Blackening of Steel




Sir,
I am interested in doing black passivation color on hardened steel parts, kindly advise.

Kapil Gupta
- Ludhiana, Punjab, India
2001



June , 2008

Hi, Kapil. You can't passivate steel like you passivate stainless steel. But it would be possible to black oxide coat the steel parts. See our FAQ: Black Oxide & Cold Blackening for a quick intro.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.


 

Sir,

I need the procedure for blackening process of steel.

Nagesh HR
- Bangalore



 

Buy it from EPI / Electrochemical Products Inc. [a finishing.com supporting advertiser] or Heatbath and follow the directions?

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"