Removal of carbonates in cadmium plating solution


(1999)

We have high carbonates in our cyanide cadmium plating solution. For high carbonates in copper cyanide plating solution, the Metal Finishing Guidebook suggests precipitating them with lime (calcium hydroxide). Is this possible in a cadmium solution also, or do we have to freeze them out. If we do have to freeze them out, is dry ice a good method or will the carbon dioxide cause any problems.

Guy Lester
- Ontario, California


(1999)

Hi Guy. If you use NaCn you can freeze them out.

anders sundman
Anders Sundman
3rd Generation in Plating
Consultant - Arvika, Sweden



(2000)

Dear Guy,

To freeze out carbonates in cyanide -cadmium electrolyte is best method, but dry ice not suitable for that,because it can increase the amount of carbonates in electrolyte.

Best regards,Nina

N.Sezin
- Haifa,Israel



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.