Looking for satin copper plating process


(2000)

dear sir,

we are a plating company that deals with acid copper plating of polyester figurines,we need a satin or brushed finish on some of our goods.I don't want to get involved with satin nickel because of it's relatively high operating temperature that sometimes causes puffs and blisters on plastics. Do you have any suggestions or guides to any suppliers of additives and brighteners for a satin copper bath that can be used in room temp.

best regards

G.Erhan Erel
Istanbul/Turkey


(2002)

Dear Sir or Madam,

I am doing my science fair project on copper plating using electrolysis and I was wondering if you would tell me exactly how you copper plate a metal?

Sincerely yours,

James Gardner
- Springhill, Louisiana


(2002)

Try the term "copper plating science project" in the search engine near the top of this page.

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.