We are in the business of aluminium anodizing since last 15 years and have been carrying out normal, two-stage electrocolor and hard anodizing. We would like to know how to go about "anodizing using AC superimposed on DC" as this method claims to use lesser energy while producing hard coating. We would also like to know more about PTFE sealing.

Dilip Kumar Patel
Yogi Industries - VithalUdyognagar, Gujarat, INDIA



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.