Home of the finishing HOTLINE since 1989

-----

Quantity of rhodium plated in auto headlight as reflector






2005

Dear sir
My name is Pierre Aghyarian from Beirut Lebanon , if possible I would like to know how much on an average rhodium is plated on the automotive headlights the reason of this question is to see if it will be worth while to extract or reclaim this metal I would appreciate any help since I couldn't get any info on this issue. Thanking you in advance.
Pierre

Pierre Aghyarian
Rhodium king - Beirut, Lebanon


I could be wrong but I thought it was aluminum deposited from a plasma/vapor process!

Peter Van de Luecht
- Melbourne, Vic, Australia
2005


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"