ELECTROLESS NICKEL (EN) COATINGS for Oil & Gas Industry


A discussion started in 1995 and continuing through 2002.
Add your Q. or A. to restore it to the "Current Topics" discussions.

(1995)

Q. Hi,
Please, We would like to know about the updated ELECTROLESS NICKEL COATINGS and its applications repairing equipment' surfaces in the oil and gas industry. We will appreciate your help. Regards.

Dany Di Fazio V. Corpoven, s.a.
PETROLEOS DE VENEZUELA (PDVSA) - Venezuela


Electroless Copper and Nickel-Phosphorous Plating
from Abe Books

or


Electroless Plating
Mallory & Hajdu
from Abe Books

or

(1999)

A. Hi, Dany. Thanks for visiting. References you might consider are:

Chemical (Electroless) Nickel Plating by G.G. Gawrilov or Electroless Plating: Fundamentals & Applications by Mallory and Hajdu

You may wish to contact suppliers of electroless nickel solutions, such as:

--or manufacturers of brush plating systems, such as:

Good luck.

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E.
finishing.com
Pine Beach, New Jersey


(2002)

A. Electroless nickel is a coating designed to protect metallic parts of any shape against corrosion-erosion in oil industry applications, for example, in choke boxes, control valves, spools, pumps, pipes, and others where corrosion and erosion resistance are required to reduce operational cost and extend lifetime of components mentioned above.

José Wong
- Caracas, Venezuela



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.