I left my yellow gold in cleaner and it turned white?




I forgot my yellow gold ear rings , necklace and coin charm in cleaner and they turned white I have worn these items for over 10 years and they have never worn or turned anyway I am sure they are gold not plate is there anyway to reverse fix them they have a lot of sentimental value

Shelly Ben
owner - Clayton, Oklahoma, USA
February 3, 2011



Hi, Shelly

This staining is probably very superficial and easily polished away by a jeweler. Good luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
February 4, 2011


if in yr cleaner there is mercury or some other chemicals which can change yr ring yellow colour to white. you simply polish it. you will regain yellow colour.

Bhupesh Mulik
- Mumbai, India
February 16, 2011


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"