Can iron be chromated?


(2000)

I study chemical engineering and I'd like to know about chromate conversion coating?

Could someone tell me if it can be used on iron? In literature has been said that it is commonly used on Al, Zn, Cu, Cd etc. How about Fe?

Marianna
- Finland


(2000)

Nope, iron cannot be chromated.

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E.
finishing.com
Pine Beach, New Jersey


(2000)

Thank you!

Is there a simple reason why iron cannot be chromated? What is the big difference between iron and other metals (that can be chromated)? Is it the reaction between metals and chromating solution or what? How is iron different?

Marianna
- Finland


(2000)

It's simply that iron does not react with dilute chromic acid and/or it does not generate useful reaction products. Iron phosphate or zinc phosphate are the usual conversion chemicals for iron materials because they do form useful reaction products. The chemistry of both chromate conversion products and phosphate conversion products are highly complex with numerous reactions products formed.

Ted Mooney, finishing.com
Teds signature
Ted Mooney, P.E.
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.