Need info about Copper Electroforming & EDM electrodes


.

Dear sirs,

As a Student of Manufacture Engineering in University of Tabriz of Iran,I am very interested in research activities.

I have been working on Copper and Nickel Electroforming and in particular on the first one for about 2 years,and I have obtained some results in solutions and additives.As there are few references in Iran in this field,I would be so thankful,if you could send me some information about Copper Electroforming and properties of EDM electrodes.

I will inform you of the results of my researches.

I am waiting to receiving from you.

Your faithfully,

Abbas Pak, Dept. of Manufacturing,
Tabriz University, Tabriz, IRAN


(2002)

Dear Sir,

We are plastic injection molding producers from Turkey and we required always copper electroforming EDM electrode. We required detailed information of this job.I would be so thankful,if you could send me some information about Copper Electroforming and properties of EDM electrodes. I am waiting to receiving from you.

Best Regards,

Ferit Cicek
ARGE LTD. STI. - Ankara, TURKEY



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.