5541E, alternate specification to and electrode potential


(2000)

Is there a commercial equivalent to MIL-STD-5541E, class 3? Does anyone know the standard electrode potential of a 5541E, Class 3 coating?

Steve Kutner
- Santa Clara, California, USA


(2000)

Hello Steve, you should obtain a copy of specification no. ASTM B449-93 [link by ed. to spec at TechStreet], "Standard Specification for Chromates on Aluminum".

Keith B. Olasin
- Whippany, New Jersey, USA



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.