DEGREASING, PICKLING AND PASSIVATION





2005

I'M A MANUFACTURER OF STAINLESS STEEL EQUIPMENTS, WHERE I NEED TO DO PICKLING & PASSIVATION OF S.S.

CAN YOU SUGGEST ME WHAT CHEMICALS OR MIXTURE OF CHEMICALS ARE USED FOR:

1. DEGREASING
2. PICKLING,
3. PASSIVATION,

HOPE TO RECEIVE YOUR FEEDBACK SOON.

REGARDS,

JIGNESH M. PARMAR
- MUMBAI, MAHARASHTRA, INDIA



Visit www.nickelinstitute.org website-there you can find very good and download free informations on SS technology!

Good luck!

Goran Budija
- Cerovski vrh Croatia
2005



2005

There are a lot of good companies in India supplying good equipment and chemicals. You may want to contact us if you need more information on this.

There are a lot of good suggestions on this Finishing.com site if you search. If you need a complete system you are best to talk to someone who has knowledge in cleaning, pickling and passivation. You can contact Dayton Dailey who can help you. I can give you his email or web site address if you contact me directly.

lee kremer
lee kremer sig
Lee Kremer
Stellar Solutions, Inc.
supporting advertiser
McHenry, Illinois
stellar solutions banner


none
www.finishing.com is made possible by supporting advertisers ...
this text gets replaced with bannerText
spacer gets replaced with bannerImages

Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"