Reticulated Cathodes for Electrowinning





I am interested in testing the possibility of using reticulated cathodes to reduce the metal content in effluents down to the 2-4 ppm level. Do you know of any suppliers of reticulated cathodes.

Al Taweel
Dalhousie University - Halifax, Nova Scotia Canada
2000



1 of 2 simultaneous responses

USFilters is suppling the RETEC equipment that has the reticulated cathodes for EW.

sara michaeli
sara michaeli signature
Sara Michaeli
Tel-Aviv-Yafo, Israel
2000




2 of 2 simultaneous responses

U.S. Filter acquired RETEC, a primary developer of reticulated electrodes. Be sure to call the right office to get more information. U.S. Filter is so big the right hand never knows what the left hand is selling. Try the Billerica, Massachusetts office. If that is a dead end, let me know. I used to work for them and have an extensive phone list.

bill vins
Bill Vins
microwave & cable assemblies - Mesa (what a place-a), Arizona
2000



Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"