topic 4042

How to black dye aluminum castings.


(1999)

How should an aluminum die casting be anodized in order to dye it black.

I've heard of a pretreatment using hydrofluoric acid with something else that will remove part of the silicon in the surface so you can get a clear coat that can be dyed. Does anyone knows how this works?

Guillermo Luna
- Mexico City, Mexico


March 1, 2009

Hi, Guillermo. Aluminum diecastings can be anodized and dyed black, but the purer the aluminum the better it can be anodized. Silicon and copper cannot be anodized, so the part is desmutted in an acid that can dissolve these before it is anodized.

Yes, a mix of nitric and hydrofluoric acid can probably successfully desmut die castings, but greater consistency and safety can be achieved by using a proprietary acid salt than raw chemicals. Good luck.

Regards,

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.