Nickel Deposition by Simple Boiling


(2000)

About 25 years ago I was using a formula for nikel deposition by simple boiling. I think it was based on nikel sulphate. Unfortunately this formula has been lost. Can anybody help me with this problem

J. K. Ibbott



(2000)

Dear Mr JK Ibbot, Sounds like Electroless Nickel plating which uses sodium Hypophosphite as a reducer. Contact any supplier of proprietary EN Chemicals or read Wolfgang Reidel's "Electroless Nickel Plating" [link is to info about book on Amazon].

Khozem Vahaanwala
Khozem Vahaanwala
Saify Ind supporting advertiser
Bangalore, Karnataka, India

saify logo



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.