History of anodising


(2000)

I am currently completing my M.A. My subject is the detailed multi-colouring of anodised aluminium. My research has been directed towards metal artists, not commercial production.

I have achieved successful results, applying up to twenty colours in an illustration. I am searching for information regarding the history of anodising aliminium, can anyone help?

J.Walsh
- Australia


(2000)

Dear Mr. Walsh, Have just read your request for any info on the history of anodising. My only suggestion is to contact the Technical Section at Alcoa Refinery, Geelong, Victoria. In the past they have been very helpful in providing material on any topic concerning aluminium.

Mc Ilvena Patrick. W.
Mac Dermid Australia - Melbourne, Victoria, Australia



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.