-----Coloured finish on nickel chromium alloy layer
We are looking for a way to develop coloured finishes on a 80Ni/20Cr wire sprayed surface layer on a iron powder metallurgy article;the article will encounter temperatues up to 400 °C in service, hence organic paints/pigments are not an option. Due to other constituents in the alloy, the maximum treatment temperature permissible is 1020 °C. Ideas please!
Kirti Krishnan- Australia
1999
I'm not sure, but you might inquire about Prismatic Stainless Steel [from B&M Finishers, a finishing.com supporting advertiser].

Ted Mooney, P.E.
Striving to live Aloha