-----Testing on cad
Is anyone familiar with the copper sulphate
⇦ on
eBay or
Amazon [affil link] testing for corrosion on cad plated parts and how well it works? I am interested in getting rid of the salt spray testing. (Sounds like a lot of you are interested in this.)
Thanks,
- Tucson, Arizona
2001
Are you sure that wasn't CASS, copper accelerated Salt Spray testing, which uses copper sulphate?
Or is the copper sulphate used as a paste? If it is an accelerated test, it may be no better than salt spray.