Electropolishing



2006

Does Electropolish can enhance the surface finish of SS 316L ?

That is, is it decreasing the Ra value of the surface ?

Keshav Gokhale
Pharmalab - Ahmedabad, Gujarat, India



Yes, Keshav. But no more abstract questions, please. Instead, start by describing your situation. Thanks.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2006


WE ARE USING ELECTROPOLISHING FOR SS PART AS A CLEANING /SURFACE TREATMENT & IT IS GIVING GOOD RESULT.

THOTE SHESHRAO
- AURANGABAD, India
2006


YES ELECTROPOLISHING IMPROVES ENHANCE FINISHING & RA VALUE IF PROPER CURRENT,TIME & CHEMICALS USED

SHESHRAO THOTE
- AURANGABAD, India
2006


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"