]
13911. Color of Brushplating on Hardchrome [Austria]
13912. Black dye = redish tint? [Washington]
13913. Plastic part plating research [Utah]
13914. Seeking Electroless-Nickel Plating Kits [England] {4/10/02}
13915. Salt air corrosion of hot dipped galvanized steel [Australia]
13916. Require assistance on nickel plating process [Mexico]
13917. Aluminium plating on brass [India]
13918. Seeking brass bed refinishing [California] {4/10/02}
13919. Rust spots on SS316L weld joints [Texas]
13920. Bonding of ciric acid on copper [Belgium]
13921. How do I clean copper without the red after tone? [Georgia]
13922. Browning solutions [California]
13923. Flaking of Powdered Metal Sintered Coating [Ohio]
13924. PVD color standard [Kentucky]
13925. SEEKING BLACK OXIDE COATING FOR WIRE MESH [California] {4/10/02}
13926. WHAT HAPPENED TO MY PARTS [California]
13927. Chroming morotrcycle wheels [Canada]
13928. Removing golf club rust [Kansas]
13929. Zinc plating compatibility with Ethylene Oxide [California]
13931. Seeking protective coatings for stainless steel [India] {4/10/02}
13932. Seeking Copper Coated Co2 Welding Wire [India] {4/10/02}
13933. Reflective Use of UV Light [Alaska]
13934. How do I clean tarnished brass? [Minnesota]
13935. Black oxide rubbing off [Texas]
13936. Filling etched steel, zinc with paint [Massachusetts]
13937. F.D.A. approval of sulphuric anodising [England]
13938. Tight fits, aluminum, anodize and galling [Massachusetts]
13939. Surface Decarburisation of Stainless Steels [Nigeria]
13940. Paint based tape [Florida]
13941. Seeking Quality EN Plating [Idaho] {4/11/02}
13942. Seeking sulfur dioxide candle for Kesternich test [Brazil] {4/11/02}
13943. Seeking Buffing Compound or Polish for SS [Texas] {4/11/02}
13944. Porcelain tub stain [Louisiana]
13945. Hard coat coil problem [Maryland]
13946. ALGAE CONTAMINATION IN DI-WATER [California]
13947. Seeking salt spray cabinet [Canada] {4/11/02}
13948. Surface treatment for fishhooks [England]
13949. Which metals corrode fastest [Australia]
13951. Seeking truck buffed [Massachusetts] {4/11/02}
13952. Removing Phenol [Singapore]
13953. Maintaining copper shine [Canada]
13954. Vacuum coating system and methods [Lithuania]
13955. Simple plating cell for a science fair project [Arizona]
13956. Dechroming of honing slurry [India]
13957. Seeking Nickel Diamond Plating Process [India] {4/11/02}
13958. Mirror Polish / Nitride Coating for Titanium Bicycle Frames [Ohio]
13959. Aluminum under water [Minnesota]
13960. Cast Iron Finish Treatment Required [Canada]
13961. Strength and life of a powder coated part [India]
13962. Seeking vacuum impregnating [Washington] {4/12/02}
13963. Seeking Mu-Metal [California] {4/12/02}
13964. Protection from chrome [Canada]
13965. Zinc plating nightmare [Canada]
13966. Stainless Steel - 316 vs. 317 [New York]
13967. METGUARD WDS-11 Specification [Australia]
13968. Seeking supplier of sheet zinc [Washington] {4/12/02}
13969. Aluminium 3003, H14 and CP118: 1969 N8 [Hong Kong]
13970. Anodize iron [Kentucky]
13971. Seeking rims dipped [New York] {4/12/02}
13972. Bright dip school project safe at home (new product?) [New York]
13973. Coating of conducting plastic with TiN in vacuum microwave plasma [The Netherlands]
13974. Anodizing Aluminum [Mexico]
13975. Seeking bumper re-chromed [Maryland] {4/12/02}
13976. Request for information on Chromium Plating Specifications [Texas]
13977. Refinishing wrought iron and brass crib [Minnesota]
13978. Plating for 250 hours salt spray [Ohio]
13979. Specifying Pickling Solutions/Procedure [Minnesota]
13980. Seeking bronzing supplies [Panama] {4/16/02}
13981. Powder Coating on Wood [Iran]
13982. Electroless nickel thermal conductivity [Georgia]
13983. Zinc phosphate specification for powder metal [Texas]
13984. Bonding to anodized finish [California]
13985. Seeking chrome phosphate treatment of aluminum sheet [Ohio] {4/15/02}
13986. Can you plate white gold/platinum over yellow gold? [UK]
13987. Scratch on stainless [California]
13988. Tantalum etch [Texas]
13989. Chromium hexavalent [Brazil]
13990. Seeking chemicals for ELECTROLESS METAL [Egypt] {4/15/02}
13991. Can't reproduce a "marblous" mistake - marbled zinc chromate effect [Ohio]
13992. Seeking nichrome heat resistant wire [New York] {4/15/02}
13993. Painting metal cabinets/cupboards [South Dakota]
13994. Coloring aluminum [Pakistan]
13995. CHROME PLATING WHEELS [Canada]
13997. Cross Reference for ASTM Electroplating Specifications [Arizona]
13998. Electroless Nickel Coating Heat Treatment [Hong Kong]
13999. Preserving colors on copper [Washington]

The finishing.com Hotline includes more than 50,000 RFQs and shop problems about metal finishing. This page is an archive of a thousand of those discussions. Rather than review this page, you may prefer to start at our home page, view the most recent letters, or search the site.


© finishing.com, inc., 1995-2009