topic 4023

E-coating service for stampings and car parts & bodies


RFQ: I'm looking for a shop that can e-prime a car body. I'm restoring a 1970 Chevelle and had it stripped. Thanks,

Brook C [last name deleted for privacy by Editor]
- Farmington Hills, Michigan

Electrocoating: a Guidebook for Finishers
from Abe Books



What technology was used for the stripping, Brook -- media blasting, rather than immersion?

I don't know of any aftermarket e-coating shops myself; it's probably expensive to rig the lines for individual cars of varying dimensions. I think you may end up having to do a different kind of priming, but maybe you can find a lead in "Hemmings Motor News" [link is to product info at Amazon]. Good luck.

Ted Mooney, Teds signature
Ted Mooney, P.E.
Pine Beach, New Jersey

August 7, 2009

RFQ: I am in the process of searching for an e-coating service capable of doing an entire car body as well, but locally to me.

A. There is one that I am aware of that could be close enough to make it worthwhile to do your Chevelle, but that's up to you. Here's a link to a Charger being restored:

The company that dipped this car is Restoration Specialties in Milwaukee, WI. I have never used them, nor contacted them, but you might want to try.

Bob D [last name deleted for privacy by Editor]
- Newburgh, New York, USA


RFQ: Have a large government contract for coil springs that require e-coating and CARC coating. Need to find a vendor that can supply both coatings in one facility. CARC would require liquid dip not spray. Contract is for 15 months with more to come.

RICHARD B [last name deleted for privacy by Editor]

July 30, 2009

RFQ: I'm looking for an E-Coat Supplier located on the West Coast. The body is white with high strength steel. The size is small, approx. 5 ft to 8 feet long. This is a very small sampling of what we will need to have done for next months' requirements. We work within the entertainment industry and will have a wide variety of needs located close to our customer.

Rochelle Y [last name deleted for privacy by Editor]
entertainment, auto. aftermarket, NASCAR, Medical - Livonia, Michigan

September 2, 2009

RFQ: Need a 'job shop' type service that can e-coat classic car parts. Parts range in size from hoods, fenders, doors, and trunk whole auto bodies (disassembled of course). Prefer a service company that also does the pre-cleaning before e-coating (dip/strip or oven bake-off) to bring parts to bare metal first. Right now I use two separate companies to do the stripping/cleaning and e-coating.


Mike M [last name deleted for privacy by Editor]
hobbyist - Hazleton, Pennsylvania, USA

April 10, 2011

RFQ: Hi, I am an industrialist manufacturing sheet metal stampings located in India.
I have a few components which require e-coat & as such I am looking for suppliers who can provide these services.


Mahesh I [last name deleted for privacy by Editor]
buyer - Belgaum, Karnataka, India

October 22, 2012

RFQ: Hello.

I've noticed that the companies that do this e-coating are all back east. One would think that as many cars here in So. Calif., there would be several companies out west offering this service to people who would like this process applied to their car. Can anyone post some names of companies here in Orange County if any or even So. Calif. would work?

Thanks, Joe

Joe Reese
- Anaheim, California U.S.A.

Ed. note: Names and locations only, please, readers. Allowing testimonials attracts salespeople who can't resist using fictitious names and posting as super-satisfied customers :-)
We can't do police background checks to tell who is real and who is phony, so we don't print testimonials.

This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site


Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices

©1995-2018, Inc., Pine Beach, NJ   -   About   -  Privacy Policy
How Google uses data when you visit this site.