Home of the finishing HOTLINE since 1989

-----

Novice trying to polish bike frame




Could someone please advise me on what tools and polishes are best to strip the paint and polish an aluminum motorcycle frame for someone who has never done it or seen it done before.

John Jackson
- Fayetteville, North Carolina
2003


Go to uponone.com. It's a sight sponsored by starboyz. Go to the how to section and there is a how to polish your frame area. I just got done doing it and it turned out awesome. It took me about 24 hours all together to do the frame, swingarm, and underneath my seat. Good luck.

Jim
- Moon, Pennsylvania
2004



August 29, 2008

Hi, John. letters 800, 1831, and 10917 go into substantial detail about aluminum polishing. Good luck!

Thanks, Jim. Full name next time, please.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"