-----How to remove surface defects from type 409 Stainless Steel?
2007
Dear sir,
We have a problem where we have ss 409 and ss 304 stretched operated metal, but it has patches somewhere yellowish and bright colour it not looks non-aesthetic -- so what to do? If I want pickling, then how to do?.
Thanking you,
filtration - Jaipur , Rajsathan , India
I'm not sure ,but you could try this:
cathode-electrolyzing with low current in hexavalent chrome bath.
Seagull - Guangzhou, China