Home of the finishing HOTLINE since 1989

-----

How to electroplate nickel aluminum alloy




August 2, 2009

how I can electroplating with nickel aluminium alloy .
what I must adding to watts bath or what bath I can used
please help me .

Mohamed Mohamed
master student - Aleppo, Syria



Hi, Mohamed. Aluminum cannot be plated out of an aqueous bath, and I doubt that it is possible to plate a nickel-aluminum alloy either. You could perhaps occlude some fines of aluminum into your nickel plating though.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
August 3, 2009


NiAl has been co-deposited from Ionic Liquids by a number of different authors although its not an industrial process. Look up W.R.Pitner for his work on [EMIM]AlCl3-

Mark Craig
- Cranfield, UK
September 9, 2009


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"