Dacrotising or Substitute needed.


(2000)

Hello,

Would anyone be able to help us in locating a source for Dacrotising Chemicals and also answer these three queries ?

1. Does Zinc-Iron plating prove better than Dacrotising as regards to wear resistance , corrosion resistance, overall performance ?

2. Can Dacrotising be accomplished with simpler machinery such as a Centrifugal Spin Dryer and baking oven, or is installation of a sophisticated Dacrotising plant a must ?

3. Has anyone substituted Dacrotising with any conventional process with good results ?

Your help as always is much appreciated.

Thanks in advance

Khozem Vahaanwala
Khozem Vahaanwala
Saify Ind supporting advertiser
Bangalore, Karnataka, India

saify logo


(2000)

Hello, Mr. Vahanwala:

Dacrotizing is a trademark owned by Metal Coatings International Inc [Chardon, OH] referring to the application of their Dacromet coatings.

It is not a generic process, so we would like to see discretion used in any feedback. We do not want to see anyone slam a given brand name on the one hand, but we also don't want to encourage on these pages the verbose and flowery praise we often see from a manufacturer or a licensee when his/her brand name is mentionedsmiley

So I would ask our readers to try to keep their responses scientific.

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey


(2000)

Dear Khozema,

For specific answers to your questions I would direct you to contact either Andrew Pfiefer, or Nippon Dacro Shamrock Co. Ltd. NDS covers the India market.

David J. Wolf David J. Wolf
Medina, Ohio



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.