HELLO, I'M LOOKING FOR BOOKS OR SOFTWARE ASSOCIATED WITH ANODIZING. WE ARE AN INVESTMENT CASTING TOOL & DIE MAKING CO.,LOOKING TO "IN HOUSE" ANODIZE SOME OF THE COMPONENTS OF OUR TOOLS.

DOES ANYONE KNOW THE WHEREABOUTS OF A GOOD BOOK ON THIS SUBJECT? I HAVE BEEN TO ALL THE LOCAL BOOKSTORES AND HAVE HAD NO LUCK IN FINDING ANYTHING !

THANKS SO MUCH FOR YOUR ASSISTANCE.

PHILIP MORGAN
MOLDING CO. - VALENCIA CA.


(1998)

I think the most complete information available on Anodizing is The Surface Treatment and Finishing of Aluminum and Its Alloys by S. Wernick, R. Pinner, P.G. Sheasby. Two volume set. It is a little pricey ( a couple hundred bucks), but is the most comprehensive of all of the literature I have seen. It also includes many references which are readily available.

Ward Barcafer, CEF
aerospace - Wichita, Kansas


(1998)

That is a great reference. A much cheaper one to get started with is Light Metals Finishing by David Montgomery and is sold by AESF. I think that you can link to them from this site, or at least get an address.

James Watts
- Navarre, Florida


(1998)

A very good book is "The Technology of Anodizing Aluminum" [link is to info at Amazon about the book], A.W. Brace P.G. Sheasby, Technicopy Limited, 66 High Street, Stonehouse,GL10 2NA, England

Raymond Hendrix Troy, Tennessee



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.