Leadframe solder plating cost?


(1999)

I'm looking at the costs of plating the leads for molded plastic electronic packages. Would anyone be willing to share what the cost is (cost to you if you do it yourself or the price you pay if you have it done) to have lead/tin solder plated onto assembled packages. I'm interested in PQFP packages and TSOP packages, both at production volumes.

Robin M.
- Canada


(2003)

We have done cost analysis of this step for several different components. Our estimate for this process is approximately 8 cents per package.

Ted Hannibal
- Waltham Massachusetts



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.