-----Random Brown Stains on Decorative Chrome
We have a problem in our commercial Chrome division with a random brown stain appearing on finished product. Full chemical testing has been done by our suppliers and they say it is to standard compliancy. In the process we can achieve brilliant success in production but in the next production the spots will appear as if a gremlin is in the tank. Can anyone out there give us an idea where to look for a solution?
Wade HarrisWorkshop owner and CEO - Lower Hutt, New Zealand
October 18, 2009
My guess is that the gremlin is in your preplate steps as in blush rust or fingerprints or similar.
James Watts- Navarre, Florida
October 19, 2009
Hello,
on which substrate is the chrome deposited and could you provide further information's please (Composition of the chrome solution, catalysts in use, pre-treatment, working parameters of the chrome solution).
Thank you and with Best regards,
- Sydney, Australia