-----Looking for best light cleaner of electroless nickel pistols
How to clean an electroless nickel pistol?
gunsmith - St. Louis, Missouri
December 30, 2010
Old formula 2% H2SO4 in ethyl alcohol (immersion max. 10 seconds), instead of that you can use next formula too: 47,5 gms citric acid ⇦ on eBay or Amazon [affil link] /47,5 gms sodium gluconate/4,9 gms tartaric acid ⇦ on eBay or Amazon [affil link] /1 lit water - can be used cold or hot (80 C). Hope it helps and good luck!
Goram Budija- Zagreb, Croatia
January 4, 2011