Hello! I'm looking for a supplier of translucent colors that can be coated over chrome to give a metallic color tone. I know basic blue and red are available in 5 gallon containers. I was told a company called Scwartz sells it in Toronto. I'm sure there must be a place in the US.

I'd really like to get pastel colors for toys I will be plating for Easter. Pink light blue, light green would be nice.

Please let me know if you know a supplier.

Thanks,

Mac Legrandi
- San Diego, California


February 19, 2009

Hi, Mac. Chrome plating is notoriously difficult to get good adhesion onto. I think you would be better off with chrome-like paint. This usually involves a base coat, followed by a layer with tiny metal flake designed to give a chrome-like shine, followed by a top coat which can be translucent to achieve the colors you seek. The banner ad at the top of the page will lead you to suppliers.

Regards,

Ted Mooney, finishing.com Teds signature
Ted Mooney, P.E. RET
finishing.com
Pine Beach, New Jersey



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.