Electroless Deposits on Aluminum




I would like to have any information about electroless nickel deposit on aluminium alloys especially on 7075-T6. If you have information about this kind of deposit on aluminium alloy I'll be pleased.

Been writing,

Aramaris Prieto Urbina
- Caracas, D.F. Venezuela
2001



July 1, 2008

Hi, Aramaris. After cleaning, etching and desmutting the aluminum, and before electroless nickel plating it you must zincate it. Have you made it that far in your planning?

Robert Probert's "Aluminum How-to" or Mallory & Hajdu's "Electroless Plating" [on eBay , Amazon, or AbeBooks affil links] will give you a detailed process cycle. Good luck.

Please get back to us if this did not answer your question sufficiently. Thanks!

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"