Home antique finishing kit for brass and silver?


(1999)

hello.... I am looking for an inexpensive kit to make brass as well as silver finishes look like antique bronze. since I am disabled, I cannot go to any hobby shops or the like to locate what I am looking for. any help or suggestions out there? any good ideas or suggestions where I get obtain such a kit would be very helpful. thanx everyone!

gail reiss 
- los angeles, California


February 25, 2009

Hi, Gail. Brass Darkening Solution [linked by editor to product info at Rockler] will turn brass a dark antique color. Liver of Sulphur [linked by editor to product info at Amazon] will turn silver blackish.

You can't make silver into a "yellow" metal, because it is a "white" metal, but you could consider applying a Rub'N'Buff [linked by editor to product info at Amazon]. Good luck with it.

Regards,

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.