Q. We want the following information from any experienced persons.

We want to give a matt(rough) finish to stainless steel 304; please give the solution (chemicals) detail for this.

Whether chemical dipping is ok or we have to use electric current for giving this finish?

the material is SS304 sheet.

thank you, D.Elangovan

ELANGOVAN DAMODARAN
- INDIA


(1999)

A. I would think a very easy way to get a finish you are looking for is abrasive blasting. You can control the grit size, the pressure and the time.

jim conner
Jim Conner
Anoplex - Dallas, Texas USA


(2007)

Q. We are looking for a chemical to give matte finish to s.s.304 and 316 series

Neha Patel
business woman - India

December 21, 2011

A. Here is a product you can use to obtain matte finish to SS steel:

"Steelmatt" from Arya Tech Solutions Pvt Ltd., Ahmedabad.

Obtain and carefully follow the MSDS. Best regards.

Deian TACHEV
- France

----
Readers: our advertisers make this site possible for technical information exchange & camaraderie; they will contact the inquirers privately regarding any commercial needs. Please appreciate that the site would drown in spam overnight if we posted offers to sell from people paying nothing.



This public forum has 60,000 threads. If you have a question in mind which seems off topic to this thread, you might prefer to Search the Site

ADD a Q or A to THIS thread START a NEW THREADView CURRENT TOPICS

Disclaimer: It's not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & Devices


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.