Techniques/recipes for coloring metal


(2000)

hello,i am getting started in decorative metal designs and am looking for techniques/recipes for coloring metal.both ferrous and non-ferrous,mainly steel and copper.personal experience or reference to literature would be greatly appreciated. thank you

matthew a azevedo
- minden,neveda


(2000)

Regarding coloring of copper, we have a FAQ on patinization. For coloring of steel, there is a chapter in the Metal Finishing Guidebook. Good luck! Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.