I am wondering if I can get the rims on my motorcycle chromed. This brings the question of what type of metals can be chromed to my attention. What are the types of metal that can be chromed?
Jason Endersin need of possibly chroming rims - Raleigh, North Carolina, USA
2004
It is practical to chrome plate most metals, including steel, stainless steel, and aluminum alloys.