Copper-nickel plated iron rusts anyway





copper plate it then nickel plate it but still there are problems of rusting. what is the solution for that

Tarun Bansal
manager - Delhi, India
September 19, 2009



September , 2009

Hi, Tarun.

1. Get the tech service person from the vendor in, or

2. Retain a consultant, or

3. Get a copy of Durney's "Trouble in Your Tank?" and be prepared to invest several weeks in troubleshooting.

I'm sorry but such problems are quite difficult and simply cannot be solved with a quick and easy reply to a 20-word internet posting. Best of luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.



With no more information than you gave, here is a short answer. You have not put enough of one or both of the platings on the parts. 27 words

Jim Watts
- FL
September 21, 2009


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"