Bismuth plating bath


2001

Is there any information on formulations for a bismuth bath?

Gilbert Alfaro
- Houston, Texas ,USA


2001

Lowenheim's book called Electroplating has a formula for bismuth plating which uses perchloric acid, so it may be an effort to use it safely.

pooky tom pullizi signature
Tom Pullizzi
Falls Township, Pennsylvania



If you have a question in mind which seems off topic, please Search the Site

ADD a Comment to THIS thread START a NEW threadView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.