"Blistering on Copper Plating of Bronze Baby Shoe Process"



2005

Hi there,

I electroplate baby shoes and have a very new problem to me in that I have had some severe blistering occurring on my last few pairs of shoes.

Has this happened to anyone else? I can't think why this would suddenly happen.

Any ideas at all?

Vicki Rowe
Bronze Keepsakes - Wellington, New Zealand
^


2005

I would think that blistering would be the most common problem in bronzing non-metallic objects like baby shoes. I believe that you should look at your metallizing step very carefully, After that, make sure that you start the current very slowing when building up metal.

tom pullizzi animated    tomPullizziSignature
Tom Pullizzi
Falls Township, Pennsylvania
^

none
finishing.com is made possible by ...
this text gets replaced with bannerText
spacer gets replaced with bannerImages

Q, A, or Comment on THIS thread SEARCH for Threads about ... My Topic Not Found: Start NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

 
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g, Train'g
& Software


About/Contact    -    Privacy Policy    -    ©1995-2021 finishing.com, Pine Beach, New Jersey, USA