About cleaning section of anodizing aluminum





My problem is that what kind of deruster can be used when anodizing aluminum 6061 or some other alloys of aluminum, and can we use "Chemapix-ACM" as a deruster for our aluminum material. Thank you very very much.

Mehmet Yilmaz
Almet- Coating - Turkiye
2006



We don't like to recommend one brand of proprietary products over another on this forum, Mehmet, but the supplier should be telling you whether the product is appropriate for desmutting aluminum. There are suppliers specializing in the plating and anodizing field in Turkey and the neighboring countries.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2006



Anything termed a "deruster" is probably not intended for use on aluminum as aluminum doesn't "rust" - a term usually reserved for steel! I tried to find "Chematrix" on the internet but drew a Google-blank!

milt stevenson jr.
Milt Stevenson, Jr.
Plating shop technical manager - Syracuse, New York
2006


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"