How to restore mirror finish on stainless steel




Q. I have a very fine (hairline) scratch on a trophy that's made of mirror polished stainless steel. Is there any product to help me repair it at home? Does it need to be professionally buffed and refinished?
(In photo, I held up red book so that scratch could be seen better against red mirrored reflection.)

Vander Vennet
- Austin, Texas
September 11, 2023

Ed. note: We have no photo from you; please attach it to e-mail to mooney@finishing.com

A. Hello Vander,
I don't know of a specific fix to the surface, but one trick I have used to cover up imperfections in metal items I have damaged at my home has been to purchase a nail polish with the exact color and paint over the scratch. Nail polish comes in every color under the sun. If the surface is shiny, put a clear topcoat on it. If the surface is matte, use a matte topcoat.

Casey Selle Charging
- Minneapolis, Minnesota
October 4, 2023




⇩ Related postings, oldest first ⇩



Want deep mirror finish on 304 SS

Q. I periodically am asked to provide a highly polished sink bowl for the private jet airplane industry. I begin with number 4 polished material, 14 or 16 ga 304 stainless. I currently end up with a nice nearly mirror polish but not the deep shine that my customer is looking for. Since my sink is fabricated I must weld each end into the bowl so I first start with 60 grit stones, paper wads and then move to 100 grit to finish the weld. Then we use polish compound 120 grit and 240 grit. Any suggestion?

Jim Nations
stainless steel kitchen products - East St. Louis, Illinois, USA
2004


A. The only suggestion I have is to use power tools. You may have to use multistep flap wheels as well.

tony kenton
AF Kenton
retired business owner - Hatboro, Pennsylvania


A. Go finer in your abrasive approach (auto polish paste and equipment could be a cheap option).

Guillermo Marrufo
Monterrey, NL, Mexico
2004


Windex Commercial Line
(same product in economy size)
windex_commercial
on eBay or

Amazon

(affil links)

A. My company also produces high end equipment with mirror polished finishes for the marine industry.

We start with mill finish stainless steel material, i.e no grain, and after all the fabricating processes are complete it then goes for finishing. All scratches are removed and all welds blended using small air die grinder [adv: die grinders on eBay or Amazon [affil links] with different grit disks on eBay or Amazon [affil links] . We start with 80 grit and then move on to 120, 180, 220, 320, 400 and 800 grit.

It goes on the buffing machine. We use white rouge white buffing bar on eBay or Amazon [affil links] and green compounds on eBay or Amazon [affil links] to produce the final mirror finish. It is very time consuming ... however the results are very satisfying.

Note that the polishing process produces quite a lot of heat and some warping could occur. For parts with hard-to-reach areas that can't be put up to the buffing machine wheel we put an arbor in the die grinder with smaller cloth wheels attached and hand finish. Windex Commercial Line on eBay or Amazon [affil links] is used to remove any finger prints prior to the finished part being wrapped and delivered. Hope this helps.

Mr. Young
- Ft.Lauderdale, Florida, USA
2004





Repairing mirror polish stainless

We are a design/build company that sells #8 polish stainless mirrors, and we have some small scratches on the surface of a few. I am looking for an economical in-house way of polishing out these scratches.

37877

Sather Duke
- Brooklyn, New York
2005


A. It's an art or craft, very tedious, so the mirrors must be worth the effort. It's usually done with help of high speed rotating hand tools equipped with different grit sizes of flap wheels, sandpapers and felt bobs with polishing pastes. Shop tool retailers and do-it-yourself stores may have the materials and equipment, but you also need a patient and careful operator.

Guillermo Marrufo
Monterrey, NL, Mexico


A. I am not familiar with #8 mirrors, but I have done work with BA mirrors, they used them in things like correctional facility's and things of that nature, anyway......have you ever tried to buff out the scratches with some jeweler's rouge,or repolish it then buff out the scratches? Just a thought hope it helps you out.

Regards,

Brian C. Gaylets
- Scranton, Pennsylvania, U.S.A.


A. A #8 I believe is electropolished. My experience has been that to do a duplicate mechanical finish is more time consuming than the replacement cost. I would suggest cutting the damaged pieces and making smaller mirrors of them or selling them as seconds.

Dave Barr
- Centralia, Washington, USA




Q. I am in need of a low(er) cost method of restoring the mirror finish on stainless flatware, as well as removing light disposal nicks left on the edges of spoons.

I purchase flatware for resale, and would like the items I sell to be 'like new' -- often I purchase these items and they have surface scratches -- on the bowls or heels of the spoons, etc. Ideally I would like to accomplish this burnishing with either a Dremel on eBay or Amazon [affil links] tool or a benchtop buffer/polisher (I can't afford to purchase a burnishing machine). I'm not sure how to accomplish this and haven't found any detailed information on how to go about doing this.

Can someone tell me how to do this, or refer me to a website or book that gives detailed instructions? I'm assuming one would start with some sort of polishing compound - and maybe progress through subsequently finer grits. Any help would be very much appreciated!

Sue Giordano
flatware sales - Brevard, North Carolina
2007


Benchtop buffer

on Amazon

(affil links)

A. You can use an inexpensive bench grinder and you'll need to outfit it with some cloth buffs and some "stainless steel" bar compound. A trip to your local Sears should get you outfitted for $100 or so.

Wear safety glasses and gloves, always buff away from edges so the parts don't catch in the buff...practice makes perfect.

jeffrey holmes
Jeffrey Holmes, CEF
Spartanburg, South Carolina





Q. My husband let some new, good quality, stainless steel flatware soak in a bleach water solution. The knives now have pits in them. It seems as some of the finish has been removed. Do I need to dispose of them?

Janelle Oen
Homemaker - Minneapolis, Minnesota
2007


A. Hi, Janelle. After you rinse off the bleach, they are not dangerous. But you can't fill pits in this circumstance, getting the pits out would involves polishing away the rest of the metal to the depth of the pits, which may prove impractical.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




Q. Well, as a overzealous housewife, I have used the green side of a sponge scrubber on my silverware (18/8) and have scratched it. how's that for an introduction of myself and my problem? it no longer shines as it should and I would LOVE to know how to polish this silverware to bring back more of a shine. I have used Wenol on eBay or Amazon [affil links] polish on it and am pretty pleased, but I feel like it must be possible to bring up more of a shine. Any suggestions?

Geri Ridenhour
n/a - Martinsville, Virginia, USA
May 19, 2011


Polishing Kit
polishing_kit
on eBay or

Amazon

(affil links)

A. Hi, Geri.

We appended your inquiry to a similar question that was already answered.

The scratches you imbedded with a kitchen scrubber should not be deep and severe, so I think you can polish them out with simple buffing attachments mounted in a battery powered electric drill ("battery powered" as in "low power", to minimize the chance of hurting yourself). You may have to pick a more aggressive buffing/polishing compound, but try the Wenol on eBay or Amazon [affil links] first.
Good luck, Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey


thumbs up sign  Just wanted to report that my husband got out his Dremel on eBay or Amazon [affil links] drill with its polishing attachments and used a bit of the Wenol cream and wow, luster restored! Thanks for all the help; I really appreciate it and will never routinely use the green scrubber on my silverware again :-)

Geri Ridenhour [returning]
- Martinsville, Virginia, USA
June 3, 2011


thumbs up sign  Thank goodness I'm not the only one looking for a way to buff out disposal damage to my flatware. I have a Dremel on eBay or Amazon [affil links] and a little bench vice, so will look up the buffing tools and look for Wenol on eBay or Amazon [affil links] at my local hardware store, and give this a try. Thanks so much for this information.

Ruth Geil
- Eureka, California, USA
November 11, 2019


thumbs up sign I'm working on buffing up a pilled spoon to make a nice full set and this information will be of value to me! I'll let you know how it goes!!

Cathy Ingraham
- Ludington Michigan
January 1, 2021





(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread


Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"