Cor-ten steel tube





I'm a steel sculptor working on outdoor pieces. I'm trying to get hold of some Cor-ten steel in tube form, as it forms a protective layer of rust and does not corrode completely, even after years of being outside. Does anyone know where I can get this from?

Rachel Merrington
- Cambridge, England
2003

Ed. note: This RFQ is outdated, but technical replies are welcome, and readers are encouraged to post their own RFQs. But no public commercial suggestions please ( huh? why?).

Ed. note: this forum is for technical postings and is made possible by supporting advertisers; they will respond in private to sourcing issues.


Cor-Ten was made by British Steel before they became known as Corus. Try a steel stockholder as a source.

trevor crichton
Trevor Crichton
R&D practical scientist
Chesham, Bucks, UK
2003


What is the composition cor-ten a?

LLUMIQUINGA MARCO
- ECUADOR
2005



Along with above satisfied answer I also want exact details for chemical composition of Cor 10 steel.
Please mail the details.

Amit Shelar
- Pune, India
April 17, 2009



April , 2009

Hi, Amit. Cor 10 is a proprietary, not a standards-based composition, so the only source for that info is the manufacturer.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"