-----How to polish a motorcyle frame?
I have a few questions on how to polish my motorcycycle frame? My question was that can I use Aircraft Stripper on my frame to take off the paint without messing up my frame and then go over it with sandpaper?
Marcus E.- Dallas, Texas, US
2003
Hi, Marcus. You can use the aircraft paint remover because that's what it's made for. If it's methylene chloride it is very aggressive on paint and not harmful to aluminum, but very harmful to people -- so read the instructions carefully about good ventilation,
goggles
⇦ on
eBay or
Amazon [affil link] and
rubber gloves
⇦ on
eBay or
Amazon [affil link] ; don't blow them off. We have many letters about motorcycle polishing on line here; please start with letter 800 or use the search engine rather than starting in on the sanding. Good luck!
Regards,

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
June 8, 2008
Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.