Want info about about nickel color plating




2006

I'm looking for (material) for nickel color plating.

and the (material) bronze plating on the brass.

( GREEN ON BRASS) color.

I'm making test:

sodium thiosulphate on eBay or Amazon [affil link] 40 g/li

nickel sulphate 100 g/li

warm 60 °C to 70 °C

But I didn't get any result.

please help me

best regards,

Mazen Bakdones
electroplating - Damascus, Syria



Try uspto.gov webpages there you can find some infos on that subject(download free full text patents database). Old Fishlock's book on metal colouring is very good starting point too. Good luck!

Goran Budija
- Cerovski vrh Croatia
2006



2006

Dear Mr Mazen
hope keeping fine .

composition you mentioned is for black nickel. for bronze plating you have to take solutions from suppliers yellow or white and last but not least for patina on brass you will get many formulations but only gateway to it is metal colouring books which you can search from finishing.com (books).

regards and best of luck from your friend

Qutub Saify
- Ajman, UAE


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"