Blemish on 3 million passivated woodscrews





We have about three million zinc plated and yellow passivate woodscrews in store exhibiting slight white/greyish discolouration in patches. Performance unaffected but unsightly and difficult to sell. Is there anything they can cheaply and easily be dipped in to hide this or am I stuck with the problem.

Terence ONeill
building contracts and supplies - Chippenham, Wiltshire, U.K.
2004



You've got some surface corrosion, possibly from damp storage. You'll have to strip and replate.

jeffrey holmes
Jeffrey Holmes, CEF
Spartanburg, South Carolina
2004


Many thanks to Jeff Holmes, Spartanburg for his advice. Rectification underway.

Happy Xmas

Terry O'Neill

Terence ONeill
Building contracts & supplies - Chippenham, Wiltshire, U.K.
2004


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"