Want brass sealer for king-size brass bed

Some clearcoating solutions (adv.)    g j nikolas banner   everbrite banner  

(1999)

I have a king-size brass bed that I'm constantly polishing to keep my wife happy. Do you know of a reliable brass sealer that will not harm the bed's finish. The sealer needs to be durable as well because I move a lot.

Thanks, Bill

Bill Bigelow
- Washington DC


(1999)

Bill,

There are lacquers made specifically for brass, by such companies as G.J. Nikolas [Bellwood, IL]. Good luck.

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E.
finishing.com
Pine Beach, New Jersey


(1999)

I have the exactly opposite problem. Does anyone know how to remove this lacquer without damaging the brass finish?

Mandar Sunthankar
- Fort Collins, Colorado


Hi, Mandar. If it's actual brass lacquer, it is easily removed with lacquer thinner [linked by editor to product info at Amazon] or Acetone [linked by editor to product info at Amazon]. Good luck.

Regards,

Ted Mooney, finishing.com
Teds signature
Ted Mooney, P.E.
finishing.com
Pine Beach, New Jersey


July 5, 2008

We had a hard finish on our brass headboard which was hard to remove so we soaked the pieces of the bed in radiator cleaner at our local radiator shop. The brass came out discolored but when we polished the pieces, they are beautiful. Now we just have to find out what to seal the pieces with. We are thinking maybe clearcoat as it is harder than lacquer.

Lynne Maitland
- Watertown, New York


July 7, 2008

Hi, Lynne. You may be interested in listening to our podcast interview with Teresa Sedmak, pres. of Everbrite Coatings, about this.

Regards,

Ted Mooney, finishing.com
Teds signature
Ted Mooney, P.E.
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site


Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2018 finishing.com, Inc., Pine Beach, NJ   -   About finishing.com   -  Privacy Policy
How Google uses data when you visit this site.